Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "IL -6" wg kryterium: Wszystkie pola


Wyświetlanie 1-2 z 2
Tytuł:
Detection of IL-1β, IL-6 and TNF-αin Sprague-Dawely rats’ atrophic thymus induced by lipopolysaccharide
Autorzy:
Zhong, Y.B.
Zhang, X.L.
Lv, M.Y.
Hu, X.F.
Li, Y.
Powiązania:
https://bibliotekanauki.pl/articles/2087664.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
lipopolysaccharide
pro-inflammatory cytokines
thymus atrophy
rat
Źródło:
Polish Journal of Veterinary Sciences; 2018, 21, 3; 589-597
1505-1773
Pojawia się w:
Polish Journal of Veterinary Sciences
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of T6 Heat Treatment on the Scratch Wear Behavior of Extruded Al-12wt.%Si Alloy
Autorzy:
Kang, Yeon-Ji
Kim, Jong-Ho
Hwang, Jong-Il
Lee, Kee-Ahn
Powiązania:
https://bibliotekanauki.pl/articles/356776.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Al-12wt.%Si alloy
scratch test
wear-resistance
T6 heat treatment
Opis:
This study investigated the effect of T6 heat treatment on the microstructure and scratch wear behavior of hypoeutectic Al-12wt.%Si alloy manufactured by extrusion. Microstructural observation identified spherical eutectic Si phases before and after the heat treatment of alloys (F, T6). Phase analysis confirmed Al matrix and Si phase as well as Al2Cu and Al3Ni, Mg2Si in both alloys. In particular, Al2Cu was finer and more evenly distributed in T6 alloy. This resulted in Vickers hardness of T6 alloy that was 2.3 times greater compared to F alloy. The scratch wear test was conducted using constant load scratch test (CLST) mode and multi-pass scratch test (MPST) mode. The scratch coefficient and worn out volume obtained by such were used to evaluate wear properties before and after heat treatment. In the case of T6 alloy, its scratch coefficient was lower than F alloy in all load ranges. After 15 repeated tests to measure worn out volume, F alloy and T6 alloy measured 1.2×10-1 mm3 and 7.8×10-2 mm3, respectively. In other words, the wear resistance of T6 alloy were confirmed to be better than those of F alloy. In addition, this study attempted to identify the microstructural factors that contribute to the better scratch wear resistance of T6 alloy and wear mechanism from surface and cross-section observations after the wear tests.
Źródło:
Archives of Metallurgy and Materials; 2019, 64, 2; 617-622
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies