Tytuł:
Quantitative Analysis of Cryomilled Nanocrystalline Ti-6Al-4V Alloy Powder by X-Ray Diffraction
Autorzy:
Oh, M.
Yu, H. K.
Lee, J.-H.
Oh, M. C.
Jung, S.-H.
Ahn, B.
Powiązania:
https://bibliotekanauki.pl/articles/356265.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
nanocrystalline
cryomilling
Ti alloy
X-ray diffraction
size-strain plot method
Opis:
A nanocrystalline Ti alloy powder was fabricated using cryomilling. The grain size and lattice strain evolution during cryomilling were quantitatively analyzed using X-ray diffraction (XRD) based on the Scherrer equation, Williamson-Hall (W-H) plotting method, and size-strain (S-S) method assuming uniform deformation. Other physical parameters including stress and strain have been calculated. The average crystallite size and the lattice strain evaluated from XRD analysis are in good agreement with the result of transmission electron microscopy (TEM).
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 3; 1439-1442
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Fabrication Of Zn4Sb3 Alloys By A Combination Of Gas-Atomization And Spark Plasma Sintering Processes
Wytwarzanie i konsolidacja proszków stopowych zn4sb3 przez kombinację procesów atomizacji gazowej i spiekania
Autorzy:
Dharmaiah, P.
Kim, H.-S.
Lee, L. H.
Hong, S.-J.
Powiązania:
https://bibliotekanauki.pl/articles/355894.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
gas atomization
microstructure
spark plasma sintering (SPS)
X-ray diffraction
atomizacja gazowa
mikrostruktura
SPS
spiekanie plazmowe
analiza rentgenowska (XRD)
Opis:
In this study, single phase polycrystalline Zn4Sb3 as well as 11 at.% Zn-rich Zn4Sb3 alloy having ε-Zn4Sb3 (majority phase) and Zn (minority phase) phases bulk samples produced by gas-atomization and subsequently consolidated by spark plasma sintering (SPS) process. The crystal structures were analyzed by X-ray diffraction (XRD) and cross-sectional microstructure were observed by the scanning electron microscopy (SEM). The internal grain microstructure of 11at.% Zn-rich Zn4Sb3 powders shows lamellar structure. Relative density, Vickers hardness and crack lengths were measured to investigate the effect of sintering temperature of Zn4Sb3 samples which are sintered at 653, 673 and 693 K. Relative density of the single phase bulk Zn4Sb3 sample reached to 99.2% of its theoretical density. The micro Vickers hardness of three different sintering temperatures were found around 2.17 – 2.236 GPa.
Źródło:
Archives of Metallurgy and Materials; 2015, 60, 2B; 1417-1421
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Surfactant Addition on Bi2Te3 Nanostructures Synthesized by Hydrothermal Method
Autorzy:
Dharmaiah, P.
Lee, C. H.
Madavali, B.
Hong, S.-J.
Powiązania:
https://bibliotekanauki.pl/articles/351609.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
bismuth telluride
hydrothermal synthesis
spark plasma sintering
thermoelectric materials
X-ray diffraction
Opis:
In the present work, we have prepared Bi2Te3 nanostructures with different morphologies such as nano-spherical, nanoplates and nanoflakes obtained using various surfactant additions (EG, PVP, and EDTA) by a hydrothermal method. The shape of the nanoparticles can be controlled by addition of surfactants. The samples were characterized by x-ray diffraction (XRD) and scanning electron microscopy (SEM). It is found that the minority BiOCl phase disappears after maintained pH at 10 with EG as surfactant. SEM bulk microstructure reveals that the sample consists of fine and coarse grains. Temperature dependence of thermoelectric properties of the nanostructured bulk sample was investigated in the range of 300-450K. The presence of nanograins in the bulk sample exhibits a reduction of thermal conductivity and less effect on electrical conductivity. As a result, a figure of merit of the sintered bulk sample reached 0.2 at 400 K. A maximum micro Vickers hardness of 102 Hv was obtained for the nanostructured sample, which was higher than the other reported results.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 2B; 1005-1010
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies