Tytuł:
On Degradation of Cast Iron Surface - Protective Paint Coat Joint
Autorzy:
Tupaj, M.
Orłowicz, A. W.
Mróz, A.
Bąk, G.
Abram, T.
Powiązania:
https://bibliotekanauki.pl/articles/381862.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
thin-wall casting
flake graphite
grey cast iron
corrosion
protective paint coat
odlewy cienkościenne
grafit
żeliwo szare
korozja
powłoka ochronna
Opis:
The paper is a presentation of a study on issues concerning degradation of protective paint coat having an adverse impact on aesthetic qualities of thin-walled cast-iron castings fabricated in furan resin sand. Microscopic examination and microanalyses of chemistry indicated that under the coat of paint covering the surface of a thin-walled casting, layers of oxides could be found presence of which can be most probably attributed to careless cleaning of the casting surface before the paint application process, as well as corrosion pits evidencing existence of damp residues under the paint layers contributing to creation of corrosion micro-cells.
Źródło:
Archives of Foundry Engineering; 2016, 16, 3; 133-136
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The properties of cast iron surface layers modified by laser ablation micromachining
Właściwości warstwy wierzchniej żeliwa szarego modyfikowanej ablacyjną mikroobróbką laserową
Autorzy:
Napadłek, W.
Woźniak, A.
Pakowski, C.
Powiązania:
https://bibliotekanauki.pl/articles/188562.pdf
Data publikacji:
2017
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
grey cast iron
oil micro-reservoirs
surface layer
ablation laser texturing
wear resistance under friction conditions
żeliwo szare
mikrozbiorniki olejowe
warstwa wierzchnia
ablacyjne teksturowanie laserowe
odporność na ścieranie w warunkach tarcia
Opis:
The article presents the results of model laboratory tests, including the measurement of temperature, friction force, and linear wear of the surface layer of samples made of grey cast iron sliding against a steel counterpart. The surface layer of the cast iron specimen was modified using ablative laser micromachining in order to change its macro- and micro-geometry. To produce regular oil micro-reservoirs in a shape of micro-channels, an Nd: YAG laser (λ = 1064 nm, ƒ = 1 – 100 kHz, E = 50 J, P = 50W) with a special focusing system was used. Comparative studies included a grey cast iron specimen subjected to conventional mechanical machining and a specimen modified by ablative laser micromachining. 41Cr4 steel with a hardness of 50 HRC was used as a counterpart. Tribological tests were run in a pin-on-disk (T-11 tribometer) test set-up. The best results in the reduction of friction, temperature, and wear were obtained for samples with oil micro-reservoirs (made of ablative laser texturing) in a shape of micro-channels covering 5% of the entire tribological contact surface.
W pracy przedstawiono wyniki modelowych badań laboratoryjnych obejmujących pomiary wybranych parametrów w węźle tarcia, tj.: temperatury, siły tarcia i zużycia mierzonego metodą liniową dla warstwy wierzchniej próbek wykonanych z żeliwa szarego w skojarzeniu ze stalowymi przeciwpróbkami. Warstwę wierzchnią ww. żeliwa poddano modyfikacji, wykorzystując ablacyjną mikroobróbkę laserową w celu zmiany jej makroi mikrogeometrii. Do wytworzenia regularnych mikrozasobników olejowych w kształcie mikrokanałów stosowano laser Nd: YAG (λ = 1064 nm, ƒ = 1 ÷ 100 kHz, E = 50 J, P = 50W) ze specjalnym systemem ogniskowania. Badaniom porównawczym poddana została warstwa wierzchnia żeliwa szarego ukształtowana na drodze tradycyjnej obróbki mechanicznej i zmodyfikowana w wyniku ablacyjnej mikroobróbki laserowej. Materiałem przeciwpróbki była stal 41Cr4 o twardości 50 HRC. W badaniach tribologicznych zastosowano metodę „pin-on-disc” w oparciu o tribometr T-11. Najlepsze efekty w zakresie zmniejszenia siły tarcia i temperatury oraz zwiększenia odporności na zużycie uzyskano w przypadku skojarzeń, w których w warstwie wierzchniej żeliwnych próbek wykonano techniką ablacyjnego teksturowania laserowego mikrozbiorniki olejowe w kształcie mikrokanałów z ich 5% udziałem powierzchniowym.
Źródło:
Tribologia; 2017, 276, 6; 59-64
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of machining of EN-GJL-250 and EN-GJS-400 cast irons on tribological behavior
Autorzy:
Martinez, J.
Pereira, A.
Perez, J. A.
Mathia, T.
Powiązania:
https://bibliotekanauki.pl/articles/94140.pdf
Data publikacji:
2015
Wydawca:
Politechnika Poznańska. Wydawnictwo Politechniki Poznańskiej
Tematy:
tribological behavior
grey cast iron
spheroidal graphite cast iron
friction
surface wear
Opis:
In transport and, particularly in the case of the present study, naval industries, one of the major objectives of research on wear and friction is focused principally on solid lubrication. In the following paper, the tribological behaviors of two well-known, different cast irons, lamellar grey iron (EN-GJL-250) and spheroidal graphite ductile iron (EN-GJS-400), are compared and the results are analyzed. For each material's family, the surfaces’ properties are characterized at different stages of the machining process. The particular influence of diverse feed rates in a turning facing is evaluated. Moreover, some tests of the laser cladding process, which contribute to the improvement of superficial properties, are carried out; therefore, the initial morphology before surface treatment is carefully characterized and evaluated in the context of subsequent adhesion qualification. The final goal of the study is to deliver feasible initial information concerning two similar cast irons that are traditionally used in the naval industry, which would be manufactured and employed in the future as dry lubricated bearings
Źródło:
Archives of Mechanical Technology and Materials; 2015, 35; 12-22
2450-9469
Pojawia się w:
Archives of Mechanical Technology and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Impact of Selected Geometry Parameter of Titanium Spatial Insert on the Surface Layer Formation on Grey Cast Iron
Autorzy:
Dziwoki, G.
Dulska, A.
Szajnar, J.
Król, M.
Powiązania:
https://bibliotekanauki.pl/articles/379470.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
grey cast iron
Titanium
Carbides
layered casting
insert
żeliwo szare
tytan
węgliki
odlewanie warstwowe
Opis:
The paper presents a method of producing a grey cast iron casting locally reinforced with a titanium insert printed using SLM method (Selective Laser Melting). This article attempts to examine the impact of the selected geometry of titanium spatial insert on the surface layer formation on grey cast iron. The scope of the research focuses on metallographic examination - observation and analysis of the structure of the reinforced surface layer on a light and scanning microscope and a hardness measurement of the titanium layer area. Based on the obtained results, it was concluded that the reaction between titanium insert and metal (grey cast iron) locally develops numerous carbides precipitation (mainly TiC particles), which increases the hardness of the reinforced surface layer and local strengthening of the material. The ratio between the thickness of the support part (grey cast iron) and the working part (titanium insert) affects the resulting layers connection structure. The properties of the obtained reinforced surface layer depend mainly on the geometry of the insert (primarily on the internal dimensions of the connector) and the volume of the casting affecting the re-melting of the insert. A more concentrated structure of carbides precipitation occurs in castings with a full connector insert.
Źródło:
Archives of Foundry Engineering; 2019, 1; 58-62
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Effect of a Thin-Wall Casting Mould Cavity Filling Conditions on the Casting Surface Quality
Autorzy:
Trytek, A.
Orłowicz, A. W.
Tupaj, M.
Mróz, M.
Markowska, O.
Bąk, G.
Abram, T.
Powiązania:
https://bibliotekanauki.pl/articles/382148.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
thin wall casting
grey cast iron
cold shots
computer simulation
odlew cienkościenny
żeliwo szare
symulacja komputerowa
Opis:
The paper presents results of metallographic examination of faults occurring in the course of founding thin-walled cast-iron castings in furan resin sand molds. A non-conformance of the scab type was Observed on surface of the casting as well as sand buckles and cold shots. Studied the chemical composition by means of a scanning electron microscope in a region of casting defects: microanalysis point and microanalysis surface. Around the observed defects discloses high concentration of oxides of iron, manganese and silicon. A computer simulation of the casting process has been carried out with the objective to establish the cause of occurrence of cold shots on casting surface. The simulation was carried out with the use of NovaFlow & Solid program. We analyzed the flowing metal in the mold cavity. The main reason for the occurrence of casting defects on the surface of the casting was gating system, which caused turbulent flow of metal with a distinctive splash stream of liquid alloy.
Źródło:
Archives of Foundry Engineering; 2016, 16, 4; 222-226
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Badania odporności na zużycie warstwy wierzchniej materiałów stosowanych na elementy silnika spalinowego po teksturowaniu laserowym
The investigation resistance to wear the surface layer of materials applied on the elements of the engine of combustion after laser texturing
Autorzy:
Napadłek, W.
Pakowski, Cz.
Powiązania:
https://bibliotekanauki.pl/articles/188837.pdf
Data publikacji:
2010
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
żeliwo szare niskostopowe
stal 54SiCr6
warstwa wierzchnia
teksturowanie laserowe
odporność na zużycie w warunkach tarcia
grey cast iron
steel 54 SiCr6
top layer
laser texturing
resistance on waste in the conditions of the friction
Opis:
W pracy przedstawiono wyniki badań laboratoryjnych w zakresie pomiaru siły tarcia oraz odporności na zużycie w warunkach tarcia warstwy wierzchniej żeliwa szarego niskostopowego stosowanego w produkcji tulei cylindrowych oraz stali 54SiCr6 przeznaczonej do azotowania, stosowanej w produkcji pierścieni tłokowych. Warstwę wierzchnią modelowych elementów węzła tribologicznego poddano modyfikacji, wykorzystując ablacyjną mikroobróbkę laserową, tj. teksturowanie laserowe, mające na celu poprawę jej makro- i mikrogeometrii. Do wytworzenia regularnych mikrozasobników olejowych w kształcie półczasz kulistych ora mikrokanałów stosowano laser Nd: YAG ze specjalnym systemem ogniskowania. Badaniom porównawczym poddana została topografia powierzchni ukształtowana na drodze tradycyjnej obróbki mechanicznej oraz zmodyfikowana w wyniku mikroobróbki laserowej. W laboratoryjnych badaniach tribologicznych zastosowano metodę badawczą "pin on disk" wykorzystującą tribometr T-11. Najlepsze efekty w zakresie zmniejszenia siły tarcia oraz zwiększenia odporności na zużycie uzyskano w przypadku modelowego skojarzenia, w którym elementy węzła tarcia poddane były teksturowaniu laserowemu przy dobranych parametrach obróbki laserowej w układzie geometrycznym ze stopniem przykrycia ok. 25%.
The results of laboratory investigations were introduced in the work in the range of the measurement of the coefficient of friction and resistance on waste in the conditions of the friction of the top layer of grey cast iron applied in the production of cylindrical funnels and solid 54 SiCr6 designed to nitrogenizing, applied in the production of piston collars. The top layer of the model units of the knot tribologycal was subjected the modification, using laser micromachining ablation: laser texturing, having on the aim of the improvement her macro- and microgeometry. The laser was applied to producing regular oil microcontainers in the shape halfbowl spherical and microchannels Nd: YAG with the special system of focussing. The topography of the surface shaped on the of the traditional processing mechanical road was subjected comparative audits and modified in the result laser micromachining. The investigative method was applied in laboratory audits tribological "pin on disk" in the support about T-11. The best effects in the range of decrease of the coefficient of the friction and the enlargement of the resistance on the waste was got in the case of model associating, in which the elements of the knot laser texturing near the well-chosen parameters of laser processing in geometrical arrangement with the degree of the cover the friction were subjected 25 % approx.
Źródło:
Tribologia; 2010, 5; 37-51
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-6 z 6

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies