Tytuł:
Influence of Cooling Rate on Magnetic Properties of $(Fe_{80}Nb_{6}B_{14})_{1-x}Tb_{x}$ Type of Bulk Nanocrystalline Alloys
Autorzy:
Chrobak, A.
Ziółkowski, G.
Haneczok, G.
Powiązania:
https://bibliotekanauki.pl/articles/1367856.pdf
Data publikacji:
2014-07
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
81.07.Bc
75.50.Tt
75.60.d
76.80.+y
Opis:
The paper refers to magnetic properties of the $(Fe_{80}Nb_{6}B_{14})_{1-x}Tb_{x}$ (x=0.06 and x=0.08) bulk nanocrystalline alloys prepared using the vacuum suction casting technique. The samples were in the form of rods with diameters of d=1.5 mm, 1 mm and 0.5 mm. It was shown that for the alloys with x=0.08 the significant magnetic hardening with the decrease of sample diameter was observed. For d=0.5 mm the coercive field equals 2.46 T and the maximum energy product $|JH|_{max}$=77.2 kJ/$m^{3}$.
Źródło:
Acta Physica Polonica A; 2014, 126, 1; 178-179
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Phase Stability of $(Fe_{80}Nb_{6}B_{14})_{0.9}Tb_{0.1}$ Bulk Nanocrystalline Magnet
Autorzy:
Chrobak, A.
Ziółkowski, G.
Randrianantoandro, N.
Powiązania:
https://bibliotekanauki.pl/articles/1367802.pdf
Data publikacji:
2014-07
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
81.07.Bc
75.50.Tt
75.60.d
76.80.+y
Opis:
The paper refers to phase stability of the $(Fe_{80}Nb_{6}B_{14})_{0.9}Tb_{0.1}$ bulk nanocrystalline alloys prepared using the vacuum suction casting technique. The samples were in the form of rods with diameters d=2, 1.5, 1 and 0.5 mm. Heating up to 900 K reveals structural changes that occur at temperatures above 680 K (DSC and M(T) measurements). The phase analysis, using Mössbauer spectra, indicates the decrease of $Tb_{2}Fe_{14}B$ and increase of Fe content in the samples after the heat treatment. The most stable is the alloy with d=1 mm, where the formation of α-Fe phase was not observed. The decrease of d causes significant hardening i.e. coercive field increases from 0.57 T to 2.66 T for d=2 mm and d=0.5 mm, respectively.
Źródło:
Acta Physica Polonica A; 2014, 126, 1; 176-177
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies