Tytuł:
The analysis of wear of the layers containing WC/W2C in abrasive soil
Analiza procesu zużywania warstw z zawartością WC/W2C w glebowej masie ściernej
Autorzy:
Napiórkowski, J.
Ligier, K.
Powiązania:
https://bibliotekanauki.pl/articles/191143.pdf
Data publikacji:
2016
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
WC/W2C carbides
abrasive wear
spinning bowl method
abrasive soil mass
węgliki WC/W2C
zużycie ścierne
metoda wirującej misy
glebowa masa ścierna
Opis:
The paper presents the results of research involving the resistance of hardfacing materials containing WC/W2C carbides to abrasive wear. The tested hardfacing materials were made using PJ5D and El-Tung FeA rods. The WC/W2 C carbide contents of the examined materials amounted to 90% and 60%. These materials are meant to be used in mining tools subject to intense abrasive wear. In spite of its higher WC/W2 C carbide content, the intensity of wear of the hardfacing material made using the PJ5D rod was higher than that of the hardfacing material made using the El-Tung FeA rod. Wear resistance tests were conducted by means of the “spinning bowl” method, using real (natural) soil masses. Light and heavy soil masses were used.
W pracy przedstawiono wyniki badań odporności na zużywanie ścierne napoin z zawartością węglików WC/W2C. Badano napoiny wykonane pałeczkami PJ5D i El-Tung FeA. Zawartość węglików WC/W2 C w badanych materiałach wynosiła 90% i 60%. Materiały te są przeznaczone do stosowania w narzędziach górniczych narażonych na intensywne zużycie ścierne. Pomimo większej zawartości węglików WC/W2C intensywność zużywania napoiny wykonanej pałeczką PJ5D była większa od napoiny wykonanej pałeczką El-Tung FeA. Badania odporności na zużycie przeprowadzono metodą „wirującej misy” z wykorzystaniem rzeczywistych (naturalnych) mas glebowych. Zastosowano masy glebowe lekkie i ciężkie.
Źródło:
Tribologia; 2016, 269, 5; 121-132
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Tribological properties of polyurethanes in abrasive soil mass
Właściwości tribologiczne tworzyw poliuretanowych w glebowej masie ściernej
Autorzy:
Napiórkowski, J.
Ligier, K.
Powiązania:
https://bibliotekanauki.pl/articles/189521.pdf
Data publikacji:
2017
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
abrasive wear
polyurethanes
abrasive soil mass
friction surface
zużycie ścierne
poliuretany
glebowa masa ścierna
powierzchnia tarcia
Opis:
This paper presents a comparative study of polyurethane wear in abrasive soil mass. Two types of polyurethanes of various chemical compositions and untreated 38GSA steel were tested, the latter being used as a reference standard. The study was conducted in a natural soil mass at a “rotating bowl” stand. Relative wear resistance was determined from measurements of mass wear for the materials under study. The conditions of the surface of the materials under wear tests were analysed.
W pracy przedstawiono badania porównawcze zużywania poliuretanów w glebowej masie ściernej. Badaniom poddano dwa rodzaje poliuretanów o różnym składzie chemicznym oraz stal 38GSA w stanie nieobrobionym, która była materiałem wzorcowym. Badania prowadzono w naturalnej masie glebowej na stanowisku typu „wirująca misa”. Na podstawie pomiarów zużycia wagowego dla badanych materiałów wyznaczono względną odporność na zużycie. Przeprowadzono analizę stanu powierzchni zużywanych materiałów.
Źródło:
Tribologia; 2017, 276, 6; 65-70
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of the Angle of Impact of an Abrasive Soil Mass on Steel Wear Intensity
Wpływ kąta oddziaływania glebowej masy ściernej na intensywność zużycia stali
Autorzy:
Napiórkowski, J.
Ligier, K.
Powiązania:
https://bibliotekanauki.pl/articles/190755.pdf
Data publikacji:
2018
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
abrasive wear
abrasive soil mass
rotating bowl
Hardox Extreme steel
zużycie ścierne
glebowa masa ścierna
wirująca misa
stal Hardox Extreme
Opis:
This article presents a study into the effect of the rake angle of the working surface of a specimen made of Hardox Extreme steel on abrasive wear intensity. The study was conducted using the “rotating bowl” method in two types of an abrasive soil mass at three specimen rake angles of 0˚, 12˚, and 17˚. No significant differences in the wear intensity were observed for a heavy abrasive soil mass, while for a light abrasive soil mass, an increase in the wear intensity was observed with an increase in the rake angle, with the greatest increase in the wear intensity occurring after a change in the rake angle from 0˚ to 12˚. Increasing the rake angle from 12˚ to 17˚ resulted in no significant change in the wear intensity. In the light abrasive soil mass, non-zero specimen rake angles increased the dynamic impact of loose abrasive wheels. The appearance of the surface of specimens subjected to abrasion under these conditions indicated a high proportion of erosive wear accompanying the scratching and ridging wear.
W artykule przedstawiono badanie wpływu kąta natarcia powierzchni roboczej próbki wykonanej ze stali Hardox Extreme na intensywność zużycia ściernego. Badania prowadzono metodą wirującej misy w dwóch rodzajach glebowej masy ściernej przy trzech kątach natarcia próbki 0˚, 12˚ i 17˚. Dla glebowej ciężkiej masy ściernej nie zaobserwowano istotnych różnic intensywności zużycia, Natomiast dla lekkiej glebowej masy ściernej wraz ze wzrostem kąta natarcia zaobserwowano wzrost intensywności zużycia, przy czym największy wzrost intensywności zużycia wystąpił przy zmianie kąta natarcia od 0˚ do 12˚ Zwiększanie kąta natarcia od 12˚ do 17˚ nie spowodowało istotnej zmiany intensywności zużycia. W lekkiej glebowej masie ściernej niezerowe kąty natarcia próbki powodowały zwiększone dynamiczne oddziaływanie luźnych ziaren ściernych. Wygląd powierzchni próbek zużywanych w tych warunkach wskazywał na duży udział zużycia erozyjnego towarzyszącego zużyciu przez rysowanie i bruzdowanie.
Źródło:
Tribologia; 2018, 279, 3; 99-105
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Analiza geometrii ziaren glebowej masy ściernej
Analysis of geometry of grains of soil abrasive mass
Autorzy:
Napiórkowski, J.
Szczyglak, P.
Kołakowski, K.
Powiązania:
https://bibliotekanauki.pl/articles/288893.pdf
Data publikacji:
2013
Wydawca:
Polskie Towarzystwo Inżynierii Rolniczej
Tematy:
glebowa masa ścierna
geometria ziarna
zużycie ścierne
mikroskop stereometryczny
soil abrasive mass
geometry of grain
abrasion
stereometric microscope
Opis:
W pracy przedstawiono analizę geometrii ziaren glebowych dla czterech rodzajów glebowej masy ściernej. Oceny geometrii dokonano przy pomocy mikroskopu stereometrycznego z wykorzystaniem programu Motic Images Plus 2.0. Ocenie poddano promień zewnętrzny okręgu opisanego na konturze ziarna ściernego, promień wewnętrzny okręgu wpisanego wewnątrz konturu ziarna, pola uwypukleń figur nieregularnych ziarna oraz obwody uwypukleń figur nieregularnych. Badano frakcje glebowe żwiru, piasku oraz iłu i pyłu w glebach piaszczystych i gliniastych. Uzyskane wyniki i obliczenia statystyczne umożliwiły stwierdzenie istotnych różnic w geometrii ziaren masy ściernej oraz zróżnicowany ich kształt w poszczególnych glebach. Najmniejsze różnice geometrii cząstek stwierdzono dla frakcji pyłu i iłu ( maksymalnie 28%), największe zaś dla frakcji piasku, dochodzące do 79%. Wskazuje to na konieczność uwzględnienia, w procesie doboru właściwości warstwy wierzchniej elementu roboczego do danego rodzaju obrabianej gleby, obok składu granulometrycznego i odczynu gleby, także geometrii ziaren glebowych. Celem pracy jest ocena geometrii ziaren frakcji żwiru, piasku i pyłu wraz z iłem, wchodzących w skład wybranych rodzajów glebowej masy ściernej.
Analysis of the geometry of soil grains for four types of soil abrasive mass was presented. Assessment of the geometry was carried out with the use of a stereometric microscope with the use of Motic Images Plus 2.0 programme. External radius of the circle inscribed in the contour line of the abrasive grain, internal radius of the circle inscribed in the contour of a grain, fields of protrusions of irregular figures of a grain and circumferences of protrusions of irregular figures were assessed. Soil fractions of gravel, sand and loam and dust in sandy and clay soils were investigated. The obtained results and statistical calculations enabled determination of significant differences in the geometry of abrasive mass of grains and their variable shape in particular soils. The smallest differences of fractions were determined for fraction of dust and loam (at the maximum 28%), whereas the biggest for sand fractions up to 79%. It proves necessary to include also geometry of soil grains in the selection process of properties of the working element surface layer to a specific type of the processed soil, next to the granulometric composition and reaction of soil. The objective of the paper was to assess geometry of grains of gravel fraction, sand and dust along with loam, which compose the selected types of soil abrasive mass.
Źródło:
Inżynieria Rolnicza; 2013, R. 17, nr 4, t. 1, 4, t. 1; 237-247
1429-7264
Pojawia się w:
Inżynieria Rolnicza
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The structural properties and resistance to abrasive wear in soil of Creusabro steel
Właściwości strukturalne i odporność na zużywanie w warunkach glebowej masy ściernej stali Creusabro
Autorzy:
Napiórkowski, J.
Konat, Ł.
Ligier, K.
Powiązania:
https://bibliotekanauki.pl/articles/971610.pdf
Data publikacji:
2016
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
steel resistant to abrasive wear
structural and mechanical properties
Creusabro steel
abrasive soil mass
własności strukturalne i mechaniczne
stal Creusabro
glebowa masa ścierna
stale odporne na zużywanie ścierne
Opis:
The paper presents the results of abrasive wear resistance tests on Creusabro 4800 and Creusabro 8000 steel. The results obtained for laboratory samples were referred to the structure of the examined types of steel and to the basic indicators characterising their mechanical properties. As a result of the conducted tests, which used the methods of light and scanning microscopy, it has been concluded that, in its delivered condition Creusabro, steel exhibits a complex type of structure, characteristic for steel with the “TRIP effect.” The identified type of structure indicates a precisely adjusted chemical composition and the use of specialised heat treatment and forming processes in the production process of those materials. The abrasive wear resistance tests conducted by means of the “spinning bowl” method in real soil masses, i.e. light soil (loamy sand), medium soil (light till) and heavy soil (normal till), as well as the conducted measurements of hardness, have proven the strict dependence of the obtained indicators of abrasive wear resistance on the phase structure and on the status of the heat treatment of the tested steel. The results of abrasive wear resistance tests for Creusabro steel were referred to 38GSA steel in a normalised condition for comparison.
W pracy przedstawiono wyniki badań odporności na zużywanie ścierne stali Creusabro 4800 i Creusabro 8000. Uzyskane wyniki prób laboratoryjnych odniesiono do budowy strukturalnej badanych stali oraz do podstawowych wskaźników charakteryzujących ich własności mechaniczne. W wyniku przeprowadzonych badań z wykorzystaniem metod mikroskopii świetlnej i skaningowej stwierdzono, iż w stanie dostarczenia stale Creusabro posiadają złożony typ budowy strukturalnej charakterystyczny dla stali z tzw. efektem TRIP. Zidentyfikowany rodzaj budowy wskazuje na precyzyjnie dobrany skład chemiczny oraz zastosowanie w procesie wytwarzania tych materiałów specjalistycznych zabiegów obróbki cieplno-plastycznej. Zrealizowane próby odporności na zużywanie ścierne metodą „wirującej misy” w rzeczywistych masach glebowych, tj. gleba lekka (piasek gliniasty), gleba średnia (glina lekka) oraz gleba ciężka (glina zwykła), a także przeprowadzone pomiary twardości wykazały ścisłą zależność uzyskanych wskaźników odporności na zużywanie ścierne od budowy fazowej oraz od stanu obróbki cieplnej badanych stali. Wyniki badań odporności na zużywanie ścierne stali Creusabro zostały odniesione porównawczo do stali 38GSA w stanie normalizowanym.
Źródło:
Tribologia; 2016, 269, 5; 105-119
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Badanie struktur i zużywania powłok napawanych w glebowej masie ściernej
Research on structures and wear processes of hard surface layers in a soil abrasive mass
Autorzy:
Napiórkowski, J.
Pękalski, G.
Kołakowski, K.
Powiązania:
https://bibliotekanauki.pl/articles/189228.pdf
Data publikacji:
2012
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
warstwa napawana
mikrostruktura warstwy
glebowa masa ścierna
proces zużywania
intensywność zużycia
hardfacing layers
microstructures of hardfacing layers
abrasive soil mass
wear process
intensity of wear
Opis:
W pracy przeanalizowano przebieg zużycia warstw napawanych o zróżnicowanych mikrostrukturach oraz budowie na zużycie jednostkowe w żwirowej i ilastej glebowej masie ściernej w dwóch ich stanach wilgotnościowych (suchym i mokrym). Do badań wybrano warstwy uzyskane poprzez napawanie materiałów na bazie stopów Fe-C-Cr zawierających pierwiastki węglikotwórcze B, V, Nb, Mn, Mo i W. Badania w warunkach laboratoryjnych realizowano na maszynie zużyciowej typu "wirującej masy" na drodze tarcia 10 km. Badania mikroskopowe wykonano za pomocą mikroskopu Neophot 52. Do obserwacji mikrostruktur wykorzystano mikroskopy skaningowe TESLA BS340 sprzężony z mikroanalizatorem TESLA NL-2001A oraz STEREOSCAN 180 z przystawkami do mikroanalizy Link System oraz Philips EM 515. Uzyskane wyniki wskazują, że wraz ze zmianą składu granulometrycznego masy ściernej zmieniają się wartości zużycia napoin. Zużycie w glebie żwirowej jest do 5× intensywniejsze niż w glebie ilastej w zależności od napawanej warstwy i stanu wilgotnościowego gleby. Zwiększenie wilgotności gleby powoduje zmniejszenie nawet 10× intensywności zużywania. Na podstawie przeprowadzonych badań stwierdzono, że zmniejszenie intensywności zużywania w glebowej masie ściernej wymaga wytworzenia warstw wierzchnich zawierających węgliki pierwotne (Fe, Cr)7 C3, węgliki typu Mo2C, VC, TiC oraz eutektyki [alfa + (Fe, Cr) 7 C3].
The paper presents the analysis of the process of the wear, using the unit wear rate, of hard surface layers with different structures in a gravel and loamy abrasive soil mass in two states of moisture, dry and wet. Test materials based on Fe-Cr-C containing carbides with elements B, V, Nb, Mn, Mo and W layers obtained by welding were selected. The laboratory research was conducted on a "spinning bowl" type wear machine with a sliding distance of 10 km. Microscopic research was performed using a Neophot 52 microscope with ordinary and inversion lenses. Scanning microscopy, TESLA BS340, connected with microanalysis TESLA NL-2001A and STEREOSCAN 180 with microanalysis Link System and a Philips EM 515 were used to observe the structures. The results show that changes in the granulometric composition of the wear mass also change the wear values of hard surface layers. The wear rate in the gravel is 5 times more intense than in the loamy soil, depending on the surfaced layer and soil moistures. Increasing soil moisture reduces the intensity of wear up to 10 times. Based on the studies, it was found that reducing the intensity of wear in abrasive soil mass requires the surface layers containing primary carbides (Fe, Cr)7 C3, carbides types Mo2C, VC, TiC, and eutectic [alfa + (Fe, Cr)7 C3].
Źródło:
Tribologia; 2012, 3; 111-117
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-6 z 6

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies