Acidic leaching of steam gasified, pyrolyzed and incinerated PCB waste from LCD screen
Autorzy:
Szczepaniak, Włodzimierz
Zabłocka-Malicka, Monika
Gurgul, Agnieszka
Ochromowicz, Katarzyna
Powiązania:
https://bibliotekanauki.pl/articles/1450359.pdf
Data publikacji:
2020
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
electronic waste
recycling
metals
thermal treatment
acidic leaching
Opis:
In the recycling of WEEE, two approaches are common: a pyrometallurgical or hydrometallurgical treatment, preceded by a mechanical and/or physical separation. In this study, twostep processing of unmodified waste samples of LCD screen inverters was investigated: hightemperature processing followed by acidic leaching under fixed conditions (1M H2SO4, 90 ℃, 1 bar). The analysis carried out concerned a correlation between the type of HT treatment (pyrolysis, incineration, or gasification) and the dynamics of metals’ leaching from samples pretreated this way. It was found that HT method can act as “thermal disintegration”, since it affects, to a varying degree, the structure of the samples and cause elimination of organics and carbonaceous residue (incineration/gasification). The greatest mass loss (~18%) and the most loosened structure was observed for the gasified sample. Varying oxygen potential in HT-processes correlates well with the leachability of thermally treated inverters. The incineration was found to be the most favorable for copper extraction (>95%) by acidic leaching due to oxidized form of Cu, whereas Cu leaching from pyrolyzed and gasified samples needed oxygen and was controlled by the oxygen supply achieving only 36/43% after 6 h. The course of Pd leaching was similar to copper, although with lower efficiencies; 47% of palladium was extracted from the incinerated sample, and only 4 or 7% from gasified and pyrolyzed samples, respectively. Au was leached immediately but only to a slight extent. Contrary to Pb, leaching of Zn, Sn, Sb, and Ni was gradual, probably due to the formation of alloys with copper.
Źródło:
Physicochemical Problems of Mineral Processing; 2020, 56, 6; 257-268
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies