Understanding the difficult selective separation characteristics of high-ash fine coal
Autorzy:
Yang, Zili
Liu, Min
Chang, Guohui
Xia, Yangchao
Li, Ming
Xing, Yaowen
Gui, Xiahui
Powiązania:
https://bibliotekanauki.pl/articles/1845210.pdf
Data publikacji:
2020
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
high-ash fine coal
flotation
rod grinding
floatability
slime coating
Opis:
As the supply of high-quality coals decreases and mechanical coal mining becomes more widespread, the high selective recovery of high-ash fine coal has become a prominent problem in the flotation process. Herein, we discuss the main reasons why the selective separation of high-ash fine coal is difficult. The analysis of high-ash fine coal properties shows that coarse particles (0.25-0.5 mm) account for 22.53% of the total size fraction and that 57.90% of the coal is moderate- or high-density (+1.4 g/cm3) intergrowth. Grinding experiments show that the traditional rod mill has little impact on the liberation of the intergrowth. Instead, its main function is to adjust the particle size composition to ensure that the particle sizes of high-ash fine coal are within the particle size range suitable for flotation. The flotation results show that a clean coal yield of 30.42%, with a 12.46% ash content, is obtained with the optimal flotation parameters through the roughing and cleaning flotation process. However, the flotation results also show that in the separation of high-ash fine coal, it is difficult to obtain clean coal with a high yield and low ash content at the same time. This is mainly due to the similar floatability of moderate-density and low-density coal particles, which allows a large number of moderate-density coal particles to be recovered, and a significant slime coating of clay on the coal’s surface that is generated during the flotation process. The results of this work provide valuable guidance for high-ash fine coal industrial flotation applications.
Źródło:
Physicochemical Problems of Mineral Processing; 2020, 56, 5; 874-883
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of ultrasonic pre-treatment on coal slime flotation
Autorzy:
Lv, Wenbao
Chen, Jun
Min, Fanfei
Hou, Baohong
Liu, Chunfu
Powiązania:
https://bibliotekanauki.pl/articles/1450106.pdf
Data publikacji:
2020
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
ultrasonic pretreatment
surface property
high-ash fine mud
flotation
Opis:
Combined with the characteristics of flotation feed originating from China’s Panyidong Coal Preparation Plant, the ash, zeta potential, X-ray fluorescence spectroscopy and contact angle test were used to study changes in the surface properties of flotation feed under ultrasonic pre-treatment, and its effect on flotation of coal slime. Results show that Preferred pre-treatment process is ultrasonic secondary treatment, ultrasonic secondary pre-treatment can remove most of the high-ash fine mud for instance kaolinite, montmorillonite and quartz in the coal slurry, reduce the surface electronegativity of coal particles, and increase the contact angle of coal particles. Thus, the concentrate ash content decreases to 13%, the recovery rate, yield of flotation concentrate and combustible matter recovery reach 92.6%, 90.9% and 97.6%, respectively.
Źródło:
Physicochemical Problems of Mineral Processing; 2020, 56, 1; 173-183
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Electrokinetic and flotation behavior of rutile in the presence of lead ions and aluminium ions
Autorzy:
Cheng, Hongwei
Liu, Changmiao
Guo, Zhenxu
Feng, Ansheng
Wei, Min
Lv, Zihu
Wu, Dongyin
Zhao, Dengkui
Powiązania:
https://bibliotekanauki.pl/articles/110558.pdf
Data publikacji:
2019
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
lead ions
aluminium ions
rutile
flotation
Opis:
The effects of Pb(II) ions and Al(III) ions on the electro kinetic and flotation behavior of rutile were investigated by micro-flotation tests, zeta potential measurements and solution chemistry analysis. Micro-flotation results indicate that the Pb(II) ions can effectively improve the flotation recovery of rutile while the Al(III) ions significantly inhibit the flotation of rutile. Zeta potential measurements reveal that a collector styrene phosphoric acid (SPA) can adsorb on the rutile surface after the addition of Pb(II) ions, but hardly adsorb on the rutile surface after the addition of Al(III) ions. Pb(II) ions adsorb on the rutile surface in the form of Pb(OH)+ and Pb(OH)2(s), and the latter one is the main reason that activates rutile flotation. Al(III) ions adsorb on the rutile surface mainly in the form of Al(OH)3(s), which prevent the direct interaction between the rutile and the collector, resulting in a decrease of rutile flotation recovery.
Źródło:
Physicochemical Problems of Mineral Processing; 2019, 55, 2; 458-466
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies