Structural properties and abrasive-wear resistance of Brinar 400 and Brinar 500 steels
Właściwości strukturalne i odporność na zużywanie ścierne stali Brinar 400 i Brinar 500
Autorzy:
Konat, Ł.
Napiórkowski, J.
Białobrzeska, B.
Powiązania:
https://bibliotekanauki.pl/articles/188465.pdf
Data publikacji:
2017
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
steel resistant to abrasive wear
structural and mechanical properties
Brinar steel
abrasive soil mass
stale odporne na zużywanie ścierne
własności strukturalne i mechaniczne
stal Brinar
glebowa masa ścierna
Opis:
In the paper, microstructures and the examination results of abrasive-wear resistance of steel grades Brinar 400 and Brinar 500 are presented. It was found on the grounds of light and electron scanning microscopy that these steels are characterised by subtle differences in microstructures, influencing their mechanical and usable properties. In as-delivered condition, the steels have fine-grained structure with post-martensitic orientation, containing few particles of carbide phases. Such microstructures of Brinar steels and the performed chemical analyses indicate that their properties are formed during specialised operations of thermo-mechanical rolling. Generally, it can be said that the examined steels were designed according to the accepted standards of material engineering, related to low-alloy, high-strength, and abrasive-wear resistant martensitic steels. According to the above, the obtained results of structural examinations of Brinar 400 and Brinar 500 steels were referred to real abrasive-wear indices obtained by the spinning bowl method with use of various abrasive soil masses. The tests carried-out in light soil (loamy sand), medium soil (sandy loam), and in heavy soil (loam), as well as hardness measurements showed strict dependence of abrasive-wear indices on microstructures and the heattreatment condition of the examined steels. Examination results of abrasive-wear resistance of Brinar steels were compared with those of steel 38GSA in normalised conditions.
W pracy przedstawiono budowę strukturalną oraz wyniki badań odporności na zużywanie ścierne stali Brinar 400 i Brinar 500. Na podstawie przeprowadzonych metodami mikroskopii świetlnej i skaningowej badań wykazano, że stale te cechują się subtelną różnicą w budowie strukturalnej rzutującą na ich charakterystyki wytrzymałościowe i użytkowe. W stanie dostarczenia rozpatrywane stale charakteryzują się drobnoziarnistą strukturą o orientacji pomartenzytycznej z nielicznymi wydzieleniami faz węglikowych. Powyższy typ budowy strukturalnej stali Brinar oraz przeprowadzone analizy spektralne składu chemicznego wskazują, iż ich właściwości kształtowane są w toku specjalistycznych zabiegów termomechanicznego walcowania. Ogólnie rzecz biorąc, można stwierdzić, że badane stale zostały zaprojektowane zgodnie z przyjętymi kanonami inżynierii materiałowej odnośnie do niskostopowych, wysokowytrzymałych stali martenzytycznych odpornych na zużywanie ścierne. Zgodnie z powyższym uzyskane wyniki badań strukturalnych stali Brinar 400 i Brinar 500 odniesiono do rzeczywistych wskaźników odporności na zużycie ścierne uzyskanych metodą „wirującej misy” z wykorzystaniem zróżnicowanych glebowych mas ściernych. Zrealizowane badania w glebie lekkiej (piasek gliniasty), glebie średniej (glina lekka) oraz glebie ciężkiej (glina zwykła), a także przeprowadzone pomiary twardości wykazały ścisłą zależność uzyskanych wskaźników odporności na zużywanie ścierne od budowy fazowej oraz od stanu obróbki cieplnej badanych stali. Wyniki badań odporności na zużywanie ścierne stali Brinar odniesiono porównawczo do stali 38GSA w stanie normalizowanym.
Źródło:
Tribologia; 2017, 273, 3; 67-75
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The structural properties and resistance to abrasive wear in soil of Creusabro steel
Właściwości strukturalne i odporność na zużywanie w warunkach glebowej masy ściernej stali Creusabro
Autorzy:
Napiórkowski, J.
Konat, Ł.
Ligier, K.
Powiązania:
https://bibliotekanauki.pl/articles/971610.pdf
Data publikacji:
2016
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
steel resistant to abrasive wear
structural and mechanical properties
Creusabro steel
abrasive soil mass
własności strukturalne i mechaniczne
stal Creusabro
glebowa masa ścierna
stale odporne na zużywanie ścierne
Opis:
The paper presents the results of abrasive wear resistance tests on Creusabro 4800 and Creusabro 8000 steel. The results obtained for laboratory samples were referred to the structure of the examined types of steel and to the basic indicators characterising their mechanical properties. As a result of the conducted tests, which used the methods of light and scanning microscopy, it has been concluded that, in its delivered condition Creusabro, steel exhibits a complex type of structure, characteristic for steel with the “TRIP effect.” The identified type of structure indicates a precisely adjusted chemical composition and the use of specialised heat treatment and forming processes in the production process of those materials. The abrasive wear resistance tests conducted by means of the “spinning bowl” method in real soil masses, i.e. light soil (loamy sand), medium soil (light till) and heavy soil (normal till), as well as the conducted measurements of hardness, have proven the strict dependence of the obtained indicators of abrasive wear resistance on the phase structure and on the status of the heat treatment of the tested steel. The results of abrasive wear resistance tests for Creusabro steel were referred to 38GSA steel in a normalised condition for comparison.
W pracy przedstawiono wyniki badań odporności na zużywanie ścierne stali Creusabro 4800 i Creusabro 8000. Uzyskane wyniki prób laboratoryjnych odniesiono do budowy strukturalnej badanych stali oraz do podstawowych wskaźników charakteryzujących ich własności mechaniczne. W wyniku przeprowadzonych badań z wykorzystaniem metod mikroskopii świetlnej i skaningowej stwierdzono, iż w stanie dostarczenia stale Creusabro posiadają złożony typ budowy strukturalnej charakterystyczny dla stali z tzw. efektem TRIP. Zidentyfikowany rodzaj budowy wskazuje na precyzyjnie dobrany skład chemiczny oraz zastosowanie w procesie wytwarzania tych materiałów specjalistycznych zabiegów obróbki cieplno-plastycznej. Zrealizowane próby odporności na zużywanie ścierne metodą „wirującej misy” w rzeczywistych masach glebowych, tj. gleba lekka (piasek gliniasty), gleba średnia (glina lekka) oraz gleba ciężka (glina zwykła), a także przeprowadzone pomiary twardości wykazały ścisłą zależność uzyskanych wskaźników odporności na zużywanie ścierne od budowy fazowej oraz od stanu obróbki cieplnej badanych stali. Wyniki badań odporności na zużywanie ścierne stali Creusabro zostały odniesione porównawczo do stali 38GSA w stanie normalizowanym.
Źródło:
Tribologia; 2016, 269, 5; 105-119
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of PE–LD and PE–HD as Modifiers of Elastomers Used in Mobile Tracks on Their Tribological Wear
Wpływ PE–LD i PE–HD jako modyfikatorów elastomerów stosowanych w gąsienicach jezdnych na ich zużywanie tribologiczne
Autorzy:
Napiórkowski, Jerzy
Olejniczak, Klaudia
Powiązania:
https://bibliotekanauki.pl/articles/191162.pdf
Data publikacji:
2019
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
polyethylene
abrasive wear
elastomers
mobile track
abrasive soil mass
polietylen
zużycie ścierne
elastomery
gąsienica jezdna
glebowa masa ścierna
Opis:
This paper presents a study of PE–LD and PE–HD as modifiers of elastomers used in mobile tracks on their tribological wear. The experiment was conducted at a “rotating bowl” test stand in three types of soil mass: light, medium, and heavy soil. Based on measurements of mass wear of the tested materials, relative resistance to wear was determined. It was found that an elastomer containing chemically modified polyethylene (PE–HD) was more resistant to wear than an elastomer containing low-density polyethylene (PE–LD). Using a microscope, the condition of the material surfaces following tribological tests was analysed.
W pracy przedstawiono badania PE–LD i PE–HD jako modyfikatorów elastomerów stosowanych w gąsienicach jezdnych na ich zużywanie tribologiczne. Badania przeprowadzono na stanowisku „wirującej misy” w trzech rodzajach masy glebowej: gleba lekka, średnia oraz ciężka. Na podstawie pomiarów zużycia masowego badanych materiałów wyznaczono względną odporność na zużycie. Stwierdzono, że elastomer zawierający polietylen modyfikowany chemicznie (PE–HD) jest bardziej odporny na ścieranie w stosunku do elastomeru o zawartości polietylenu o niskiej gęstości (PE–LD). Za pomocą mikroskopu dokonano analizy stanu powierzchni materiałów po badaniach tribologicznych.
Źródło:
Tribologia; 2019, 285, 3; 89-95
0208-7774
Pojawia się w:
Tribologia
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies