The experimental and theoretical investigations of damage development and distribution in double-forged tungsten under plasma irradiation-initiated extreme heat loads
Autorzy:
Väli, B.
Laas, T.
Paju, J.
Shirokova, V.
Paduch, M.
Gribkov, V. A.
Demina, E. V.
Pimenov, V. N.
Makhlaj, V. A.
Antonov, M.
Powiązania:
https://bibliotekanauki.pl/articles/148167.pdf
Data publikacji:
2016
Wydawca:
Instytut Chemii i Techniki Jądrowej
Tematy:
divertor material
nuclear fusion
off-normal events
thermal shock
tungsten
Opis:
The influence of extreme heat loads, as produced by a multiple pulses of non-homogeneous flow of slow plasma (0.1–1 keV) and fast ions (100 keV), on double-forged tungsten (DFW) was investigated. For generation of deuterium plasma and fast deuterons, plasma-focus devices PF-12 and PF-1000 are used. Depending on devices and conditions, the power flux density of plasma varied in a range of 107–1010 W/cm2 with pulse duration of 50–100 ns. Power flux density of fast ions was 1010–1012 W/cm2 at the pulse duration of 10–50 ns. To achieve the combined effect of different kind of plasmas, the samples were later irradiated with hydrogen plasma (105 W/cm2, 0.25 ms) by a QSPA Kh-50 plasma generator. Surface modification was analysed by scanning electron microscopy (SEM) and microroughness measurements. For estimation of damages in the bulk of material, an electrical conductivity method was used. Investigations showed that irradiation of DFW with multiple plasma pulses generated a mesh of micro- and macrocracks due to high heat load. A comparison with single forged tungsten (W) and tungsten doped with 1% lanthanum-oxide (WL10) reveals the better crack-resistance of DFW. Also, sizes of cells formed between the cracks on the DFW’s surface were larger than in cases of W or WL10. Measurements of electrical conductivity indicated a layer of decreased conductivity, which reached up to 500 µm. It depended mainly on values of power flux density of fast ions, but not on the number of pulses. Thus, it may be concluded that bulk defects (weakening bonds between grains and crystals, dislocations, point-defects) were generated due to mechanical shock wave, which was generated by the fast ions flux. Damages and erosion of materials under different combined radiation conditions have also been discussed.
Źródło:
Nukleonika; 2016, 61, 2; 169-177
0029-5922
1508-5791
Pojawia się w:
Nukleonika
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies