Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "turbine blades" wg kryterium: Temat


Wyświetlanie 1-4 z 4
Tytuł:
Modern materials used for environmental barrier coatings – a review
Nowoczesne materiały stosowane na powłoki EBC – przegląd
Autorzy:
Mokrzycka, Magdalena
Jopek, Jakub
Słyś, Anita
Góral, Marek
Ochał, Kamil
Powiązania:
https://bibliotekanauki.pl/articles/41156632.pdf
Data publikacji:
2023
Wydawca:
Wydawnictwo SIGMA-NOT
Tematy:
environmental barrier coatings
high temperature corrosion
oxidation
turbine blades
środowiskowe bariery cieplne
EBC
korozja wysokotemperaturowa
utlenianie
łopatki turbin
Opis:
In this article, the materials used for EBC coatings, representing next stage in the development of heat-resistant layers, and thermal barrier coatings are reviewed. In the introduction, the design of gas turbine is characterized, as well as the materials used for the hot part components and the requirements for protective coatings. Ceramic materials that can be an alternative to currently used nickel superalloys for turbine blades are also described. The requirements for EBC coatings were analyzed and then the various types of EBC coatings were characterized, as well as their degradation mechanisms.
W artykule dokonano krótkiego przeglądu materiałów stosowanych na powłoki EBC (environmental barrier coatings) reprezentujących kolejny etap zaawansowania warstw żaroodpornych i powłokowych barier cieplnych (TBC – thermal barrier coatings). Opisano konstrukcję turbiny gazowej i materiały stosowane do produkcji elementów części gorącej oraz wymagania w zakresie powłok ochronnych. Opisane zostały również materiały ceramiczne, które mogą być alternatywą dla obecnie stosowanych nadstopów niklu używanych do wytwarzania łopatek turbin. Przeprowadzono analizę wymagań dotyczących powłok EBC, a następnie scharakteryzowano poszczególne rodzaje tych powłok, a także mechanizmy ich degradacji.
Źródło:
Ochrona przed Korozją; 2023, 4; 104-112
0473-7733
2449-9501
Pojawia się w:
Ochrona przed Korozją
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Regeneracja warstw aluminidkowych na podłożu nadstopów niklu stosowanych na łopatki silników lotniczych
Selected aspects of aluminide coating regeneration on nickel superalloys used for production of turbine blades
Autorzy:
Kwolek, Przemysław
Góral, Marek
Poznańska, Anna
Wierzbińska, Małgorzata
Ochał, Kamil
Powiązania:
https://bibliotekanauki.pl/articles/945989.pdf
Data publikacji:
2019
Wydawca:
Politechnika Rzeszowska im. Ignacego Łukasiewicza. Oficyna Wydawnicza
Tematy:
warstwa aluminidkowa
regeneracja warstw
rozpuszczanie
łopatki turbin
nadstopy
Inconel 100
aluminide coating
coatings regeneration
dissolution
turbine blades
superalloys
IN-100
Opis:
W artykule przedstawiono wybrane metody usuwania dyfuzyjnych warstw aluminidkowych stosowanych do ochrony powierzchni łopatek turbin silników lotniczych przed oddziaływaniem korozji wysokotemperaturowej. Scharakteryzowano opracowane dotychczas chemiczne i elektrochemiczne metody rozpuszczania warstw aluminidkowych. Na podstawie analizy danych literaturowych wytypowano 3 roztwory: kwasu siarkowego(VI) o stężeniu 25% mas., mieszaninę stężonego kwasu solnego (40% obj.) i etanolu (60% obj.) oraz mieszaninę stężonych kwasów ortofosforowego (50% obj.), octowego (25% obj.), azotowego (25% obj.). Przeprowadzono badania kinetyki rozpuszczania modelowej warstwy aluminidkowej modyfikowanej cyrkonem na podłożu stopu Inconel 100. Wykazano, że niezależnie od zastosowanych roztworów, rozpuszczanie następuje równomiernie na powierzchni warstwy. Stwierdzono, że największą skutecznością w usuwaniu warstw cechowała się mieszanina kwasów: ortofosforowego, octowego i azotowego, w której rozpuszczenie warstwy aluminidkowej następowało po ok. 80 min.
Selected methods of removing diffusion alluminide coating used for protection of turbine blades were presented in the article. The chemical and electrochemical methods of coatings dissolution used in aerospace industry were described. Three selected removing agents were selected for experimental tests: hydrochloric acid in ethanol solution, sulphuric acid in water as well as mixture of orthophosphoric, acetic and nitride acids. The aluminide coating obtained on IN-100 nickel superalloy was used for tests. The conducted research showed that the mixture of orthophosphoric, acetic and nitride acids can dissolve outer-zone of aluminidce coating during 80 min dissolution process. The removing process takes place evenly on the whole surface of sample.
Źródło:
Zeszyty Naukowe Politechniki Rzeszowskiej. Mechanika; 2019, z. 91 [299], 1-2; 53-65
0209-2689
2300-5211
Pojawia się w:
Zeszyty Naukowe Politechniki Rzeszowskiej. Mechanika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The quality assurance of cast and wrought aero jet engine components made from Ni-base superalloys with using of quantitative metallography methods and alloys lifetime prediction
Autorzy:
Belan, Juraj
Kuchariková, Lenka
Mazur, Magdalena
Tillová, Eva
Hanusová, Patrícia
Powiązania:
https://bibliotekanauki.pl/articles/104037.pdf
Data publikacji:
2019
Wydawca:
Stowarzyszenie Menedżerów Jakości i Produkcji
Tematy:
quality assurance
cast Ni-base superalloys
wrought Ni-base superalloys
turbine blades
turbine disc
quantitative metallography
zapewnienie jakości
superstopy na bazie Ni
łopatki turbin
tarcza turbiny
metalografia ilościowa
Opis:
The Ni-base superalloys are used in the aircraft industry for the production of aero engine most stressed parts, turbine blades or turbine discs. Quality of aero jet engine components has a significant influence on the overall lifetime of a jet engine as itself as well as the whole airplane. From this reason a dendrite arm spacing, grain size, morphology, number and value of γ' - phase are very important structural characteristics for blade or discs lifetime prediction. The methods of quantitative metallography are very often used for evaluation of structural characteristics mentioned above. The high-temperature effect on structural characteristics and application of quantitative methods evaluation are presented in this paper. The two different groups of Ni-base alloys have been used as experimental material: cast alloys ZhS6K and IN713LC, which are used for small turbine blades production and wrought alloys EI 698VD and EI 929, which are used for turbine disc production. Selected alloys have been evaluated in the starting stage and after applied heattreatment at 850°C for 24 hrs. This applied heat-treatment causes structural changes in all alloys groups. In cast alloy dendritic structure is degraded and gamma prime average size has grown what has a negative influence on turbine blade creep rupture life. Wrought alloys show partially grain boundary melting and grain size changed due to recrystallization what causes mechanical properties decreasing - ultimate tensile strength mainly.
Źródło:
Quality Production Improvement - QPI; 2019, 1, 1; 222-229
2657-8603
Pojawia się w:
Quality Production Improvement - QPI
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Application of Non-Destructive Methods to Quality Assessment of Pattern Assembly and Ceramic Mould in the Investment Casting Elements of Aircraft Engines
Zastosowanie nieniszczących metod do oceny jakości woskowych zestawów modelowych oraz ceramicznych form w procesie odlewania precyzyjnego elementów silników lotniczych
Autorzy:
Żaba, K.
Nowak, S.
Kwiatkowski, M.
Nowosielski, M.
Kita, P.
Sioma, A.
Powiązania:
https://bibliotekanauki.pl/articles/354370.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
special processes
investment casting
turbine blades
3D scan
thermovision
computed tomography
proces specjalny
odlewanie precyzyjne
łopatki turbin
3D
termowizja
tomografia komputerowa
Opis:
The aim of this paper is manufacturing of turbocharger engine jet blades made of nickel superalloys. Processes for producing molds and casting realized in a production line are special processes. It means that the results are known only after inspection of the finished product. There is lack of the methods and techniques of effective and efficient quality control of the work in stock, above all molds. Therefore, the unknown is the state ceramic mold for the precision casting, which resulting in risk of referral to a defective mold of the casting process and thus give the product does not comply, is eliminated in the final inspection. One method of reducing this risk is particularly thorough monitoring of all parameters of each process and keeping them in the desired operating point. Operating point is a set of parameters of processes. Such monitoring is possible with the commitment to the methods and techniques to automatically, without human intervention, data collection and processing methods appropriate for use in operational control. The paper presents results of research on the attitude to the problem of a special process. This change is the introduction to the process efficient and effective form of quality control tools in the course of its preparation. In this case, the method of photogrammetry, thermal imaging and computed tomography were used. With the infrared camera will be possible to determine the temperature field, the disorder in relation to the pattern indicates the type of defect. Computed tomography and will be used to develop patterns of correlated defects associated with thermal imagers. Photogrammetry is the use of a model set of quality control (comparison of the actual state of the model *.CAD). It also allows the designation of a wall thickness of the mold.
Referat dotyczy procesu wytwarzania łopatek turbosprężarek silników odrzutowych wykonanych z nadstopów niklu. Procesy wytwarzania form i odlewania, realizowane w linii technologicznej są procesami specjalnymi. Oznacza to, że ich wyniki są znane dopiero po kontroli wyrobu gotowego. Brak jest, bowiem metod i technik efektywnej i skutecznej kontroli jakości półproduktu, przede wszystkim formy. Tym samym nieznany jest stan formy przeznaczanej do odlewania, co skutkuje ryzykiem skierowania do procesu odlewania wadliwej formy i tym samym wytworzeniem wyrobu niezgodnego, eliminowanego dopiero podczas końcowej kontroli odbiorczej. Jedną z metod zmniejszania tego typu ryzyka jest szczególnie gruntowne nadzorowanie wszystkich parametrów poszczególnych procesów i utrzymanie ich w wybranym punkcie pracy. Punkt pracy jest zbiorem parametrów realizacji procesów. Takie nadzorowanie jest możliwe w przypadku zaangażowania do tego celu metod i technik automatycznego, bez udziału człowieka, zbierania danych oraz metod właściwego ich przetwarzania na użytek operacyjnego sterowania. W artykule przedstawiono wyniki badań nad zmianą podejścia do problemu procesu specjalnego. Zmiana ta polega na wprowadzeniu do procesu efektywnych i skutecznych narzędzi kontroli jakosci formy w trakcie jej wytwarzania. W tym celu wykorzystano metody fotogrametrii, termowizji oraz tomografii komputerowej. Dzięki zastosowaniu kamery termowizyjnej możliwe będzie określenie pola temperatury, którego zaburzenie w stosunku do wzorca wskaże na rodzaj wady. Tomografia komputerowa natomiast będzie służyła do opracowania wzorców wad skorelowanych z obrazami termowizyjnymi. Fotogrametria znajduje natomiast zastosowanie w kontroli jakości zestawu modelowego (porównanie rzeczywistego stanu z modelem *.CAD). Umożliwia także wyznaczenie grubości ścianki formy.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 4; 1517-1525
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-4 z 4

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies