Tytuł:
An Evaluation of Cu-B₄C Composites Manufactured by Powder Metallurgy
Autorzy:
Yener, T.
Altinsoy, I.
Yener, S.
Celebi Efe, G.
Ozbek, I.
Bindal, C.
Powiązania:
https://bibliotekanauki.pl/articles/1401279.pdf
Data publikacji:
2015-04
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
81.05.Ni
81.20.Ev
72.80.Tm
Opis:
In this study, the influences of B₄C ratios on some mechanical and physical properties such as relative density, microhardness and electrical properties of cold pressed Cu-B₄C composites were investigated. Curve fitting is applied for the estimation of electrical conductivity. Commercial copper powders with 40 μm particle size were reinforced with B₄C, with particle size of 40 μm, at ratios of 1, 2, 3 wt.%, for improving mechanical properties of copper used as electrical conductor. Cu-B₄C composites have been fabricated by powder sintering process at a temperature of 900°C for 2 h. The presence of Cu and B₄C, which are dominant components in the sintered composites, were confirmed by X-ray diffraction analysis technique and SEM-EDS. Scanning electron microscope (SEM-EDS) has shown that B₄C particles are distributed homogenously in the copper matrix. The relative densities of Cu and Cu-B₄C composites, sintered at 900°C, ranged from 95.7 to 91.6%. Microhardness of composites ranged from 84.5 to 94.6 HB. It was observed that cold pressed Cu-1 wt.% B₄C composites revealed promising physical properties. Results of electrical conductivity measurement of Cu-B₄C composite material are compared to the results of the model and the overall accuracy level above 96% is obtained.
Źródło:
Acta Physica Polonica A; 2015, 127, 4; 1045-1047
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Production and characterization of niobium toughened Ti-TiAl₃ metallic-intermetallic composite
Autorzy:
Yener, T.
Zeytin, S.
Powiązania:
https://bibliotekanauki.pl/articles/1054969.pdf
Data publikacji:
2017-09
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
46.50.+a
72.80.Tm
Opis:
Ti-TiAl₃ in situ composites with 10 wt.% Nb were successfully prepared from Ti, Al, and Nb metallic powders by powder metallurgy processing technique of electric current activated/assisted sintering. The current and process time used for producing metallic-intermetallic composites were 2000 A and 90 s, respectively. In terms of fracture toughness, effects of addition of ductile niobium phase to Ti-TiAl₃ composites were investigated. According to SEM-EDS and XRD results, the synthesized composites mainly consisted of TiAl₃ matrix and dispersive Nb reinforcing phases, as well as ductile Ti phases. Hardness and fracture toughness values of the samples were measured by Vickers hardness tester under loads of 100 g and 10 kg, respectively. Fracture toughness value of TiAl₃ intermetallic composites was increased with Nb ductile phase addititon from 1.69± 0.05 MPa m^{1/2} to 5.23± 0.3 MPa m^{1/2}.
Źródło:
Acta Physica Polonica A; 2017, 132, 3; 941-943
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Determination of the Young Modulus of Ti-TiAl₃ Metallic Intermetallic Laminate Composites by Nano-Indentation
Autorzy:
Yener, T.
Güler, S.
Siddique, S.
Walther, F.
Zeytin, S.
Powiązania:
https://bibliotekanauki.pl/articles/1398728.pdf
Data publikacji:
2016-04
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
72.80.Tm
61.82.Bg
68.55.Nq
Opis:
Nano-indentation is an important technique to determine the Young modulus of multiphase materials where normal tensile tests are not appropriate. In this work, Ti-TiAl₃ metallic-intermetallic laminate composites have been fabricated successfully in open atmosphere using commercial purity Al and Ti foils with 250 μm and 500 μm initial thicknesses, respectively. Sintering process was performed at 700°C under 2 MPa pressure for 7.5 h. Mechanical properties including the Young modulus were determined after manufacturing. The Young moduli of metallic and intermetallic phases were determined as 89 GPa and 140 GPa, respectively. Microstructure analyses showed that aluminum foil was almost consumed by forming a titanium aluminide intermetallic compound. Titanium aluminides grow up through spherical shaped islands and metallic-intermetallic interface is a wavy form in Ti-Al system. Thus, the final microstructure consists of alternating layers of intermetallic compound and unreacted Ti metal. Microstructure and phase characterizations were performed by scanning electron microscopy, energy dispersive spectroscopy, and X-ray diffraction. Hardness of test samples was determined as 600 HV for intermetallic zone and 130 HV for metallic zone by the Vickers indentation method.
Źródło:
Acta Physica Polonica A; 2016, 129, 4; 604-606
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies