Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "81.10.Jt" wg kryterium: Temat


Wyświetlanie 1-2 z 2
Tytuł:
The Effect of $P_2O_5$ and Heat Treatment on the Crystallization of $Li_2O \cdot 2SiO_2 - BaO \cdot 2SiO_2 (LS_2 - BS_2)$ Glass
Autorzy:
Ertuğ, B.
Demirkesen, E.
Powiązania:
https://bibliotekanauki.pl/articles/1399675.pdf
Data publikacji:
2013-02
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
81.05.Kf
81.10.Jt
61.72.-y
Opis:
In this paper, the effects of $P_2O_5$ and heat treatment on the crystalline phases and microstructure of lithium disilicate-barium disilicate glass were examined. A wider and broad peak in the differential thermal analysis curve indicates a presence of surface crystallization instead of volume crystallization despite the use of nucleating agent, $P_2O_5$. The heat treatment schedules were planned according to differential thermal analysis data. The controlled crystallization of the compositions studied was carried out using two-stage heat treatment procedure. The glass transition temperature, $T_{g}$ of the as-cast sample were used to determine the optimum nucleation temperature. The optimum nucleation temperature was determined to be 520°C. The crystallization was carried out at 720C and 880C for 15 min. Lithium disilicate and sanbornite was the major phases and moganite or coesite were also present depending on the heat treatment duration. Due to coexistence of lithium disilicate and barium disilicate phases, the change in the melting entropy prevented the formation of spherulitic morphology and recrystallization after further heat treatments. The rise in the crystallization temperature enhanced grain coarsening and formed massive microstructures.
Źródło:
Acta Physica Polonica A; 2013, 123, 2; 191-192
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Nanocrystallisation of Soft Magnetic Fe-Co-Zr-Cu-B Alloys
Autorzy:
Wlazłowska, A.
Ferenc, J.
Latuch, J.
Kulik, T.
Powiązania:
https://bibliotekanauki.pl/articles/2035520.pdf
Data publikacji:
2002-08
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
61.43.Dq
75.50.Bb
75.50.Kj
75.60.Ej
81.05.Kf
81.10.Jt
81.70.Ex
81.70.Pg
Opis:
In the present study, Fe$\text{}_{41}$Co$\text{}_{41}$B$\text{}_{10}$Zr$\text{}_{7}$Cu$\text{}_{1}$ alloy has been investigated in order to evaluate its thermal stability and structure after heat treatment, as well as the impact of heat treatment on magnetic properties. X-ray diffractometry, differential scanning calorimetry, chemical composition microanalysis, transmission electron microscopy, and magnetic hysteresis loop measurement techniques were employed. The crystallisation temperature of the as-quenched alloy is 490ºC (continuous heating at 5ºC/min). The melt-spun ribbon having 27μm in thickness was annealed for 1 hour at temperatures from 400 to 700ºC. The alloy after treatment at about 550ºC underwent primary crystallisation, with the average size of crystals under 20 nm. This specimen shows the coercive field of 38 A/m, as compared to about 160 A/m reported for a similar alloy (Fe$\text{}_{44}$Co$\text{}_{44}$B$\text{}_{4}$Zr$\text{}_{7}$Cu$\text{}_{1}$) with a similar structure, annealed at 600ºC.
Źródło:
Acta Physica Polonica A; 2002, 102, 2; 323-328
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies