Tytuł:
Assessment of gold with titanium alloy weldability in conditions of a dental technique laboratory
Autorzy:
Jania, G.
Żmudzki, J.
Topolska, S.
Powiązania:
https://bibliotekanauki.pl/articles/24200598.pdf
Data publikacji:
2022
Wydawca:
Stowarzyszenie Komputerowej Nauki o Materiałach i Inżynierii Powierzchni w Gliwicach
Tematy:
titanium alloy
gold
laser welding
prosthetic
implant denture
microstructure
stop tytanu
złoto
spawanie laserowe
protetyka
proteza implantu
mikrostruktura
Opis:
Purpose: In dental practice, there is necessary to weld gold with titanium under the conditions of a dental technique laboratory, which is difficult. The aim was to assess the weldability of pure gold with the titanium alloy Ti6Al4V using a prosthetic laser welding machine. Design/methodology/approach: Gold wire in a diameter of 0.4 mm made with the use of a jewellery drawbar (GOLDPORT, Szczecin, Poland) was welded to a titanium alloy Ti6Al4V substrate of dental implant abutment screw (MegaGen). Dental laser welding parameters (Bego Laser Star T plus) were 230 V; 6.5 ms; 2.5 Hz; laser spot 0.3 mm, and argon blow. Samples were included in resin, ground (500-4000 SiC), polished (Al2O3 suspension) and etched (Kroll solution) per 20 s before observation under a light microscope. Findings: There were well-welded and poorly joined zones. The discontinuities and voids there were not visible or sparse next to the initial weld point. Dendritic structure at well-welded remelting zones and two-phase microstructure of titanium and Ti3Au phase were found. The heat-affected zone was about of 20 microns. Research limitations/implications: Light microscopy was used, and precise phase identification required further investigations. Weld strength assessment requires further micro-hardness and load-bearing ability tests. Weldability concerns the model system with pure gold. Practical implications: In the case of elements with dimensions below 0.4 mm, the use of a laser with a smaller spot should be considered for better control of the remelting zone and mechanical positioning of the elements in order to stabilize and avoid discontinuities and voids. Originality/value: Prosthetic laser welding with a laser spot about of 0.3 mm allows to obtain well-welded parts of 0.3 mm in diameter under stable stitching conditions and higher than 0.4 mm in dimensions.
Źródło:
Archives of Materials Science and Engineering; 2022, 118, 1; 36--41
1897-2764
Pojawia się w:
Archives of Materials Science and Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Impact of pouring temperature on the mechanical properties of Al5.9Cu1.9Mg alloy
Autorzy:
Akhyar, Akhyar
Iswanto, P.T.
Malau, V.
Powiązania:
https://bibliotekanauki.pl/articles/2201133.pdf
Data publikacji:
2022
Wydawca:
Stowarzyszenie Komputerowej Nauki o Materiałach i Inżynierii Powierzchni w Gliwicach
Tematy:
mechanical properties
Al-Cu-Mg alloy
casting metal
pouring temperature
właściwości mechaniczne
Stop Al-Cu-Mg
metal odlewniczy
temperatura odlewania
Opis:
Purpose: This experiment aims to determine the influence of pouring temperature on the hardness, impact energy, tensile strength, and changes in the microstructure of the Al-5.9Cu- 1.9Mg alloy. Design/methodology/approach: A total of three samples of aluminium alloy were heated to 688, 738, and 788°C, and poured into permanent moulds in form of plates at a constant temperature of 220°C. The cast products are machined according to testing standards for hardness, impact tests, and tensile strength. Findings: The results showed that the metal hardness and impact energy increased to 103 BHN and 7.48 J at 788°C, respectively, while the tensile strength rises as the temperatures decreases. Furthermore, the changes in the microstructure were affected, which indicated that all the properties of the aluminium alloy were influenced by the variations in temperature. Research limitations/implications: During the metal casting process, only three different pouring temperatures affected the properties of the metal alloy, therefore, there is a need for more variations. Practical implications: The proposed pouring temperature parameter is an important condition for industrial foundry applications to obtain the right product for use in a machining element. Originality/value: This research shows the influence of the difference in pouring temperatures on the properties of metal alloys due to casting, where they will be adapted for a particular use.
Źródło:
Archives of Materials Science and Engineering; 2022, 113, 2; 49--55
1897-2764
Pojawia się w:
Archives of Materials Science and Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The effect of the modification by ultrafine silicon carbide powder on the structure and properties of the Al-Si alloy
Autorzy:
Kovbasiuk, T. M.
Selivorstov, V. Yu.
Dotsenko, Yu. V.
Duriagina, Z. A.
Kulyk, V. V.
Kasai, O. M.
Voitovych, V. V.
Powiązania:
https://bibliotekanauki.pl/articles/1818500.pdf
Data publikacji:
2020
Wydawca:
Stowarzyszenie Komputerowej Nauki o Materiałach i Inżynierii Powierzchni w Gliwicach
Tematy:
Al-Si alloy
silicon carbide
modification
mechanical properties
microstructure
microhardness
Stop Al-Si
węglik krzemu
modyfikacja
właściwości mechaniczne
mikrostruktura
mikrotwardość
Opis:
Purpose: Determine the possibility of modifying aluminium alloys of the Al-Si system with an ultrafine SiC modifier with a particie size of 3-5 pm. Design/methodology/approach: Processing of the Al-Si alloy was carried out by introducing an ultrafine modifier in the amount of 0.1, 0.2, or 0.3 wt.%. Silicon carbide (SiC) with a particle size in the range of 3-5 pm was used as a modifier. To study the microstructure of the formed surface layers, a metallographic analysis was performed according to the standard method on a microscope MIKPOTEX® MMT-14C using TopView software. Microhardness studies of the samples were carried out on a Vickers microhardness tester NOVOTEST TC-MKV1. The microstructure of castings of the AlSi12 grade was studied at magnification from 100 to 400 times on the horizontal and vertical surfaces of the samples after etching with a 2% NaOH aqueous solution. Findings: Aluminium cast alloy of Al-Si system has been synthesized with the addition of 0.1, 0.2, and 0.3 wt.% ultrafine SiC modifier. It was found that the modification of the AlSi12 alloy by SiC particles of 3-5 pm in size led to an improvement of its microstructure due to the reduction of the volume fraction of micropores and primary Si crystals. It was shown that the AlSi12 aluminium alloy due to the modification by 0.2 wt.% SiC has the best micromechanical properties and macrostructure density. Research limitations/implications: The obtained research results are relevant for cast specimens of the indicated sizes and shapes. The studies did not take into account the influence of the scale factor of the castings. Practical implications: The developed modification technology was recommended for use in the conditions of the foundry "Dnipropetrovsk Aggregate Plant" (Dnipro, Ukraine). Originality/value: The technology of AlSi12 alloy modification of ultrafine SIC modifier with a particle size of 3-5 pm was used for the first time.
Źródło:
Archives of Materials Science and Engineering; 2020, 101, 2; 57--62
1897-2764
Pojawia się w:
Archives of Materials Science and Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The effect of thermal treatment of the melt before crystallization on the structure and properties of castings
Autorzy:
Kondratyuk, S. Ye.
Veis, V. I.
Parkhomchuk, Z. V.
Powiązania:
https://bibliotekanauki.pl/articles/1818512.pdf
Data publikacji:
2020
Wydawca:
Stowarzyszenie Komputerowej Nauki o Materiałach i Inżynierii Powierzchni w Gliwicach
Tematy:
steel
aluminium alloy
isothermal treatment
crystallization
heredity of structure
mechanical properties
stal
stop aluminium
obróbka izotermiczna
krystalizacja
dziedziczność struktury
właściwości mechaniczne
Opis:
Purpose: The aim of the proposed research is to investigate the influence of temperature and duration of isothermal melt processing on structural characteristics of castings in connection with technological background of charge metal. Design/methodology/approach: Ferrous and non-ferrous alloys were obtained by remelting a charge with a dispersion-structured structure (which was ensured by high- speed crystallization). Remelting was carried out at different temperatures of overheating of the melt over the liquidus with different isothermal exposure at these temperatures. Experimental castings were crystallized under normal conditions. It was studied a change of structure formation and mechanical characteristics depending on the temperature and duration of thermal treatment of the melt before crystallization. Findings: It is established that isothermal treatment of the melt at the overheating of the liquid metal above a certain equilibrium temperature of the micro-inhomogeneous melt (Te) causes a gradual loss of hereditary characteristics of the original charge metal, increase of the chemical homogeneity of the melt and the formation of crystallization and formation a corresponding change in the mechanical properties of castings. Research limitations/implications: The results can be complemented by studies of the effect of thermal treatment in the temperature range of crystallization. Practical implications: The results can be used to select the optimal heat treatment during remelting and, accordingly, the mechanical properties of the resulting casting. Originality/value: The obtained results testify to the predominant influence of temperature on the dispersion of the cast structure of steels, given the duration of technological operations of preparation and casting of steels in the manufacture of castings in industrial conditions.
Źródło:
Archives of Materials Science and Engineering; 2020, 104, 1; 23--29
1897-2764
Pojawia się w:
Archives of Materials Science and Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-4 z 4

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies