Setting Time and after Setting Properties of High Calcium Fly Ash Geopolymers with Different Concentration of Sodium Hydroxide
Autorzy:
Mohamed, Rosnita
Razak, Rafiza Abd
Abdullah, Mohd Mustafa Al Bakri
Sofri, Liyana Ahmad
Aziz, Ikmal Hakem
Shahedan, Noor Fifinatasha
Powiązania:
https://bibliotekanauki.pl/articles/2106582.pdf
Data publikacji:
2022
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
high calcium fly ash geopolymers
setting time
heat evolved
early age properties
concentration of sodium hydroxide
Opis:
Setting time in geopolymers is known as the time taken for the transition phase of liquid to solid of the geopolymer system in which is represented in the initial setting and final setting. Setting time is significant specifically for application in the construction field. This study intends to determine the setting time of high calcium fly ash geopolymers and the properties of the geopolymers after setting (1-day age). This includes the determination of heat evolved throughout geopolymerization using Differential Scanning Calorimeter. After setting properties determination includes compressive strength and morphology analysis at 1-day age. High calcium fly ash was used as geopolymer precursor. Meanwhile, for mixing design, the alkali activator was a mixture of sodium silicate and sodium hydroxide (concentration varied from 6M-14M) with a ratio of 2.5 and a solid-to-liquid ratio of 2.5. From this study, it was found that high calcium fly ash geopolymer with 12M of NaOH has a reasonable setting time which is suitable for on-site application as well as an optimal heat evolved (-212 J/g) which leads to the highest compressive strength at 1-day age and no formation of microcracks observed on the morphology. Beyond 12M, too much heat evolved in the geopolymer system can cause micro-cracks formation thus lowering the compressive strength at 1-day age.
Źródło:
Archives of Metallurgy and Materials; 2022, 67, 2; 563--567
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies