Tytuł:
Investigation of Fracture Surfaces of Soft Magnetic Materials
Autorzy:
Bidulská, J.
Kvačkaj, T.
Bidulský, R.
Actis Grande, M.
Ferraris, L.
Powiązania:
https://bibliotekanauki.pl/articles/1533971.pdf
Data publikacji:
2010-11
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
75.50.-y
81.20.Ev
81.40.Np
Opis:
The present paper focused on the analysis of the fracture surfaces of a new development insulated iron powder compound with the addition of the aluminium alloy in order to improve the mechanical properties. Results show that in the pressed state, mainly pores act as crack initiators and due to their presence the distribution of stress is inhomogeneous across the cross-section and leads to the reduction of the effective load bearing area. Investigation of fracture surfaces concluded that improvements in bonding during the pressing process and heat treatment can be helpful in the development of soft magnetic materials to give a suitable combination between pressing pressure, annealing temperature and time as well as magnetic properties.
Źródło:
Acta Physica Polonica A; 2010, 118, 5; 800-801
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Analysis of the Fracture Surfaces of New Development Insulated Iron Powder Compounds
Autorzy:
Bidulský, R.
Bidulská, J.
Kvačkaj, T.
Actis Grande, M.
Powiązania:
https://bibliotekanauki.pl/articles/1201089.pdf
Data publikacji:
2014-07
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
75.50.-y
81.20.Ev
81.40.Np
Opis:
Goal of the present paper is the analysis of the fracture surfaces of an Insulated Iron Powder Compound (IIPC) with different additions of aluminium alloy (0.25, 0.5 and 0.75 wt.%), in order to improve the mechanical properties, evaluated as the transverse rupture strength (TRS) with sufficient magnetic properties (mainly represented by the iron loss and coercivity force). Investigation of microstructure and porosity development concluded that improvements in bending strength and impact values require the reduction of surface oxides during the heat treatment, in order to get a proper load bearing area between the adjacent particles.
Źródło:
Acta Physica Polonica A; 2014, 126, 1; 154-155
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies