Tytuł:
Effect of Heat Treatment on Machining Properties of the AlSi9Cu3(Fe) Alloy
Autorzy:
Wieroński, W.
Pezda, J.
Ponikwia, Ł.
Powiązania:
https://bibliotekanauki.pl/articles/379474.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
silumin
heat treatment
machinability
refining
mechanical properties
cutting power
aluminum alloys
obróbka cieplna
obróbka mechaniczna
rafinacja
właściwości mechaniczne
cięcie
stopy aluminium
Opis:
Automation of machining operations, being result of mass volume production of components, imposes more restrictive requirements concerning mechanical properties of starting materials, inclusive of machinability mainly. In stage of preparation of material, the machinability is influenced by such factors as chemical composition, structure, mechanical properties, plastic working and heat treatment, as well as a factors present during machining operations, as machining type, cutting parameters, material and geometry of cutting tools, stiffness of the system: workpiece – machine tool – fixture and cutting tool. In the paper are presented investigations concerning machinability of the EN AC-AlSi9Cu3(Fe) silumin put to refining, modification and heat treatment. As the parameter to describe starting condition of the alloy was used its tensile strength Rm. Measurement of the machining properties of the investigated alloy was performed using a reboring method with measurement of cutting force, cutting torque and cutting power. It has been determined an effect of the starting condition of the alloy on its machining properties in terms of the cutting power, being indication of machinability of the investigated alloy. The best machining properties (minimal cutting power - Pc=48,3W) were obtained for the refined alloy, without heat treatment, for which the tensile strength Rm=250 MPa. The worst machinability (maximal cutting power Pc=89,0W) was obtained for the alloy after refining, solutioning at temperature 510 oC for 1,5 hour and aged for 5 hours at temperature 175 oC. A further investigations should be connected with selection of optimal parameters of solutioning and ageing treatments, and with their effect on the starting condition of the alloy in terms of improvement of both mechanical properties of the alloy and its machining properties, taking into consideration obtained surface roughness.
Źródło:
Archives of Foundry Engineering; 2016, 16, 3; 137-140
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies