AMADEUS Project - Opis:
- In this work, for the first time the results of an experimental evaluation of the high temperature behavior of molten Si-B alloy in contact with refractory materials at temperatures up to 1750°C, under static argon atmosphere (p = 850– 900 mbar), is shown. The material investigated, having a nominal chemical composition of Si-13.5B (at. %), was fabricated by using the crucible-less electric arc-melting process assisted by the levitation drop method. The wettability of the molten alloy in contact with commercial hexagonal boron nitride (h-BN) substrates was evaluated by means of especially developed sessile drop technique combined with a contact heating procedure. It was found that both couples show a lack of wettability in the whole tested temperature range (the measured contact angle was θ > 130°). The more stable behavior in contact with molten Si-13.B alloy, evidenced by higher θ values and a lack of drop vibration during the high temperature exposition, was observed for the h-BN based composite substrate.
- Źródło:
-
Prace Instytutu Odlewnictwa; 2017, 57, 4; 321-326