Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "anion resin" wg kryterium: Temat


Wyświetlanie 1-2 z 2
Tytuł:
Nondestructive Radioactive Tracer Technique in Characterization of Anion Exchange Resins Purolite NRW-8000 and Duolite A-368
Autorzy:
Singare, P.U.
Powiązania:
https://bibliotekanauki.pl/articles/411749.pdf
Data publikacji:
2013
Wydawca:
Przedsiębiorstwo Wydawnictw Naukowych Darwin / Scientific Publishing House DARWIN
Tematy:
ion-exchange resin
anion exchange
Purolite NRW-8000
Duolite A-368
radio tracer isotopes
131I
82Br
characterization
isotopic Exchange
Opis:
Radioactive tracer isotopes 131I and 82Br were used to characterize anion exchange resins Purolite NRW-8000 and Duolite A-368 by application of nondestructive technique. The resin characterization was based on their performance during iodide and bromide ion-isotopic exchange reactions. It was observed that during the iodide ion-isotopic exchange reaction at a constant temperature of 40.0 °C, as the concentration of labeled iodide ion solution increases from 0.001 mol/L to 0.004 mol/L, the percentage of iodide ions exchanged increases from 62.10 % to 68.10 % using Purolite NRW-8000 resins and from 44.20 % to 46.80 % using Duolite A-368 resins. Also at a constant temperature of 40.0 °C, 1.000 g of ion exchange resins and 0.003 mol/L labeled iodide ion solution, the values of specific reaction rate (min-1), amount of iodide ion exchanged (mmol), initial rate of iodide ion exchange (mmol/min) and log Kd were calculated as 0.260, 0.500, 0.130 and 11.8 respectively for Purolite NRW-8000 resin, which was higher than the respective values of 0.130, 0.345, 0.045 and 6.7 as that obtained for Duolite A-368 resins. The similar trend was observed for the two resins during bromide ion-isotopic exchange reaction. From the overall results it appears that under identical experimental conditions, Purolite NRW-8000 resins show superior performance over Duolite A-368 resins. It is expected here that the present nondestructive technique can be extended further for characterization of different industrial grade ion exchange resins, which will help in their selection for specific industrial application.
Źródło:
International Letters of Chemistry, Physics and Astronomy; 2013, 12; 14-27
2299-3843
Pojawia się w:
International Letters of Chemistry, Physics and Astronomy
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Non Destructive Application of Radioactive Tracer Isotopes for Performance Evaluation of Industrial Grade Anion Exchange Resins Tulsion A-33 and Indion NSSR
Autorzy:
Singare, P. U.
Powiązania:
https://bibliotekanauki.pl/articles/411857.pdf
Data publikacji:
2013
Wydawca:
Przedsiębiorstwo Wydawnictw Naukowych Darwin / Scientific Publishing House DARWIN
Tematy:
radioisotopes
non-destructive technique
Tulsion A-33
Indion NSSR
nuclear grade resin
anion exchange resins
performance evaluation
operational parameters
131I
82Br
Opis:
The present study deals with non-destructive application of radioactive tracer isotopes to evaluate the performance of Tulsion A-33 (nuclear grade) and Indion NSSR (non-nuclear grade) anion exchange resins. The performance evaluation was done by carrying out the iodide and bromide ion-isotopic exchange reactions using the above resins. It was observed that at a constant temperature of 40.0 °C, as the concentration of labeled iodide ion solution increases 0.001 M to 0.004 M, the percentage of iodide ions exchanged increases from 58.0 % to 64.0 % for Tulsion A-33 resins; and from 48.4 % to 50.8 % for Indion NSSR resins. Similarly in case of bromide ion-isotopic exchange reaction under identical experimental conditions, the percentage of bromide ions exchanged increases from 45.6 % to 50.4 % for Tulsion A-33 resin; and from 39.8 % to 44.6 % for Indion NSSR resin. It was also observed that during iodide ion-isotopic exchange reaction at 40.0 °C, using 1.000 g of ion exchange resins and 0.003 M labeled ionic solution, using Tulsion A-33 resin the values of specific reaction rate (min-1), amount of iodide ion exchanged (mmol), initial rate of iodide ion exchange (mmol/min) and log Kd were 0.229, 0.469, 0.107 and 10.6 respectively, which was higher than the values of 0.167, 0.375, 0.063 and 7.6 respectively as obtained by using Indion NSSR resins under identical experimental conditions. The overall results indicate superior performance of Tulsion A-33 over Indion NSSR resin under identical operational parameters.
Źródło:
International Letters of Chemistry, Physics and Astronomy; 2013, 13; 50-62
2299-3843
Pojawia się w:
International Letters of Chemistry, Physics and Astronomy
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-2 z 2

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies