Tytuł:
The influence of heat treatment on point defect concentration in Fe-Al and Fe-Al-Cr systems
Autorzy:
Kansy, J.
Hanc, A.
Giebel, D.
Powiązania:
https://bibliotekanauki.pl/articles/146336.pdf
Data publikacji:
2010
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
positron annihilation
Fe-Al
Fe-Al-Cr
point defects
Opis:
FeAl alloys of nominal Al content 28, 38 and 45 at.% and Fe28Al5Cr with minor alloying elements added to improve their application properties are studied by positron annihilation lifetime analysis. The lifetime spectra of samples FeXAl with X greater-than or equal to 38 (both quenched and cooled with furnace) are described by a single lifetime component related to the saturated positron trapping by quenched-in vacancies of concentration much higher than 100 ppm. A very strong dependence of retained vacancy concentration on the rate of cooling is shown for Fe28Al and Fe28Al5Cr alloys. After quenching, the concentration is of the order of 10.4 whereas in samples slowly cooled it is reduced to 10.5. The chromium addition to Fe28Al5Cr dismisses the vacancies concentration in comparison to the concentration in Fe28Al after the same heat treatment.
Źródło:
Nukleonika; 2010, 55, 1; 21-25
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Change of the defect structure in FeAl alloy as a result of its aging at ambient temperature
Autorzy:
Kansy, J.
Hanc-Kuczkowska, A.
Giebel, D.
Powiązania:
https://bibliotekanauki.pl/articles/148012.pdf
Data publikacji:
2013
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
PALS
FeAl
LT10
defect structure
Opis:
Positron annihilation lifetime spectroscopy (PALS) was used to study the defect structure of stoichiometric FeAl samples after their slow cooling or quenching from the temperatures of 1000 and 540 centigrade. The high value of positron lifetime in the quenched-in defects suggests that they are mainly of di-vacancy type. After long storage at ambient temperature, the concentration of defects in the samples strongly decreases and mono-vacancies predominate. Annealing at 540 centigrade generates an additional amount of defects may be ascribed to the formation of FeAl2 phase in the FeAl matrix.
Źródło:
Nukleonika; 2013, 58, 1; 221-224
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies