Tytuł:
Hydrometallurgical treatment of non-sulfide zinc ore for precipitation of zinc oxide nanoparticles
Autorzy:
Abdel-Aal, E.-S. A.
Rashad, M. M.
El-Shazly, A. N.
Ibrahim, I. A.
El-Shahat, M. F.
Powiązania:
https://bibliotekanauki.pl/articles/110748.pdf
Data publikacji:
2016
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
zinc ore
sulfuric acid leaching
filtration rate
zinc sulfate
zinc oxide nanoparticles
MB photocatalytic degradation
Opis:
Acid leaching of Egyptian zinc ore from the Um Gheig area was carried out with sulfuric acid. This study determines the optimum conditions for dissolution of non-sulfide zinc ore. The optimum conditions are 25% -74m particle size, 45 °C temperature, 2 h leaching time, 1.1 stoichiometric molar ratio of H2SO4 to Zn, 1:3 solid/liquid ratio. The maximum filtration rate is 1.6 Mg Zn•m-2•day-1at pressure difference of 0.80 bar. The zinc recovery is about 90%. As the zinc ore contains zinc silicate, some additives were tested to enhance filtration and prevent formation of silica gel. To increase the added value of the product, zinc oxide was precipitated by a co-precipitation method in a nanosize powder with average particle size ~ 20 nm. Photocatalytic degradation of methylene blue dye under UV light using ZnO nanopowders produced at different conditions was investigated. Photocatalytic efficiency with methylene blue (MB) concentration was reduced as much as 85% in 240 min with the produced nanoparticles.
Źródło:
Physicochemical Problems of Mineral Processing; 2016, 52, 2; 729-737
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effect of particle shape properties on selective separation of chromite from serpentine by flotation
Autorzy:
Guven, Onur
Serdengecti, M. Tayhan
Tunc, Berivan
Ozdemir, Orhan
Karaagaclioglu, Ibrahim E.
Çelik, Mehmet S.
Powiązania:
https://bibliotekanauki.pl/articles/1845205.pdf
Data publikacji:
2020
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
chromite
serpentine
morphology
flotation
mineral mixtures
Opis:
Although many studies have been conducted on the morphological variations and its effects on flotation recoveries of a single mineral system, a systematic study for the flotation behavior of mixtures of minerals has not dwelled much. In this study, th flotation behavior of chromite and serpentine minerals was investigated to distinguish and isolate the contribution of morphology in single and binary systems. For this purpose, the shape analyses for the minerals ground as single and mixture were performed, and their flotation behaviors determined with the micro-flotation experiments. Additionally, the zeta potential measurements were carried out in the presence of sodium oleate as a collector. The shape analysis of the ground samples showed that while the roundness values of chromite and serpentine (gangue) minerals as single were quite different, the particle shape of chromite favored serpentine in the mixture system which in turn suggested that the mineral with the high hardness value dominates the shape characteristics in binary grinding conditions. Accordingly, while the flotation characteristics of chromite in the mixture followed the same trend with the flotation of a single chromite system as a function of particle shape, almost a reverse trend was obtained for the shape and flotation of serpentine in the mixture compared to a single serpentine system. Thus, at roundness values of chromite particles from 0.797 to 0.732, the flotation recoveries of chromite in the mixture increased from 51.0% to 75.4%. On the other hand, likewise chromite, the flotation recoveries of serpentine increased from 20.0% to 37.3% proportional to the roundness range of 0.757 and 0.709. These findings in turn showed that the grinding conditions dictate the soft component to be monitored by the harder and denser component which dominates the angularity and floatability of the mixture.
Źródło:
Physicochemical Problems of Mineral Processing; 2020, 56, 5; 818-828
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Role of ammonium phosphate in improving the physical characteristics of malachite sulfidation flotation
Autorzy:
Ibrahim, Ayman M.
Jia, Xiaodong
Cai, Jinpeng
Su, Chao
Yu, Xingcai
Zheng, Qifang
Peng, Rong
Shen, Peilun
Liu, Dianwen
Powiązania:
https://bibliotekanauki.pl/articles/2200339.pdf
Data publikacji:
2023
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
malachite sulfidation
sample preparation
ammonium phosphate
sodium sulfide
floatability
physical characteristics
Opis:
In this study, ammonium phosphate ((NH4)3PO4) was employed to realize improvement by modifying the physical characteristics of the malachite surface, ensuring sustainable flotation throughout the flotation operations, and enhancing the flotation process to be more stable. Furthermore, various techniques, including X-ray photoelectron spectroscopy, were intensely used to investigate the configuration and physico-chemical surface characteristics through micro-flotation experiments, contact angle and zeta potential measurements, and XRD, ToF-SIMS, EPMA, and FTIR spectrum analyses. The FTIR findings showed that new characteristic peaks of -C(=S)-N.H. groups formed and adsorbed on the surfaces of malachite at 1636 cm-1. The -CH2 groups throughout the flotation process, further promoted the attachment of the CH3 ligand to the Cu2+ ion, and the XPS analysis confirmed this. Consequently, it can be concluded that (NH4)3PO4 played a substantial part in the improved recovery rate, as demonstrated and confirmed by the methods carried out in this study. Thus, it was used to modify the physical properties surface before adding Na2S to efficiently enhance malachite floatability and reduce the loss rate of malachite. Regarding the alterations in the physical characteristics which occurred to the malachite surface, and as a consequence of increasing the recovery results of flotation, the malachite sample treated initially with (NH4)3PO4 exhibited micro flotation results with a considerably greater flotation recovery than malachite treated initially with only Na2S ions.
Źródło:
Physicochemical Problems of Mineral Processing; 2023, 59, 1; art. no. 161510
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies