Tytuł:
Manufacturing of Porous Al-Cr Preforms for Composite Reinforcing Using Microwave Activated Combustion Synthesis
Wytwarzanie porowatych preform Al-Cr do umacniania kompozytów poprzez syntezę spaleniową aktywowaną mikrofalami
Autorzy:
Naplocha, K.
Granat, K.
Powiązania:
https://bibliotekanauki.pl/articles/353758.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
SHS
microwave
Al-Cr
preform
composite
mikrofale
preforma
kompozyt
Opis:
The combustion synthesis of porous skeletons (preforms) of intermetallic Al–Cr compounds intended for metal matrix composite MMC reinforcing was developed. Mixture of Al and Cr powders with granularity of −10, −44, −74mm were cold isostatic pressed and next ignited and synthetized in a microwave reactor under argon atmosphere (microwave-activated combustion synthesis MACS). In order to ignite the synthesis, microwave energy was focused by a tuner on the specimen. The analysis of reaction temperature diagrams revealed that the synthesis proceeded through the following peritectic transformations: L(liquidus)+Al7Cr→L+Al11Cr2→L+Al4Cr. Moreover, EDS and XRD examinations showed that the reaction proceeded between a solid Cr and a liquid Al to create a distinct envelope of Al9Cr4 on Cr particle which next extended and spreaded over the entire structure. The produced preforms with uniform structure and interconnected porosity were infiltrated with liquid Cu and Al alloy. The obtained composite materials exhibited high hardness, wear and distinct temperature oxidation resistance.
Wytworzono poprzez syntezę spaleniową porowate preformy (szkielety) ze związków międzymetalicznych Al-Cr do umacniania materiałów kompozytowych o osnowie metalowej. Sprasowane na zimno, jednoosiowo (CIP) mieszaniny proszków Al i Cr o ziarnistości −10, −44, −74mm podgrzewano w reaktorze mikrofalowym w atmosferze argonu. W celu zainicjowania syntezy wykorzystano proces aktywacji mikrofalami MACS (microwave-activated combustion synthesis) skupiając promieniowanie na powierzchni próbki za pomocą stroika falowodowego. Na podstawie analizy krzywych temperatur ATD określono przebieg syntezy z następującymi przemianami perytektycznymi:: L(liquidus)+Al7Cr→L+Al11Cr2→L+Al4Cr. Ponadto, analiza chemiczna EDS oraz fazowa XRD wykazały, że reakcja przebiega pomiędzy proszkiem Cr oraz ciekłym Al tworząc wyraźną otoczkę ze związku Al9Cr4 na cząstkach Cr, które z postępem reakcji rozszerzają się i zanikają. Wytworzone preformy o jednorodnej strukturze z otwartymi porowatościami użyto do infiltracji ciekłym Al oraz Cu i wytworzenia kompozytów. Charakteryzowały się one dużą twardością, odpornością na ścieranie oraz odpornością na utlenianie w wysokiej temperaturze.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 3; 1125-1127
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Manufacturing of Al Alloy Matrix Composite Materials Reinforced with MAX Phases
Autorzy:
Dmitruk, A.
Naplocha, K.
Powiązania:
https://bibliotekanauki.pl/articles/382950.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
MAX phase
SHS synthesis
microwave
porous structure
squeeze casting
faza MAX
synteza SHS
mikrofala
struktura porowata
Opis:
A method for manufacturing of Al-Si alloy (EN AC-44200) matrix composite materials reinforced with MAX type phases in Ti-Al-C systems was developed. The MAX phases were synthesized using the Self-propagating High-Temperature Synthesis (SHS) method in its microwave assisted mode to allow Ti2AlC and Ti3AlC2 to be created in the form of spatial structures with open porosity. Obtained structures were subjected to the squeeze casting infiltration in order to create a composite material. Microstructures of the produced materials were observed by the means of optical and SEM microscopies. The applied infiltration process allows forming of homogeneous materials with a negligible residual porosity. The obtained composite materials possess no visible defects or discontinuities in the structure, which could fundamentally deteriorate their performance and mechanical properties. The produced composites, together with the reference sample of a sole matrix material, were subjected to mechanical properties tests: nanohardness or hardness (HV) and instrumental modulus of longitudinal elasticity (EIT).
Źródło:
Archives of Foundry Engineering; 2018, 18, 2; 198-202
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Własności trybologiczne materiałów kompozytowych na osnowie stopu aluminium 7075 umacnianych włóknami Al2O3
Tribological properties of Al 7075 alloy based composites strengthened with Al2O3 fibres
Autorzy:
Naplocha, K.
Kaczmar, J. W.
Powiązania:
https://bibliotekanauki.pl/articles/381055.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
materiał kompozytowy
stop 7075
włókno AI2O3
tarcie suche
composite material
7075 alloy
Al2O3 fibre
dry sliding
Opis:
Badano odporność na zużycie ścierne materiałów kompozytowych na osnowie stopu aluminium 7075 umacnianych włóknami Al2O3 Saffil. Pomiary przeprowadzono metodą pin-on-disc w warunkach tarcia suchego dociskając próbki do obracającej się żeliwnej tarczy. Określono wpływ ciśnienia wywieranego przez próbki oraz ukierunkowania włókien, w stosunku do powierzchni ścieranej na stopień zużycia. Materiały wytwarzano metodą prasowania w stanie ciekłym nasycając stopem aluminium 7075 kształtki ceramiczne z włókien Saffil o porowatości 80-90%. Odporność na zużycie materiałów kompozytowych, w stosunku do nieumocnionego stopu 7075, była nieznacznie gorsza przy mniejszym ciśnieniu 0,8MPa wywieranym przez próbkę z kompozytu na żeliwną tarczę. Pod większym ciśnieniem 1,2 MPa odporność stopu nieumocnionego była jeszcze lepsza, a ukierunkowanie włókien w materiałach kompozytowych nie miało większego znaczenia na zużycie. Zaobserwowano również znaczne zużycie przeciwpróbki, gdyż zużyty materiał kompozytowy wraz z rozdrobnionymi włóknami Al2O3 pełnił rolę ścierniwa. Wzrost odporności na ścieranie materiałów kompozytowych na osnowie stopu 7075 uzyskano po zastosowaniu umocnienia zawierającego oprócz włókien Al2O3 również włókna C.
Wear resistance of 7075 aluminium alloy based composite materials reinforced with Al2O3 Saffil fibres was investigated. The measurements of wear were performed applying the pin-on-disc method at dry friction conditions with the gray iron counterpart. The effects of pressure of composite samples on the counterpart made of gray iron and the orientation of fibers in relation to the friction surface on wear rate were determined. The materials were produced by squeeze casting method where 80-90% porous ceramic preform were infiltrated. After T6 heat treatment hardness increased about 50-60% both for unreinforced alloy and composites containing strengthening Saffil fibres. Wear resistance of composite materials in relation to the unreinforced 7075 alloy was slightly worse at lower pressure of 0.8 MPa. Under higher pressure of 1.2 MPa wear resistance of unreinforced 7075 alloy was even better whereas no effect of orientation of fibers on wear in composite materials was observed. Additionally, significant wear of counterface in the presence of debris with fragmented Al2O3 fibres as abrasives was observed. Wear resistance improvement of composite materials was obtained when with alumina Saffil fibres Carbon C fibres in the preforms were applied.
Źródło:
Archives of Foundry Engineering; 2011, 11, 2 spec.; 153-158
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Processing of Porous NiTi Preforms for NiTi/Mg Composites
Autorzy:
Kucharczyk, A.
Naplocha, K.
Tomanik, M.
Powiązania:
https://bibliotekanauki.pl/articles/352563.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
metal matrix composite
magnesium
nitinol
SHS
squeeze casting
Opis:
NiTi alloys are successfully used in engineering and medical applications because of their properties, such as shape memory effect, superelasticity or mechanical strength. A composite with Mg matrix, due to its vibration damping properties, can be characterized by low weight and good vibration damping properties. In this study, a combination of two techniques was used for successful fabrication of Mg composite reinforced by NiTi alloy preform. The porous preforms synthesized by Self-propagating Hightemperature Synthesis (SHS) from elemental powders were subsequently infiltrated with Mg by squeeze casting. The effects were examined with scanning electron microscope with EDS detector, X-ray diffraction and microindentation. The inspection has shown well-connected matrix and reinforcement; no reaction at the interface and open porosities fully infiltrated by liquid Mg. Moreover, analysis of samples’ fracture has exhibited that crack propagates inside the Mg matrix and there is no detachment of reinforcement.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 2; 747-752
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
A Comparative Study of the Feasibility of Cellular MAX Phase Preforms Formation by Microwave-Assisted SHS and SPS Techniques
Autorzy:
Dmitruk, A.
Lagos, M.
Naplocha, K.
Egizabal, P.
Powiązania:
https://bibliotekanauki.pl/articles/352206.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
MAX phases
SHS synthesis
microwave
SPS
porous preform
Opis:
Two methods were evaluated in terms of manufacturing of MAX phase preforms characterized with open porosity: microwave-assisted self-propagating high-temperature synthesis (SHS) and spark plasma sintering (SPS). The main purpose of fabrication of such open-porous preforms is that they can be successfully applied as a reinforcement in metal matrix composite (MMC) materials. In order to simulate the most similar conditions to microwave-assisted SHS, the sintering time of SPS was significantly reduced and the pressure was maintained at a minimum value. The chosen approach allows these two methods to be compared in terms of structure homogeneity, complete reactive charge conversion and energy effectivity. Study was performed in Ti-Al-C system, in which the samples were compacted from elemental powders of Ti, Al, C in molar ratio of 2:1:1. Manufactured materials after syntheses were subjected to SEM, XRD and STEM analyses in order to investigate their microstructures and chemical compositions. As was concluded, only microwave-assisted SHS synthesis allows the creation of MAX phases in the studied system. SPS technique led only to the formation of intermetallic secondary phases. The fabrication of MAX phases’ foams by microwave-assisted SHS presents some interesting advantages compared to conventional manufacturing methods. This work presents the characterization of foams obtained by microwave-assisted SHS comparing the results with materials produced by SPS. The analysis of SPS products for different sintering temperatures provided the better insight into the synthesis of MAX phases, supporting the established mechanism. Dissimilarities in the heating mechanisms that lead to the differing synthesis products were also discussed.
Źródło:
Archives of Metallurgy and Materials; 2020, 65, 2; 575-582
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Design of Honeycomb Structures Produced by Investment Casting
Autorzy:
Naplocha, K.
Dmitruk, A.
Mayer, P.
Kaczmar, J. W.
Powiązania:
https://bibliotekanauki.pl/articles/382969.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
investment casting
3D printing
honeycomb design
light structure
odlewnie
drukowanie 3d
projekt plaster miodu
plaster miodu
lekkie konstrukcje
Opis:
Investment casting combined with the additive manufacturing technology enables production of the thin-walled elements, that are geometrically complex, precise and can be easy commercialized. This paper presents design of aluminium alloy honeycombs, which are characterized with light structure, internal parallel oriented channels and suitable stiffness. Based on 3D printed pattern the mould was prepared from standard ceramic material subjected subsequently to appropriate heat treatment. Into created mould cavity with intricate and susceptible structure molten AC 44200 aluminium alloy was poured under low pressure. Properly designed gating system and selected process parameters enabled to limit the shrinkage voids, porosities and misruns. Compression examination performed in two directions showed different mechanisms of cell deformation. Characteristic plateau region of stress-strain curves allowed to determine absorbed energy per unit volume, which was 485 or 402 J/mm3 depending on load direction. Elaborated technology will be applied for the production of honeycomb based elements designated for energy absorption capability.
Źródło:
Archives of Foundry Engineering; 2019, 4; 76-80
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Enhancement of Heat Transfer in PCM by Cellular Zn-Al Structure
Autorzy:
Naplocha, K.
Koniuszewska, A.
Lichota, J.
Kaczmar, J. W.
Powiązania:
https://bibliotekanauki.pl/articles/382339.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
innovative foundry technology
innovative foundry material
metal cellular foam
porous Zn-Al structure
investment casting
heat transfer
innowacyjna technologia odlewnicza
innowacyjny materiał odlewniczy
pianka metalowa
struktura porowata Zn-Al
odlewanie precyzyjne
wymiana ciepła
Opis:
Development of open cellular metal foam technology based on investment casting applying the polyurethane pattern is discussed. Technological process comprises preparing of the ceramic mold applying PUR foam as the pattern, firing of the mold, pouring of the liquid Zn-Al alloy into the mold and washing out of the ceramic material from cellular casting. Critical parameters such as the temperature of mold and poured metal, design of gating system affected by metalostatic pressure allowed to produce castings with cellular structure characterized by the open porosity. Metal cellular foams with the open porosity embedded in phase change material (PCM) enhance heat transfer and reduce time operations in energy storage systems. Charging and discharging were performed at the laboratory accumulator by heating and cooling with flowing water characterized by the temperatures of 97-100ºC. Temperature measurements were collected from 7 different thermocouples located in the accumulator. In relation to the tests with pure paraffin, embedding of the metal Zn-Al cellular foam in paraffin significantly decreases temperature gradients and melting time of paraffin applied as PCM characterized by the low thermal conductivity. Similarly, reduction of discharging time by this method improves the efficiency of thermal energy storage system applied in solar power plants or for the systems of energy efficient buildings.
Źródło:
Archives of Foundry Engineering; 2016, 16, 4; 91-94
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Production and wear properties of copper based MMC strengthened with δ-alumina fibres
Wytwarzanie oraz własności tribologiczne materiałów kompozytowych na osnowie miedzi umocnionej włóknami tlenku aluminium
Autorzy:
Granat, K.
Pietrzak, K.
Grodzka, E.
Naplocha, K.
Kaczmar, J. W.
Powiązania:
https://bibliotekanauki.pl/articles/382379.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
metal matrix composite
copper alloy
alumina fibre
squeeze casting
wear resistance
kompozyty o osnowie metalowej
włókna tlenku glinu
infiltracja ciśnieniowa
zużycie ścierne
Opis:
The investigation was carried out on the production by pressure infiltration (squeeze casting) of metal matrix composite materials based on pure Cu-ETP copper containing δ-alumina SAFFIL fibres The microstructure of composite specimens and morphology was examined using SEM and optical microscopy. Physical properties: Brinell hardness HBW and density were characterized. Preforms with 10, 15 and 20 vol. % of fibres were preheated and infiltrated applying the infiltration pressure of 100 MPa. The strengthening of matrix with SAFFIL fibres resulted in significant increase of hardness. Metallographic examinations showed, that SAFFIL fibres are not destroyed in course of the infiltration process and are uniformly distributed in copper matrix. SEM observations confirm the poor wettability of fibres by liquid Cu-ETP. The wear of manufactured MMCs during dry sliding against cast iron applying a pin-on-disc tester were recorded after 1, 3.5 and 8.5 km of friction distance. Increasing content of SAFFIL fibres in the copper matrix results in the significant decreasing of wear.
Przeprowadzono obserwacje mikroskopowe, badania twardości tribologicznej materiałów kompozytowych na osnowie miedzi M1E umocnionej włóknami δ-Al2O3 SAFFIL. Porowate kształtki z włókien ceramicznych nasycano miedzią metodą infiltracji ciśnieniowej (squeeze casting) pod ciśnieniem 100 MPa. Przeprowadzone badania z wykorzystaniem mikroskopu skaningowego oraz optycznego wykazały równomierne rozmieszczenie włókien, jednakże z licznymi defektami i słabą zwilżalnością umocnienia przez ciekłą miedź. Zbadano twardość Brinella HBW oraz gęstość materiałów kompozytowych zawierających 10, 15 i 20 obj. % włókien Al2O3. Stosując urządzenie do badania zużycia typu „pin-on-disc” przeprowadzono badania odporności na zużycie ścierne w warunkach tarcia suchego i stwierdzono, że wraz ze wzrostem zawartości włókien zwiększa się twardość i odporność na zużycie ścierne. W stosunku do nieumocnionej osnowy odporność materiałów kompozytowych zawierających 20% włókien zwiększa się około 10-krotnie. W mniejszym stopniu ulega zmianie współczynnik tarcia, który przy tarciu w parze z materiałami kompozytowymi jest o około 10-20% mniejszy niż przy ścieraniu z nieumocnioną miedzią.
Źródło:
Archives of Foundry Engineering; 2011, 11, 2 spec.; 71-74
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Własności trybologiczne materiałów kompozytowych na bazie stopów EN AW-2024 i EN AW-7075
Autorzy:
Kurzawa, A.
Granat, K.
Grodzka, E.
Naplocha, K.
Kaczmar, J. W.
Powiązania:
https://bibliotekanauki.pl/articles/381611.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
materiał kompozytowy
tlenek glinu
własności trybologiczne
composite material
alumina
tribological properties
Opis:
W pracy zostały przedstawione wyniki badań intensywności zużycia ściernego materiałów kompozytowych na bazie stopów EN AW-2024 i EN AW-7075 umacnianych cząstkami ceramicznymi Al2O3. Materiały zawierające 10÷40%obj. cząstek umacniających wytworzone metodą squeeze casting poddano ścieraniu z zastosowaniem metody pin-on-disc. Pozytywny efekt wzrostu odporności na zużycie ścierne potwierdzono dla materiałów opartych na stopie 7075 umocnionych od 10 do 30%obj. Al2O3. Umocnienie cząstkami stopu 2024, chociaż nieznacznie podniosło ich odporność na ścieranie przy zawartościach objętościowych cząstek ceramicznych 10 i 20% obj. to nie jest jednak satysfakcjonujące. Siła docisku próbki wpływa w zasadniczy sposób na intensywność zużycia materiałów kompozytowych. Pod mniejszym ciśnieniem 0,2 MPa pomiędzy próbką a tarczą materiały kompozytowe wykazały ok. 2-3 krotnie większą odporność na zużycie w porównaniu do stopu nieumocnionego. Zwiększenie ciśnienia do 1,0 MPa i 1,2 MPa spowodowało zwiększenie szybkości zużycia próbek, w szczególności dla materiałów zawierających 40% obj. cząstek Al2O3. Materiały kompozytowe na osnowie stopu AW-2024 generowały o ok 20÷25% większe opory tarcia od materiałów wytworzonych na osnowie stopu AW-7075. W wyniku analizy powierzchni ścierania stwierdzono, że wraz ze wzrostem zawartości objętości cząstek umacniających zmieniał się charakter zużycia z mieszanego, adhezyjno-ściernego występującego w kompozytach z 10% obj. cząstek Al2O3 w typowo ścierne występujące w materiałach zawierających 40% obj. udział umocnienia. Stopień zużycia przeciwpróbki silnie zależał od użytego materiału osnowy. Pomimo że stop nieumocniony AW-2024 wpływał na zużycie żeliwnej tarczy wolniej od stopu AW-7075, to jednak w materiałach zawierających umocnienie tendencja była odwrotna. Chropowatość Ra dna rowka przeciwpróbki potwierdza głębsze bruzdowanie przy ścieraniu kompozytów wytworzonych na osnowie stopu AW-2024. Największą chropowatość wykazały powierzchnie tarcz na których ścierano próbki z zawartością 10% obj. cząstek. Wraz ze wzrostem udziału cząstek w materiałach kompozytowych chropowatość przeciwpróbki maleje.
Źródło:
Archives of Foundry Engineering; 2013, 13, 1 spec.; 97-102
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Bending strength and fracture investigations of Cu based composite materials strengthened with \delta-alumina fibres
Autorzy:
Kaczmar, J. W.
Granat, K.
Naplocha, K.
Kurzawa, A.
Grodzka, E.
Samociuk, B.
Powiązania:
https://bibliotekanauki.pl/articles/383012.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
metal matrix composite
copper
alumina fibre
squeeze casting
bending strength
kompozyt metalowy
miedź
włókno aluminiowe
prasowanie stopu
wytrzymałość na zginanie
Opis:
Bending strength, thermal and electric conductivity and microstructure examinations of Cu based composite materials reinforced with Saffil alumina fibres are presented. Materials were produced by squeeze casting method applying the designed device and specially elaborated production parameters. Applying infiltration pressure of 90MPa and suitable temperature parameters provided manufacturing of copper based composite materials strengthened with Saffil alumina fibres characterized by the low rest porosity and good fibre-matrix interface. Three point bending tests at temperatures of 25, 100 and 300ºC were performed on specimens reinforced with 10, 15 and 20% of Saffil fibres. Introduced reinforcement effected on the relatively high bending strengths at elevated temperatures. In relation to unreinforced Cu casting strength of composite material Cu – 15vol.% Saffil fibres increase by about 25%, whereas at the highest applied test temperature of 300ºC the improvement was almost 100%. Fibres by strengthening of the copper matrix and by transferring loads from the matrix reduce its plastic deformation and hinder the micro-crack developed during bending tests. Decreasing of thermal and electrical conductivity of Cu after incorporating fibres in the matrix are relatively small and these properties can be acceptable for electric and thermal applications.
Źródło:
Archives of Foundry Engineering; 2013, 13, 2; 59-63
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-10 z 10

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies