Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "high-temperature corrosion" wg kryterium: Temat


Wyświetlanie 1-3 z 3
Tytuł:
High-temperature oxidation of cast steel in water vapour
Wysokotemperaturowe utlenianie staliwa w parze wodnej
Autorzy:
Zapała, R.
Pach, S.
Górny, M.
Homa, M.
Siewiorek, A.
Powiązania:
https://bibliotekanauki.pl/articles/391690.pdf
Data publikacji:
2015
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Odlewnictwa
Tematy:
cast heat-resistant steel
microstructure
high-temperature corrosion
water vapour
staliwo żaroodporne
mikrostruktura
korozja wysokotemperaturowa
para wodna
Opis:
The article presents the results of studies of the oxidation process conducted at 900°C for 12 hours in an atmosphere of water vapour on cast heat-resistant steel with a diversified structure (ferritic-austenitic, austenitic, and austenitic with carbides). Based on the studies of oxidation kinetics, it was found that samples were oxidized in approximation with the rules of linear law. Depending on the chemical composition and structure of tested alloys, the scale formed on the alloy surface had different properties. In the tested material characterised by a ferritic-austenitic structure, the tendency of the scale to detach from the surface of the metallic substrate was observed. It was probably due to different coefficients of the thermal expansion of austenite and ferrite.
Praca prezentuje wyniki badań utleniania w atmosferze pary wodnej staliwa żaroodpornego o różnej strukturze (ferrytyczno-austenitycznej, austenitycznej i austenitycznej z węglikami) w temperaturze 900°C w ciągu 12 godzin. Na podstawie badań kinetyki utleniania stwierdzono, że badane próbki utleniały się w przybliżeniu zgodnie z prawem liniowym. W zależności od składu chemicznego i struktury badanych stopów obserwowano odmienne właściwości powstałych zgorzelin. W przypadku materiału o strukturze ferrytyczno-austenitycznej stwierdzono odpadanie zgorzeliny od powierzchni rdzenia metalicznego związane prawdopodobnie z różnym współczynnikiem rozszerzalności cieplnej austenitu i ferrytu.
Źródło:
Prace Instytutu Odlewnictwa; 2015, T. 55, nr 3, 3; 61-70
1899-2439
Pojawia się w:
Prace Instytutu Odlewnictwa
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Wysokotemperaturowa korozja materiałów w parze wodnej w sektorze energetycznym
High temperature performance of materials for the energy sector exposed to water steam
Autorzy:
Dudziak, T.
Powiązania:
https://bibliotekanauki.pl/articles/391674.pdf
Data publikacji:
2014
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Odlewnictwa
Tematy:
korozja wysokotemperaturowa
blok energetyczny
stopy żelaza z chromem
stop niklu
high temperature corrosion
power unit
Fe-based alloys with Cr content
Ni based alloy
Opis:
W artykule opisano zagadnienia związane z polskim sektorem energetycznym, w którym decydującą rolę odgrywa technologia subkrytyczna, w której spalanie węgla odbywa się w zakresie temperatur 500−530°C i przy ciśnieniu 14−16 MPa. Ponadto przedstawiono mechanizm korozji materiałów na bazie żelaza i niklu, zawierających różne ilości chromu, przeznaczonych na budowę nowych bloków energetycznych. Z przeprowadzonych badań w wysokich temperaturach (675°C oraz 725°C) w atmosferze czystej pary wodnej, wynika, iż stopy żelaza z dużą zawartością (18% wag.) chromu tworzą spinel Fe-Cr, który ma gorsze właściwości ochronne niż tlenek Cr2O3, lecz jest bardziej ochronny niż magnetyt (Fe3O4) czy też hematyt (Fe2O3). Stwierdzono również, że stopy żelaza charakteryzowały się powstawaniem wysepek bogatych w magnetyt Fe3O4. Powstawanie takich miejsc jest związane z różnym stężeniem żelaza w osnowie stopu i jego aktywnością, a także niską koncentracją chromu i brakiem możliwości stworzenia ochronnej cienkiej warstwy spinelu czy też samodzielnej warstwy Cr2O3. Stop na bazie niklu IN718+ wytworzył warstewkę spinelu Ni-Cr (NiCr2O4), jego zgorzelina nie przekraczała 2 μm grubości.
In this work, issues regarding the energy sector in Poland are described in terms of subcritical technology which is commonly used and plays the most important role in electric power production. In such technology steam temperature reaches 500−530°C with 14−16 MPa pressure. In addition, in this study the mechanism of high temperature corrosion of Fe and Ni- based materials with a different content of Cr considered for construction of new coal power plants will be discussed. The study clearly shows that at high temperatures (675°C and 725°C) in a pure steam atmosphere the Fe based alloy with 18 wt.% of Cr creates the formation of Fe-Cr spinel, the phase indicates poorer corrosion resistance than Cr2O3, however better than magnetite (Fe3O4) or hematite (Fe2O3). It was also shown that Fe based alloys were characterised by the development of islands rich in Fe3O4. The formation of such islands is related to an unequal distribution of iron concentration and its activity within the matrix, and the inability to create a thin protective layer of spinel or an independent layer of Cr2O3. The Ni based alloy 718+ developed a layer of Ni-Cr spinel (NiCr2O4) with a thickness of 2 μm.
Źródło:
Prace Instytutu Odlewnictwa; 2014, T. 54, nr 3, 3; 43-57
1899-2439
Pojawia się w:
Prace Instytutu Odlewnictwa
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
High temperature corrosion of low alloyed steel in air and salt mist atmospheres
Korozja wysokotemperaturowa niskostopowych stali wygrzewanych w powietrzu i atmosferze mgły solnej
Autorzy:
Dudziak, T.
Jura, K.
Powiązania:
https://bibliotekanauki.pl/articles/391785.pdf
Data publikacji:
2016
Wydawca:
Sieć Badawcza Łukasiewicz - Instytut Odlewnictwa
Tematy:
air oxidation
salt mist corrosion
high temperature
utlenianie w powietrzu
mgła solna
wysoka temperatura
Opis:
The aim of this work has been to show the influence of air oxidation and salt mist corrosion on the behaviour of low alloyed steels 18K (K18), 16M (16Mo3), 15HM (13CrMo4-4) and finally 10CrMo9-10 (10H2M) employed in the Polish energy sector. The exposures have been carried out at 450°C, 500°C, and finally 550°C for 500 hours. The obtained results indicate that in both atmospheres, the exposed steels developed similar phases containing Fe3O4 (magnetite) and Fe2O3 (hematite). The scale thicknesses developed under both corrosion conditions have indicated similar values. On the other hand, the addition of 1% NaCl – 1% Na2SO4 to deionised water generates the development of layered structures on low-alloyed steels with different Fe2O3 and Fe3O4 ratio, the effect originates most probably from the presence of S and Cl within the oxide scale. The presence of layers with different phase ratio generates the formation of stresses originating from different coefficients of thermal expansion (CTE) between the phases (Fe2O3, Fe3O4) and between the layers themselves.
W artykule opisano zagadnienia związane z korozją wysokotemperaturową stali niskostopowych 18K (K18), 16M (16Mo3), 15HM (13CrMo4-4) oraz 10CrMo9-10 (10H2M), które są często stosowane w polskim sektorze energetycznym. Testy wysokotemperaturowe zostały wykonane w temperaturach 450°C, 500°C i 550°C przez okres 500 godzin. Otrzymane wyniki pokazują, iż w dwóch różnych atmosferach korozyjnych, stale niskostopowe wytworzyły takie same fazy, głównie Fe2O3 (hematyt) oraz Fe3O4 (magnetyt) z tą różnicą, iż w atmosferze mgły solnej zawierającej 1% NaCl – 1% Na2SO4 zgorzelina tlenkowa miała charakter warstwowy. Charakter ten prawdopodobnie zawdzięczany jest obecności S i Cl wewnątrz zgorzeliny tlenkowej, co więcej warstwy różnią się zwartością Fe2O3 oraz Fe3O4, co powoduje powstawanie naprężeń, tendencje do odpadania z powodu różnych wartości współczynnika rozszerzalności cieplnej między fazami Fe2O3 oraz Fe3O4, a także między warstwami.
Źródło:
Prace Instytutu Odlewnictwa; 2016, 56, 2; 77-85
1899-2439
Pojawia się w:
Prace Instytutu Odlewnictwa
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies