Influence of Shot Peening on Abrasion Wear in Real Conditions of Ni-Cu-Ausferritic Ductile Iron
Autorzy:
Wieczorek, A. N.
Powiązania:
https://bibliotekanauki.pl/articles/350866.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ADI
shot peening
wear
abrasion
Opis:
The paper presents results of the wear tests of chain wheels made of austempered ductile iron with various content of residual austenite. The aim of this study was to demonstrate the impact of the dynamic surface treatment (shot peening) on wear properties of surface layers of the chain wheels tested that were subjected to the action of quartz abrasive. Apart from determining the value of the abrasive wear, examinations of the magnetic phase content in the microstructure were carried out and plots of hardness of the surface layer as a function of the distance from the surface and microstructure of the materials were prepared. Based on the results, the following was found: an increase in the abrasive wear and a reduction in the hardness of the surface layer of chain wheels subjected to shot peening, as well as reduction of susceptibility to negative action of the shot for cast irons with the structure of upper ausferrite.
Źródło:
Archives of Metallurgy and Materials; 2016, 61, 4; 1985-1990
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Operation-Oriented Studies on Wear Properties of Surface-Hardened Alloy Cast Steels Used in Mining in the Conditions of the Combined Action of Dynamic Forces and an Abrasive Material
Autorzy:
Wieczorek, A. N.
Powiązania:
https://bibliotekanauki.pl/articles/356119.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
steel cast
dynamic force
synergism
wear
shot-peening
Opis:
This paper presents the results of wear tests of shot-peened and not shot-peened cast steels used in the mining machinery industry, in particular in the construction of chain drums for armoured face conveyors. Wear tests were carried out in the conditions corresponding to the real operating conditions of armoured face conveyors during drifting work in rocks such as sandstone. The operating factors subjected to the analyses included the presence of quartz abrasive and the impact of external dynamic forces. On the basis of the wear tests as well as the microhardness and microstructure examinations performed, it has been found that the action of an additional dynamic force has a synergistic impact on the process of abrasive wear in loose quartz abrasive. It has been further found that the value of abrasive wear of chain wheels operated in the conditions of a combined action of abrasive and a dynamic force depends on whether the area of mating of wheels with the chain was shot-peened or not before the wear tests – an increase in the abrasive wear was observed for the wheels made of cast steel subjected to shot peening in the area of mating with the chain. Lower resistance to abrasive wear of the cast steels subjected to shot peening before the wear tests could result from the formation of cracks in the surface layer caused by the action of shot.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 4; 2381-2389
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Role of Operational Factors in Shaping of Wear Properties of Alloyed Austempered Ductile Iron. Part I. Experimental Studies Abrasive Wear of Austempered Ductile Iron (ADI) in the Presence of Loose Quartz Abrasive
Rola czynników eksploatacyjnych w kształtowaniu właściwości zużyciowych stopowych żeliw sferoidalnych ausferrytycznych. Część I. Eksperymentalne badania zużycia ściernego w obecności luźnego ścierniwa kwarcowego żeliw ADI
Autorzy:
Wieczorek, A. N.
Powiązania:
https://bibliotekanauki.pl/articles/353090.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
tribology
austempered ductile iron
wear resistance
tribologia
żeliwo sferoidalne ADI
odporność na zużycie
Opis:
The paper presents the results of the wear tests of alloyed austempered ductile iron performed on a specially designed test rig simulating real operating conditions for chain wheels which were selected for testing due to their complex rolling and sliding form of contact between elements. The chain wheels subjected to tests were operated with the use of loose quartz abrasive and without it. The studies involved the determination of strength and plastic properties, hardness distributions, microstructure and linear wear of the ADI in question considered as a function of the austempering temperature. Based on the results obtained, the following was found: phase transition of austempered ductile iron can take place for combinations typical of industrial applications, a non-linear increase in the wear as a function of the austempering temperature occurs, an increase in the hardness of all the analysed types of ADI takes place during the operation without the presence of abrasive, the phase transition of austenite into martensite in ADI with a lower content of austenite requires higher loads as compared with cast iron containing 40% of austenite.
W pracy przedstawiono wyniki badań zużyciowych stopowych żeliw ausferrytycznych na specjalnie skonstruowanym stanowisku badawczym imitujacym rzeczywiste warunki eksploatacyjne kół łancuchowych, wybranych do testów z uwagi na złożoną toczno-ślizgowa postać współpracy elementów. Testowane koła łańcuchowe były eksploatowane z udziałem luźnego ścierniwa kwarcowego i bez niego. W ramach badań wyznaczono właściwości wytrzymałościowe i plastyczne, rozkłady twardości, mikrostrukture i zużycie liniowe rozpatrywanych żeliw ADI w funkcji temperatury ausferytyzacji. Na podstawie uzyskanych wyników stwierdzono: w skojarzeniach typowych dla zastosowań przemysłowych może dojść do przemiany fazowej ausferytycznych żeliw sferoidalnych, nieliniowy wzrost zużycia w funkcji temperatury ausferytyzacji, zwiększenie twardości wszystkich analizowanych żeliw ADI przy pracy bez udziału ścierniwa oraz zaistnienie przemiany fazowej austenitu w martenzyt w żeliwach ADI o mniejszej zawartości austenitu wymaga oddziaływania wyższych obciążeń w porównaniu z żeliwem zawierającym 40% austenitu.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 4; 1653-1662
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Role of Operational Factors in Shaping of Wear Properties of Alloyed Austempered Ductile Iron. Part II. An Assessment of the Cumulative Effect of Abrasives Processes and the Dynamic Activity on the Wear Property of Ausferritic Ductile Iron
Rola czynników eksploatacyjnych w kształtowaniu właściwości zużyciowych stopowych żeliw sferoidalnych ausferrytycznych. Część II. Ocena skumulowanego działania ścierniwa i wymuszeń dynamicznych na właściwości zużyciowe sferoidalnych żeliw ausferrytycznych
Autorzy:
Wieczorek, A. N.
Powiązania:
https://bibliotekanauki.pl/articles/351212.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
tribology
austempered ductile iron
wear resistance
tribologia
żeliwo sferoidalne ADI
odporność na zużycie
Opis:
The study presents results of the second part of wear tests of austempered ductile irons on a specially designed test rig that allows simulating the real operating conditions of chain wheels. The chain wheels subjected to testing were operated in conditions characterized by combined action of loose quartz abrasive and an external dynamic force. The studies involved the determination of the hardness, microstructure and linear wear of the ADIs in question considered as a function of the austempering temperature and the austenite content. Based on the results obtained, the following was observed: a decrease in the wear as a function of the austempering temperature and thus in the content of austenite in ADIs; a slight deformation of graphite after completing the wear test involving external dynamic forces; a negative linear dependence between the linear wear and the impact resistance. It was found that the increased wear of cast irons with a lower content of austenite may be caused by the propagation of cracks initiated by damage to graphite nodules, while in the conditions characterized by combined action of abrasive wear and dynamic load the cast irons with a higher content of austenite and higher impact resistance have better wear properties.
W pracy przedstawiono rezultaty drugiej częćci badań zużyciowych stopowych żeliw ausferytycznych na specjalnie skonstruowanym stanowisku badawczym imitującym rzeczywiste warunki eksploatacyjne kół łancuchowych. Testowane koła łańcuchowe były eksploatowane w warunkach skojarzonego oddziaływania luźnego ścierniwa kwarcowego i zewnętrznej siły dynamicznej. W ramach badań wyznaczono przebiegi twardości, mikrostrukturę i zużycie liniowe rozpatrywanych żeliw ADI w funkcji temperatury ausferytyzacji i zawartości austenitu. Na podstawie uzyskanych wyników zauważono: spadek zużycia w funkcji temperatury ausferytyzacji, a tym samym zawartości austenitu w żeliwach ADI, nieznaczne odkształcenia grafitu po zakończeniu testu zużyciowego z udziałem zewnętrznych sił dynamicznych, zużycie liniowe i udarność wykazały ujemną liniową zalezność. Stwierdzono, że powodem zwiększenia zużycia żeliw o mniejszej zawartości austenitu mogła być propagacja pęknięć zainicjowanych uszkodzeniami kulek grafitu oraz w warunkach skojarzonego działania zużycia ściernego i obciążenia dynamicznego lepszymi właściwościami zużyciowymi odznaczają się żeliwa o większej zawartości austenitu charakteryzujące się większą udarnoącią.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 4; 1663-1671
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Comparative Studies on the Wear of ADI Alloy Cast Irons as Well as Selected Steels and Surface-Hardened Alloy Cast Steels in the Presence of Abrasive
Autorzy:
Wieczorek, A. N.
Powiązania:
https://bibliotekanauki.pl/articles/351738.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
austempered ductile iron
steel
steel cast
wear
abrasion
Opis:
The paper presents the results of wear tests obtained for 4 groups of materials: surface-hardened alloy steels and alloy cast steels for structural applications, hard-wearing surface-hardened alloy cast steels, and austempered alloy cast irons. The wear tests have been performed on a specially designed test rig that allows reproducing the real operating conditions of chain wheels, including the rolling and sliding form of contact between elements. The chain wheels subjected to tests were operated with the use of loose quartz abrasive. This study presents results of measurements of material parameters, micro-structure of a surface subject to wear, as well as the linear wear determined for the materials considered. Based on the results, the following was found: the best wear properties were obtained for surface-hardened alloy steels and wear surface; strengthening of the ADI surface took place - most probably as a result of transformation of austenite into martensite; the uniformity of the structure of the materials affects the surface wear process. The study also indicated a significant degree of graphite deformation in ADI characterized by the upper ausferritic structure and its oblique orientation in relation to the surface, which resulted in a facilitated degradation of the surface caused by the quartz abrasive.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 1; 119-128
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Alteration of mélange-hosted chromitites from Korydallos, Pindos ophiolite complex, Greece: evidence for modification by a residual high-T post-magmatic fluid
Autorzy:
Kapsiotis, A. N.
Powiązania:
https://bibliotekanauki.pl/articles/138612.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Ferrian chromite
Cr-spinel
metamorphism
Ophiolites
Pindos
spinel Cr
metamorfizm
ofiolity
Opis:
The peridotites from the area of Korydallos, in the Pindos ophiolitic massif, crop out as deformed slices of a rather dismembered sub-oceanic, lithospheric mantle section and are tectonically enclosed within the Avdella mélange. The most sizeable block is a chromitite-bearing serpentinite showing a mesh texture. Accessory, subhedral to euhedral Cr-spinels in the serpentinite display Cr# [Cr/(Cr + Al)] values that range from 0.36 to 0.42 and Mg# [Mg/(Mg + Fe2+)] values that vary between 0.57 and 0.62, whereas the TiO2 content may be up to 0.47 wt.%. The serpentinite fragment is characterized by low abundances of magmaphile elements (Al2O3: 0.66 wt.%, CaO: 0.12 wt.%, Na2O: 0.08 wt.%, TiO2: 0.007 wt.%, Sc: 4 ppm) and enrichment in compatible elements (Cr: 2780 ppm and Ni: 2110 ppm). Overall data are in accordance with derivation of the serpentinite exotic block from a dunite that was formed in the mantle region underneath a back-arc basin before tectonic incorporation in the Korydallos mélange. Two compositionally different chromitite pods are recognized in the studied serpentinite fragment, a Cr-rich chromitite and a high-Al chromitite, which have been ascribed to crystallization from a single, progressively differentiating MORB/IAT melt. Although both pods are fully serpentinized only the Al-rich one shows signs of limited Cr-spinel replacement by an opaque spinel phase and clinochlore across grain boundaries and fractures. Modification of the ore-making Cr-spinel is uneven among the Al-rich chromitite specimens. Textural features such as olivine replacement by clinochlore and clinochlore disruption by serpentine indicate that Cr-spinel alteration is not apparently related to serpentinization. From the unaltered Cr-spinel cores to their reworked boundaries the Al2O3 and MgO abundances decrease, being mainly compensated by FeOt and Cr2O3 increases. Such compositional variations are suggestive of restricted ferrian chromite (and minor magnetite) substitution for Cr-spinel during a short-lived but relatively intense, low amphibolite facies metamorphic episode (temperature: 400–700 °C). The presence of tremolite and clinochlore in the interstitial groundmass of the high-Al chromitite and their absence from the Cr-rich chromitite matrix imply that after chromitite formation a small volume of a high temperature, post-magmatic fluid reacted with Cr-spinel, triggering its alteration.
Źródło:
Acta Geologica Polonica; 2014, 64, 4; 473-494
0001-5709
Pojawia się w:
Acta Geologica Polonica
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Numerical Implementation of the Fictitious Domain Method for Elliptic Equations
Autorzy:
Temirbekov, A. N.
Wójcik, W.
Powiązania:
https://bibliotekanauki.pl/articles/226820.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
elliptic equation
Dirichlet problem
equation with rapidly varying coefficients
computational algorithm
iterative process
fictitious domain method
boundary conditions
Opis:
In this paper, we consider an elliptic equation with strongly varying coefficients. Interest in the study of these equations is connected with the fact that this type of equation is obtained when using the fictitious domain method. In this paper, we propose a special method for the numerical solution of elliptic equations with strongly varying coefficients. A theorem is proved for the rate of convergence of the iterative process developed. A computational algorithm and numerical calculations are developed to illustrate the effectiveness of the proposed method.
Źródło:
International Journal of Electronics and Telecommunications; 2014, 60, 3; 219-223
2300-1933
Pojawia się w:
International Journal of Electronics and Telecommunications
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Abrasive Wear Properties of Fe-Based Alloys Designed for Mining Applications
Autorzy:
Wieczorek, A. N.
Myszka, D.
Powiązania:
https://bibliotekanauki.pl/articles/354479.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
wear
abrasion
ADI
steel
cast steel
Opis:
The purpose of this study was to determine experimentally the wear properties of 5 groups of iron-based alloys used in the mining and transport machines exposed to the action of a hard abrasive material. The groups of materials to be examined included austempered ductile irons (ADI), steels and cast steel designed for quenching and tempering and for surface hardening, hard-wearing hardened steels and structural steels. The wear tests were carried out on a disc-on-disc test rig. The test samples were examined under conditions of sliding mating, while the leading destructive process was microcutting of the surface with loose corundum grain. The loss of mass of the examined samples was measured as a parameter characterizing the wear. Base on it, other wear coefficients were determined, for example the volume loss, the intensity of wear and the wear rate. The volume loss values determined were presented as a function of the strength and the initial hardness. Based on the results obtained, it was found that the hardened steel and ADI had comparable wear properties, while the ADI surface was strengthened probably as a result of the transition of austenite into martensite and the impact of the deformation of the graphite contained in ADI on the abrasive wear of the surface.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 3; 1521-1534
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Albian ammonites from northern Pakistan
Autorzy:
Kennedy, W. J.
Fatmi, A. N.
Powiązania:
https://bibliotekanauki.pl/articles/138606.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ammonites
Cretaceous
Albian
Pakistan
amonity
kreda
alb
Opis:
The occurrence of rich Albian ammonite faunas in what is now northern Pakistan has been known for more than 80 years, but there has been no comprehensive account of the assemblages present. A total of 36 taxa are described below. The middle part of the Lumshiwal Formation yields Upper Aptian ammonites south of the Samana Range. Elsewhere, it yields Douvilleiceras leightonense Casey, 1962, of the lower Lower Albian Leymeriella regularis Zone and the Sonneratia perinflata and S. kitchini Subzones of the Sonneratia chalensis Zone of the northwest European sequence. The top one to two metres of the Lumshiwal yields an abundant fauna of rolled and phosphatised ammonites that includes elements from much of the Albian. Of these, Prolyelliceras gevreyi (Jacob, 1907) first appears in the lower Lower Albian Leymeriella tardefurcata Zone. The commonest ammonite is Douvilleiceras mammillatum (Schlotheim, 1813) sensu lato, which ranges from the perinflata Subzone of the chalensis Zone to the Otohoplites bulliensis Subzone of the O. auritiformis Zone of the Lower Albian. The presence of Lyelliceras pseudolyelli (Parona and Bonarelli, 1897) indicates the uppermost, pseudolyelli Subzone of the auritiformis Zone. The presence of Lyelliceras lyelli (d’Orbigny, 1841) indicates the basal Middle Albian lyelli Subzone of the Hoplites dentatus Zone. There is no evidence for the higher parts of the Middle Albian. Dipoloceras (Rhytidoceras ) sp. indicates the presence of lower Upper Albian, possibly the pricei Zone. There is evidence, in the form of specifically indeterminate Mortoniceras (Mortoniceras) sp., of a level within the inflatum to fallax Zone inteval from a single locality, but no evidence of the succeeding parts of the upper Upper Albian. The base of the Kawagarth Formation that succeeds the Lumshiwal yields lower Upper Albian Mortoniceras (M.) geometricum Spath, 1932 of the Mortoniceras pricei Zone, northwest of Darmasand in the Samana range.
Źródło:
Acta Geologica Polonica; 2014, 64, 1; 47-98
0001-5709
Pojawia się w:
Acta Geologica Polonica
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Experimental Determination of the Synergistic Components of Tribocorrosive Wear of Ni-Cu-Mo-Ausferritic Ductile Iron
Autorzy:
Wieczorek, A. N.
Stachowiak, A.
Zwierzycki, W.
Powiązania:
https://bibliotekanauki.pl/articles/350818.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ADI
tribocorrosion
wear
Opis:
The paper presents results of a two-stage study on the tribocorrosive wear of ADI alloy cast iron containing Ni and Cu. In the first stage of the wear tests with use test rig type pin-on-plate, there were determined the parameters of the process of tribocorrosion of the ADI cast iron in 3.5% NaCl solution. In the second stage, the tests were carried out on a test rig simulating real operating conditions of chain wheels used in armoured face conveyors. The purpose of this study was to demonstrate the impact of the combined action of corrosive agents (water and NaCl) and quartz abrasive on the wear of the wheels tested. As part of the test, the abrasive wear in the presence of the abrasive material alone and in the presence of a mixture of the abrasive material, water and NaCl was determined. The microstructure and the hardness of the surface layer as a function of the distance from the surface were also determined. During the study it has been found that regardless of the type of test there is a synergy between the effects of corrosion and friction which led to an increase of the resulting wear by 30%.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 1; 87-97
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Prediction of Tribocorrosive Properties of ADI Containing Ni-Cu-Mo
Autorzy:
Wieczorek, A. N.
Stachowiak, A.
Zwierzycki, W.
Powiązania:
https://bibliotekanauki.pl/articles/354058.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ADI
tribocorrosion
wear
Opis:
In the case of mining machines, tribocorrosion damage is often observed. This type of consumption is caused by the joint action of mining environment factors such as abrasive and water. The search for methods to counteract tribocorrosion is of great practical importance, but it must be combined with the knowledge of methods of forecasting the value of wear. This paper presents a model of prediction of tribocorrosive wear adapted to corrodible materials – ADI containing Ni and Cu, with the strength class of 800 MPa – and results of a two-stage study on the tribocorrosive wear. Presented results indicate a distinct effect of synergy between friction and corrosion in the total wear of ADI. The tribocorrosion tests confimed the adequacy of the model developed for the ADI.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 3; 1417-1422
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Blood antioxidant enzymes (SOD, GPX), biochemical and haematological parameters in pigs naturally infected with porcine reproductive and respiratory syndrome virus
Autorzy:
Stukelj, M.
Toplak, I.
Svete, A.N.
Powiązania:
https://bibliotekanauki.pl/articles/30625.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Opis:
Porcine reproductive and respiratory syndrome (PRRS) has become one of the most economically important diseases for the swine industry worldwide. The objective of the study was to determine selected blood antioxidant enzymes (glutathione peroxidase (GPX), superoxide dismutase (SOD)), biochemical and haematological parameters in PRRS positive and negative pigs of three different categories, mainly to test oxidative stress hypothesis in pigs naturally infected with PRRS virus. Ninety PRRS positive and 90 PRRS negative pigs were included in the study. The presence of PRRS was confirmed by serological detection of antibodies against PRRS virus (PRRSV) and detection of PRRS viral RNA by RT-PCR. Pigs were further divided into three groups of 30: piglets just before weaning (weaners), fatteners and finishers. Blood samples for determining selected blood parameters were collected from the vena cava cranialis. Significantly (P < 0.05) higher activities of SOD in weaners and fatteners and of GPX in weaners were determined in PRRS positive pigs than in corresponding groups of PRRS negative pigs. In contrast, significantly (P < 0.05) lower GPX activity was observed in finishers of PRRS positive pigs than in the corresponding group of PRRS negative pigs. Concentrations of serum total protein in PRRS positive weaners and fatteners were significantly (P < 0.05) higher than those found in PRRS negative pigs. Leukopenia was observed in all three groups of PRRS positive pigs. It has been demonstrated, for the first time, that oxidative stress might be increased in PRRSV naturally infected pigs, especially in weaners.
Źródło:
Polish Journal of Veterinary Sciences; 2013, 16, 2
1505-1773
Pojawia się w:
Polish Journal of Veterinary Sciences
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Investigation of the Stability and Convergence of Difference Schemes for the Three-dimensional Equations of the Atmospheric Boundary Layer
Autorzy:
Temirbekov, A. N.
Urmashev, B. A.
Gromaszek, K.
Powiązania:
https://bibliotekanauki.pl/articles/226826.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
atmospheric boundary layer equations
difference scheme
approximation error
stability
convergence algorithms
numerical solution
Opis:
In this article we construct a finite-difference scheme for the three-dimensional equations of the atmospheric boundary layer. The solvability of the mathematical model is proved and quality properties of the solutions are studied. A priori estimates are derived for the solution of the differential equations. The mathematical questions of the difference schemes for the equations of the atmospheric boundary layer are studied. Nonlinear terms are approximated such that the integral term of the identity vanishes when it is scalar multiplied. This property of the difference scheme is formulated as a lemma. Main a priori estimates for the solution of the difference problem are derived. Approximation properties are investigated and the theorem of convergence of the difference solution to the solution of the differential problem is proved.
Źródło:
International Journal of Electronics and Telecommunications; 2018, 64, 3; 391-396
2300-1933
Pojawia się w:
International Journal of Electronics and Telecommunications
Dostawca treści:
Biblioteka Nauki
Artykuł

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies