Tytuł:
Analysis of the Thermal and Magnetic Properties of Amorphous Ribbons of Fe₆₁Co₁₀B₂₀Y₈Me₁ (where Me = W, Zr, Nb, Mo)
Autorzy:
Pietrusiewicz, P.
Nabiałek, M.
Powiązania:
https://bibliotekanauki.pl/articles/1032157.pdf
Data publikacji:
2017-04
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
61.43.Dq
75.50.Kj
65.60.+a
75.30.Gw
Opis:
This paper presents the results pertaining to thermal and magnetic studies of rapidly-cooled samples of the alloy family Fe₆₁Co₁₀B₂₀Y₈Me₁ (where Me = Nb, Zr, W, Mo). The resulting ribbons, or tapes, have amorphous structure. It has been found that the addition of Me elements alters the thermal and magnetic properties. It is noted that the saturation magnetization decreases with increasing number of unpaired electrons on the valence shells. In addition, the value of the coercivity and effective anisotropy have been determined.
Źródło:
Acta Physica Polonica A; 2017, 131, 4; 678-680
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Crystallization Processes of $R_{4.5}Fe_{77}B_{18.5}$ (R = Pr, Nd) Amorphous Alloys
Autorzy:
Musiał, A.
Śniadecki, Z.
Pagnani, D.
Idzikowski, B.
Powiązania:
https://bibliotekanauki.pl/articles/1371300.pdf
Data publikacji:
2014-07
Wydawca:
Polska Akademia Nauk. Instytut Fizyki PAN
Tematy:
61.43.Dq
65.60.+a
75.50.Bb
Opis:
The amorphous alloys $R_{4.5}Fe_{77}B_{18.5}$ (R=Pr, Nd) were prepared by melt-spinning technique under argon atmosphere on a cooper wheel rotating with surface velocity of 25 m·$s^{-1}$. The ribbons have been investigated by means of X-ray diffraction (XRD) and differential scanning calorimetry (DSC). Temperatures of crystallization for $Pr_{4.5}Fe_{77}B_{18.5}$, measured at the heating rate 20 K/min, are equal $T_{x1}$=591°C for the first exothermic effect and $T_{x2}$=603°C for the second one (for $Nd_{4.5}Fe_{77}B_{18.5} T_{x1}$=594°C and $T_{x2}$=633°C). In the amorphous ribbons the crystallization of $Fe_{3}B$ phase in the first step, followed by the crystallization of $Pr_{2}Fe_{23}B_{3}$ and $Nd_{2}Fe_{23}B_{3}$, was observed. Both later phases appear in the process of recrystallization, immediately after $Fe_{3}B$ formation.
Źródło:
Acta Physica Polonica A; 2014, 126, 1; 316-317
0587-4246
1898-794X
Pojawia się w:
Acta Physica Polonica A
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies