Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "alloy" wg kryterium: Temat


Tytuł:
Aluminum Alloy Development for Wheel Production by Low Pressure Die Casting with New Generation Computational Materials Engineering Approaches
Autorzy:
Yağcı, T.
Cöcen, Ü.
Çulha, O.
Powiązania:
https://bibliotekanauki.pl/articles/2079795.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
aluminum alloy
foundry industry
wheels
low pressure casting
materials engineering
mechanical properties
microstructural design
stop aluminium
przemysł odlewniczy
koła
odlewanie niskociśnieniowe
inżynieria materiałowa
właściwości mechaniczne
projektowanie mikrostrukturalne
Opis:
Computational Materials Engineering (CME) is a high technological approach used to design and develop new materials including the physical, thermal and mechanical properties by combining materials models at multiple techniques. With the recent advances in technology, the importance of microstructural design in CME environments and the contribution that such an approach can make in the estimation of material properties in simulations are frequently discussed in scientific, academic, and industrial platforms. Determination of the raw material characteristics that can be modeled in a virtual environment at an atomic scale by means of simulation programs plays a big role in combining experimental and virtual worlds and creating digital twins of the production chain and the products. In this study, a new generation, alternative and effective approach that could be used to the development of Al-Si based wheel casting alloys is proposed. This approach is based on the procedure of optimizing the physical and thermodynamic alloy properties developed in a computer environment with the CME technique before the casting phase. This article demonstrates the applicability of this approach in alloy development studies to produce Al-Si alloy wheels using the low pressure die casting (LPDC) method. With this study, an alternative and economical way is presented to the alloy development studies by trial and error in the aluminum casting industry. In other respects, since the study is directly related to the automotive industry, the reduction in fuel consumption in vehicles is an expected effect, as the new alloy aims to reduce the weight of the wheels. In addition to conserving energy, reducing carbon emissions also highlights the environmental aspects of this study.
Źródło:
Archives of Foundry Engineering; 2021, 21, 4; 35-46
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Analysis of the Microstructure, Properties and Machinability of Al-Cu-Si Alloys
Autorzy:
Kozana, J.
Piękoś, M.
Maj, M.
Garbacz-Klempka, A.
Żak, P. L.
Powiązania:
https://bibliotekanauki.pl/articles/1840820.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
casting of non-ferrous metals
aluminum alloys
ternary Al-Cu-Si alloy
mechanical properties
microstructure
thermo-calc
odlewanie metali nieżelaznych
stopy aluminium
stop trójskładnikowy Al-Cu-Si
właściwości mechaniczne
mikrostruktura
Opis:
As part of the studies conducted in the field of broadly understood casting of non-ferrous metals, selected results on the impact of variable additions of copper and silicon in aluminium were presented. A series of melts was carried out with copper content kept constant at a level of 2% (1st stage) and 4% (2nd stage) and variable contents of silicon introduced into aluminium. The crystallization characteristics of the examined alloys and the percentage of structural constituents at ambient temperature were obtained by modelling the thermodynamic parameters of individual phases with the CALPHAD method. The microstructure of the obtained alloys was examined and microhardness was measured by the Vickers-Hanemann method. The alloy properties were assessed based on the results of mechanical tests, including ultimate tensile strength (UTS), hardness (BHN) and elongation (E). The machinability of the tested alloys was analyzed in a machinability test carried out by the Keep-Bauer method, which consisted in drilling with a constant feed force. The obtained results clearly indicate changes in the images of microstructure, such as the reduction in grain size, solution hardening and precipitation hardening. The changes in the microstructure are also reflected in the results of mechanical properties testing, causing an increase in strength and hardness, and plasticity variations in the range of 4 ÷ 16%, mainly due to the introduced additions of copper and silicon. The process of alloy strengthening is also visible in the results of machinability tests. The plotted curves showing the depth of the hole as a function of time and the images of chips produced during the test indicate an improvement in the wear resistance obtained for the tested group of aluminium alloys with the additions of copper and silicon.
Źródło:
Archives of Foundry Engineering; 2020, 20, 4; 145-153
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Assessment of AlSi21CuNi alloy’s quality with use of ATND method
Autorzy:
Pezda, J.
Powiązania:
https://bibliotekanauki.pl/articles/380515.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
hypereutectic Al-Si alloy
modification
ATND
mechanical properties
stop nadeutektyczny Al-Si
modyfikacja
metoda ATND
właściwości mechaniczne
Opis:
Majority of combustion engines is produced (poured) from Al-Si alloys with low thermal expansion coefficient, so called piston silumins. Hypereutectic alloys normally contain coarse, primary angular Si particles together with eutectic Si phase. The structure and mechanical properties of these alloys are highly dependent upon cooling rate, composition, modification and heat-treatment operations. In the paper one depicts use of the ATND method (thermal-voltage-derivative analysis) and regression analysis to assessment of quality of the AlSi21CuNi alloy modified with Cu-P on stage of its preparation, in aspect of obtained mechanical properties (R0,02, Rm, A5, HB). Obtained dependencies enable prediction of mechanical properties of the investigated alloy in laboratory conditions, using values of characteristic points from curves of the ATND method.
Źródło:
Archives of Foundry Engineering; 2013, 13, 4; 87-92
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Assessment of Quality of EN AC-43300 Alloy with Use of ATND Method
Autorzy:
Pezda, J.
Powiązania:
https://bibliotekanauki.pl/articles/381845.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
aluminum alloy
ATND method
mechanical properties
stop aluminium
metoda ATND
właściwości mechaniczne
Opis:
Application of the silumins expands together with nowadays tendency to reduction of design structures mass. Technological and mechanical properties of Al-Si casting alloys depend mainly from structure of eutectic mixture, which is modified in result of introduction of micro alloying elements to liquid alloy, and that is why proper use of knowledge on crystallization to control of crystallization kinetics of produced alloys to optimize obtained structure is a significant factor leading to improvement of quality of the castings. In the paper one depicts use of the ATND method (thermal-voltage-derivative analysis) and regression analysis to assessment of quality of the EN AC-43300 alloy modified with strontium on stage of its preparation, in aspect of obtained mechanical properties (R0,02, R0,2, Rm, A5). Obtained dependencies enable prediction of mechanical properties of the investigated alloy, basing on values of characteristic points from the ATND method.
Źródło:
Archives of Foundry Engineering; 2013, 13, 1 spec.; 139-142
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Crystallization Behavior and Properties of Hypereutectic Al-Si Alloys with Different Iron Content
Autorzy:
Deev, V.
Prusov, E.
Prikhodko, O.
Ri, E.
Kutsenko, A.
Smetanyuk, S.
Powiązania:
https://bibliotekanauki.pl/articles/1837865.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
aluminium-silicon alloys
hypereutectic alloy
iron-rich compounds
intermetallics phase
crystallization
mechanical properties
stop aluminiowo-krzemowy
stop nadeutektyczny
fazy międzymetaliczne
krystalizacja
właściwości mechaniczne
Opis:
Understanding the influence of iron impurity on the formation of the structure and the properties of hypereutectic aluminum-silicon alloys are important for achieving the required quality of castings, especially those obtained from secondary materials. In the present work, the influence of different iron contents (0.3, 1.1, and 2.0 wt.%) on the crystallization process, microstructure and mechanical properties of the Al-15% Si alloy was studied. It is shown that the presence of iron impurity in the Al-15% Si alloy leads to increasing the eutectic crystallization time from 6.2 to 7.6 s at increasing the iron content from 0.3 wt.% to 1.1 wt.%, changing the structure of the alloy eutectic in the solid state. The primary silicon and β-Al5SiFe phase coexist in the structure of the Al-15% Si alloys at a temperature below 575°C in the range of iron concentrations from 0 to 2 wt.% in equilibrium conditions. In the experimental alloys structure, the primary crystals of the β-phase were metallographically detected only in the alloys containing 1.1 and 2 wt.% of iron impurity. Increase of the iron content up to 2 wt.% significantly reduces the mechanical properties of the Al-15% Si alloy due to the formation of large platelet-like inclusions of β-Al5SiFe phase.
Źródło:
Archives of Foundry Engineering; 2020, 20, 4; 101-107
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Degradation of Creep Resistant Ni - alloy During Aging at Elevated Temperature Part I: Mechanical Properties
Autorzy:
Kaczorowski, M.
Skoczylas, P.
Gulbinowicz, Z.
Powiązania:
https://bibliotekanauki.pl/articles/381428.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
creep resistant alloy
Ni alloy
mechanical properties
hydrogen embrittlement
stop żarowytrzymały
stop Ni
właściwości mechaniczne
kruchość wodorowa
Opis:
The results of experimental study of mechanical properties degradation of creep resistant Ni-base alloy are presented. The material studied was subjected to long-term influence of high pressure hydrogen atmosphere at temperature 750K and 850K. The mechanical properties of specimens taken at different distance from inner surface of thick wall tube were evaluated. The results of mechanical testing showed distinct influence of the temperature on mechanical properties of Ni creep resistant alloy. Moreover, the mechanical properties of studied alloy depend on the location of the specimen with respect to the dissociated ammonia source i.e. distance from the inner surface of the chamber. The results of mechanical testing show that the higher the distance from inner surface of the chamber the better mechanical properties of studied Ni base super-alloy.
Źródło:
Archives of Foundry Engineering; 2015, 15, 3 spec.; 25-28
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Heat Treatment on the Mechanical Properties of Two-Phase Titanium Alloy Ti6Al7Nb
Wpływ obróbki cieplnej na własności mechaniczne dwufazowego stopu tytanu Ti6Al7Nb
Autorzy:
Dąbrowski, R.
Powiązania:
https://bibliotekanauki.pl/articles/351360.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
heat treatment
microstructure
mechanical properties
two-phase titanium alloy
obróbka cieplna
mikrostruktura
właściwości mechaniczne
dwufazowy stop tytanu
Opis:
Mechanical properties of the two-phase titanium alloy Ti6Al7Nb, after the heat treatment based on soaking this alloy in the α + β range, cooling in water or oil and ageing at two selected temperatures, were determined in the hereby paper. The alloy mechanical properties were determined in tensile and impact tests, supported by the fractographic analysis of fractures. In addition, its hardness was measured and the analysis of changes occurring in the microstructure was performed for all variants of the alloy heat treatment. Regardless of the applied cooling rate of the alloy, from a temperature of 970°C followed by ageing at 450 and 650°C, none essential changes were noticed in its microstructure. It was shown that applying less intensive cooling medium (oil) instead of water (before tempering) decreases strength properties indicators, i.e. tensile strength and yield strength as well as hardness (only slightly). The decrease of the above mentioned indicators is accompanied by an increase of an elongation and impacts strength. Fractures of tensile and impact tests are of a ductile character regardless of the applied heat treatment.
Wartykule określono własności mechaniczne dwufazowego stopu tytanu Ti6Al7Nb po obróbce cieplnej polegającej na wygrzewaniu stopu w zakresie dwufazowym, oziębianiu w wodzie lub oleju oraz starzeniu przy wybranych dwóch temperaturach. Własności mechaniczne stopu wyznaczono w próbie rozciągania i w próbie udarności, które poparto analizą fraktograficzną przełomów. Dodatkowo, dla wszystkich wariantów obróbki cieplnej stopu zmierzono twardość i dokonano analizy zmian zachodzących w mikrostrukturze. Niezależnie od zastosowanej szybkości oziębiania badanego stopu od temperatury 970°C i następnego starzenia przy 450 i 650°C, nie odnotowano istotnych zmian zachodzących w jego mikrostrukturze. Wykazano, że zastosowanie mniej intensywnego ośrodka chłodzącego (oleju) zamiast wody (przed zabiegiem odpuszczania), obniza wskaźniki własności wytrzymałościowych, tj. wytrzymałość na rozciąganie i umowną granice plastyczności, a także nieznacznie twardość. Obniżeniu ww. wskaźników towarzyszy wzrost wydłużenia oraz udarności. Przełomy próbek rozciąganych i udarnościowych niezależnie od zastosowanej obróbki cieplnej mają charakter ciągliwy.
Źródło:
Archives of Metallurgy and Materials; 2014, 59, 4; 1713-1716
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of Microstructure of Fe-C-V Alloys on Selected Functional Properties
Autorzy:
Kawalec, M.
Kozana, J.
Powiązania:
https://bibliotekanauki.pl/articles/382066.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
microstructure
Fe-C-V alloy
workability
mechanical properties
vanadium carbide
mikrostruktura
stop Fe-C-V
urabialność
właściwości mechaniczne
węglik wanadu
Opis:
The cast alloys crystallizing in Fe-C-V system are classified as white cast iron, because all the carbon is bound in vanadium carbides. High vanadium cast iron has a very high abrasion resistance due to hard VC vanadium carbides. However, as opposed to ordinary white cast iron, this material can be treated using conventional machining tools. This article contains the results of the group of Fe-C-V alloys of various microstructure which are been tested metallographic, mechanical using an INSTRON machine and machinability with the method of drilling. The study shows that controlling the proper chemical composition can influence on the type and shape of the crystallized matrix and vanadium carbides. This makes it possible to obtain a high-vanadium cast iron with very high wear resistance while maintaining a good workability.
Źródło:
Archives of Foundry Engineering; 2014, 14, 3; 33-36
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of T6 heat treatment on mechanical properties and microstructure of EN AB-42000 alloy modified with strontium
Autorzy:
Pezda, J.
Powiązania:
https://bibliotekanauki.pl/articles/381247.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
alloy modification
heat treatment
thermal derivative analysis
mechanical properties
modyfikacja stopu
obróbka termiczna
analiza termiczna
analiza derywacyjna
właściwości mechaniczne
Opis:
Process of silumin properties perfection in scope of classic (simple and cheap) methods is connected with change of morphology of silumin precipitations through: process of alloy modification, maintaining suitable temperature of superheating treatment and pouring into moulds, as well as perfection of heat treatment operations. In the paper are presented results of a tests aimed at investigation of an effects of performed heat treatment operations on change of tensile strength of EN AC-42000 silumin modified with strontium. Investigated alloy was melted in electric resistance furnace. Course of crystallization process was recorded with use of thermal-derivative analysis (ATD), and on base of this analysis one determined temperatures range of heat treatment operations of the alloy. Performed heat treatment operation resulted in change of mechanical properties (Rm, A5) of the investigated alloy, whereas performed tests enabled determination of temperature and duration of solutioning and ageing treatments, which condition improvement of its mechanical properties.
Źródło:
Archives of Foundry Engineering; 2011, 11, 2 spec.; 169-174
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Evaluation of structure and properties of welded joint of magnesium alloy EZ33A-T5
Autorzy:
Kocurek, R.
Adamiec, J.
Powiązania:
https://bibliotekanauki.pl/articles/380590.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
mechanical properties
weldability of alloy
magnesium alloy
EZ33
microstructure
quantitative procedure
właściwości mechaniczne
spawalność stopu
stop magnezu
mikrostruktura stopu
metoda ilościowa
Opis:
In recent years, improvement of casting magnesium alloys welding technology has resulted in an increase in the number of publications on this topic. The symptom of this trend is to replace traditional construction materials of magnesium alloys. Magnesium alloys of Mg-Zn-RE-Zr group are used in the automotive, aerospace and defense industries, mainly as gravitional casts to sand moulds or die-casting. Casting defects often appear in these casts (misruns, micro-shrinkage, cracks). The welding technologies are most often applicable to repair of casts, mainly nonconsumable electrode welding in the inert gas cover. The premise of this research work was to define structure and mechanical properties of welded joints of magnesium alloy EZ33A-T5. For this purpose, were attempted trails welding and conducted non-destructive testing, metallographic and strength mechanical tests allowing to assess the properties of welded joints. Evaluation of properties of welded joints was possible by carrying out welding trials and execution of non-destructive tests and metallographic. Research of the microstructure was used with the methodology and test procedures for the quantitative evaluation of the structure of welded joints which was developed in the Department of Materials Science of Silesian University of Technology.
Źródło:
Archives of Foundry Engineering; 2013, 13, 1 spec.; 65-71
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Evaluation of the Effect of the Cr, Mo, V and W Content in an Al-Si Alloy Used for Pressure Casting on its Proof Stress
Autorzy:
Szymczak, T.
Szymszal, J.
Gumienny, G.
Powiązania:
https://bibliotekanauki.pl/articles/380502.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
mechanical properties
statistical method
multicomponent alloy
Al-Si alloy
pressure casting
proof stress
właściwości mechaniczne
metoda statystyczna
stop wieloskładnikowy
stop Al-Si
odlewanie ciśnieniowe
Opis:
The study presents the results of the application of a statistical analysis for the evaluation of the effect of high-melting additions introduced into a pressure cast Al-Si alloy on the obtained level of its proof stress Rp0.2. The base Al-Si alloy used for the tests was a typical alloy used for pressure casting grade EN AC-46000. The base alloy was enriched with high-melting additions, such as: Cr, Mo, V and W. The additions were introduced into the base Al-Si alloy in all the possible combinations. The content of the particular high-melting addition in the Al-Si alloy was within the scope of 0.05 to 0.50%. The investigations were performed on both the base alloy and alloy with the high-melting element additions. Within the implementation of the studies, the values of Rp0.2 were determined for all the considered chemical compositions of the Al-Si alloy. A database was created for the statistical analysis, containing the independent variables (chemical composition data) and dependent variables (examined Rp0.2 values). The performed statistical analysis aimed at determining whether the examined high-melting additions had a significant effect on the level of Rp0.2 of the Al-Si alloy as well as optimizing their contents in order to obtain the highest values of the Al-Si alloy's proof stress Rp0.2. The analyses showed that each considered high-melting addition introduced into the Al-Si alloy in a proper amount can cause an increase of the proof stress Rp0.2 of the alloy, and the optimal content of each examined high-melting addition in respect of the highest obtained value of Rp0.2 equals 0.05%.
Źródło:
Archives of Foundry Engineering; 2018, 18, 2; 105-111
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Experimental and Simulation Tests on the Impact of the Conditions of Casting Solidification from AlSi9Cu3 Alloy on their Structure and Mechanical Properties
Autorzy:
Hajkowski, J.
Ignaszak, Z.
Powiązania:
https://bibliotekanauki.pl/articles/380310.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
alloy Al-Si-Cu
casting solidification
casting technologies
microstructure
mechanical properties
stop Al-Si-Cu
krzepnięcie odlewu
technologie odlewania
mikrostruktura
właściwości mechaniczne
Opis:
The impact of casting conditions on microstructure a and mechanical properties was described, especially for cast products from AlSi9Cu3 alloy. Particular attention was paid to the parameters of dendritic structure: DAS 1 and DAS 2. Selected mechanical properties (by static tension test) of test castings made using basic technologies of casting: GSC - gravity sand casting, GDC - gravity die-casting and HPDC - high-pressure die-casting, are presented for cast-on test bars and cast separately. Casts were made of the same alloy AlSi9Cu3. Fractures and the zone near the fracture (after static tension test) was subjected to VT - visual tests, PT - penetration tests and metallographic tests. The condition of porosity (fracture zone) was also assessed. The analysis of virtual results was performed using the NovaFlow & Solid system together with the database and they were compared to experimental tests. This way of validation was applied in order to assess the correlation between the local rate of cooling and the size of DAS for GSC, GDC and HPDC technologies. Finally, the correlation between the parameters of structure and mechanical properties with regard to the impact of porosity was signalized.
Źródło:
Archives of Foundry Engineering; 2018, 18, 1; 167-175
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Fabrication And Mechanical Properties Of A Nanostructured Complex Aluminum Alloy By Three-Layer Stack Accumulative Roll-Bonding
Wytwarzanie i właściwości mechaniczne nanostrukturalnego złożonego stopu aluminium wytworzonego przez walcowanie pakietowe trzech warstw
Autorzy:
Lee, S. H.
Lee, S. R.
Powiązania:
https://bibliotekanauki.pl/articles/351499.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
accumulative roll-bonding (ARB)
aluminum alloy
microstructre
mechanical properties
akumulacyjne walcowanie pakietowe
stop aluminium
mikrostruktura
właściwości mechaniczne
Opis:
A multi-layered complex aluminum alloy was successfully fabricated by three-layer stack accumulative roll bonding(ARB) process. The ARB using AA1050 and AA5052 alloy sheets was performed up to 7 cycles at ambient temperature without lubrication. The specimen processed by the ARB showed a multi-layer aluminum alloy sheet in which two aluminum alloys are alternately stacked. The grain size of the specimen decreased with the number of ARB cycles, became about 350nm in diameter after 7cycles. The tensile strength increased with the number of ARB cycles, after 6c it reached 281MPa which is about twice higher than that of the starting material. The microstructures and mechanical properties of a three-layer AA1050/AA5052 alloy fabricated by the ARB were compared to those of the conventional ARB-processed material.
Źródło:
Archives of Metallurgy and Materials; 2015, 60, 2B; 1195-1198
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Formation of Structure and Properties in Casting Processes on the Example of AZ91 Magnesium Alloy
Autorzy:
Augustyn, B.
Szymanek, M.
Kapinos, D.
Boczkal, S.
Korczak, P.
Powiązania:
https://bibliotekanauki.pl/articles/383152.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
innovative foundry technologies
innovative foundry materials
magnesium alloy
AZ91 alloy
RS process
mechanical properties
innowacyjne technologie odlewnicze
innowacyjne materiały odlewnicze
stop magnezu
stop AZ91
właściwości mechaniczne
Opis:
Contemporary materials engineering requires the use of materials characterised by high mechanical properties, as these precisely properties determine the choice of material for parts of machinery and equipment. Owing to these properties it is possible to reduce the weight and, consequently, the consumption of both material and energy. Trying to meet these expectations, the designers are increasingly looking for solutions in the application of magnesium alloys as materials offering a very beneficial strength-to-weight ratio. However, besides alloying elements, the properties are to a great extent shaped by the solidification conditions and related structure. The process of structure formation depends on the choice of casting method forced by the specific properties of casting or by the specific intended use of final product. The article presents a comparison of AZ91 magnesium alloys processed by different casting technologies. A short characteristic was offered for materials processed by the traditional semi-continuous casting process, which uses the solidification rates comprised in a range of 5 - 20⁰C/s, and for materials made in the process of Rapid Solidification, where the solidification rate can reach 106⁰C/s. As a result of the casting process, a feedstock in the form of billets and thin strips was obtained and was subjected next to the process of plastic forming. The article presents the results of structural analysis of the final product. The mechanical properties of the ø7 mm extruded rods were also evaluated and compared.
Źródło:
Archives of Foundry Engineering; 2014, 14, 2; 43-48
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Friction and Wear Properties of Plasma Sprayed YSZ/Ni-Cr-Al Coated 6063-T6 Aluminum Alloy
Autorzy:
Erzi, E.
Dispinar, D.
Yilmaz, S.
Powiązania:
https://bibliotekanauki.pl/articles/383089.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
aluminum alloy
mechanical properties
abrasive wear
plasma spraying
YSZ coating
stop aluminium
właściwości mechaniczne
zużycie ścierne
natryskiwanie
powłoka YSZ
Opis:
In this study T6 heat treated 6063 aluminum alloys were used as substrate material. In order to form a bond between the substrate and the main coating, all samples were coated with Ni-Cr-Al powders. 8 wt% Yttria Stabilized Zirconia powders (YSZ) were coated with plasma spray technique. Thickness of YSZ was 150 m and bond coating was 36 m. XRD and SEM-EDS analyses were performed to characterize the coating layers. These YSZ coated and uncoated samples were subjected to wear testing under different spindle speed, loading and working distance. Wear test results were compared with the kinetic friction coefficients and weight loss values. Wear marks on YSZ coated and uncoated samples were investigated by SEM analysis. By coating with plasma spray technique, the wear resistance of Al alloys was increased without changing the friction coefficient. It was found that spindle speed had significant effect over the wear properties than the load applied. By YSZ coating, wear properties were increased 10 times.
Źródło:
Archives of Foundry Engineering; 2017, 17, 3; 168-174
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies