Stress rupture test of MAR-M509 alloy with structure refined by rapid resolidification
Autorzy:
Mróz, M.
Orłowicz, W.
Tupaj, M.
Trytek, A.
Powiązania:
https://bibliotekanauki.pl/articles/380450.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stop MAR M509
mikrostruktura
MAR-M509 alloy
rapid resolidification
microstructure
stress rupture test
Opis:
This study presents results of stress rupture test of MAR-M-509 cobalt alloy samples, as-cast and after surface refining with a concentrated stream of heat. Tests were conducted on samples of MAR-M-509 alloy castings, obtained using the lost-wax method. Casting structure refining was performed with the GTAW method in argon atmosphere, using the current I = 200 A and electrical arc scanning velocity vs = 100, 150, 200 and 250 mm/min. The effect of rapid resolidification of the MAR-M-509 alloy on the microstructure was examined and significant improvement in stress rupture test was observed.
Źródło:
Archives of Foundry Engineering; 2012, 12, 4; 117-120
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Geometry of remeltings and efficiency of the surface remelting process applied to cobalt alloy castings
Autorzy:
Mróz, M.
Orłowicz, W.
Tupaj, M.
Powiązania:
https://bibliotekanauki.pl/articles/381741.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
MAR-M509 alloy
surface remelting
remelting geometry
thermal efficiency
melting efficiency
stop MAR M509
przetapianie powierzchniowe
geometria przetopienia
sprawność cieplna
efektywność topienia
Opis:
The paper summarises results of measurements of remelting area geometry, thermal efficiency and melting efficiency characterising the surface remelting process applied to castings of MAR-M-509 cobalt alloy. The remelting process was carried out with the use of GTAW (Gas Tungsten Arc Welding) method in protective atmosphere of helium, at the electric current intensity in the range from 100 A to 300 A, and the electric arc scanning velocity vs in the range from 200 mm/min to 800 mm/min. The effect of current intensity and electric arc scanning velocity on geometrical parameters of remeltings, thermal efficiency, and melting efficiency characterising the remelting process has been determined.
Źródło:
Archives of Foundry Engineering; 2013, 13, 2; 95-98
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies