Tytuł:
Microstructure and hardness characteristics of Al₂O₃-B₄C particle-reinforced Cu matrix composites
Autorzy:
Öksüz, K.
Şahin, Y.
Powiązania:
https://bibliotekanauki.pl/articles/1155450.pdf
Data publikacji:
2016-04
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
81.05.Ni
81.20.Ev
81.40.Ef
46.55.+d
Opis:
Copper is widely used in industrial applications because of its high electrical and thermal conductivity, easiness of processing and good corrosion resistance. However, copper also has some distinct limitations such as low hardness, low tensile yield strength and poor creep resistance. In this report copper matrix was reinforced with ceramics like Al₂O₃ and B₄C particles using powder metallurgy (PM) method and its microstructure was examined with SEM and EDS. The microstructure has revealed an uniform distribution of particles in the matrix and a good interface bonding between B₄C particles and the matrix. However the dispersion of Al₂O₃ particles, of larger sizes, has led to some porosity and inter-particle contacts in the composites. Therefore, hardness of B₄C particle-reinforced composites is significantly higher than that of Al₂O₃ particle-reinforced composites.
Źródło:
Acta Physica Polonica A; 2016, 129, 4; 650-652
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Spark Plasma Sintering of Boron Carbide Ceramics Using Different Sample Geometries and Dimensions
Autorzy:
Cengiz, M.
Yavas, B.
Celik, Y.
Goller, G.
Yucel, O.
Sahin, F.
Powiązania:
https://bibliotekanauki.pl/articles/1216387.pdf
Data publikacji:
2014-02
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
81.20.Ev
81.05.Je
Opis:
$B_4C$ ceramics were fabricated by spark plasma sintering technique at 1700°C-1800C for 5 min under applied pressure of 50 MPa under vacuum atmosphere. Two different grades of $B_4C$ powder from H.C. Starck Company namely HP grade and HS grade were used in all related experiments. Effect of sample geometry and dimensions as well as sample thickness on sintering parameters were analyzed. Samples having 5 mm thickness and 50 mm diameter, 8 mm thickness in circular geometries and 50 × 50 square cross-section, 8 mm thickness were fabricated. Using the powder, which provided the densest sample, yttrium oxide $(Y_2O_3)$ was added, mixed and sintered. Optimization of SPS method production parameters for pure $B_4C$ samples and $B_4C$ samples with 5 wt% yttrium oxide additive were accomplished. The effect of geometry on density, Vickers hardness, fracture toughness, and microstructure were examined. The hardness and fracture toughness values of the samples were evaluated by the Vickers indentation technique.
Źródło:
Acta Physica Polonica A; 2014, 125, 2; 260-262
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies