Tytuł:
The Impact of the Thickness of the Ceramic Shell Mould on the (γ + γ) Eutectic in the IN713C Superalloy Airfoil Blade Casting
Autorzy:
Szczotok, A.
Nawrocki, J.
Pietraszek, J.
Powiązania:
https://bibliotekanauki.pl/articles/356978.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
investment casting
IN713C superalloy
(y+y') eutectic
computing methods
statistical analysis
repeatability
Opis:
In the study the wall thickness of ceramic shell mould influence on (γ + γ') eutectic in the IN713C nickel-based superalloy airfoil blade casting was described. Two castings formed as a blade from two wax pattern assemblies were analysed. In the experiment in one pattern the thick ceramic layer was obtained on pressure side and in another one on suction side of the airfoil blade. The microstructure of the crosssections of the castings were observed on polished and etched metallographic specimens. The microstructure and phases chemical compositions of specimens was analyzed by using the scanning electron microscope Hitachi S-4200 equipped with EDS. It was established, that wall thickness of ceramic shell mould affect size, shape and volume fraction of (γ + γ') eutectic islands in airfoil blade made from IN713C superalloy. The analysis was provided in accordance to the typical statistical methodology [1].
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 2A; 587-593
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Evaluation of Carbides in Turbine Blade Made of IN713C Superalloy After Hot Isostatic Pressing
Autorzy:
Kościelniak, B.
Roskosz, S.
Cwajna, J.
Powiązania:
https://bibliotekanauki.pl/articles/351248.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
IN713C superalloy
hot isostatic pressing
turbine blades
qualitative and quantitative analysis of carbides
Opis:
The IN713C is nickel-based superalloy, used to produce low pressure turbine blades in a process of investment casting. However, porosity which is formed during the casting, decreases mechanical properties of IN713C. Therefore, to eliminate porosity, a process of hot isostatic pressing was applied. Nonetheless, HIP also least to some changes in the microstructure of tested material. The main aim of this paper is to characterize the morphology of carbides before and after hot isostatic pressing. Microstructural characterization was carried out with the use of a scanning electron microscope equipped with an energy dispersive X-ray spectrometer and an electron backscatter diffraction detector. The size and shape of carbides were evaluated by quantitative metallography methods methods. The results show that the amount, size and heterogeneity of arrangement of the carbides increased after application of HIP treatment.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 1; 247-252
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The fixed-effects analysis of the relation between SDAS and carbides for the airfoil blade traces
Autorzy:
Pietraszek, J.
Szczotok, A.
Radek, N.
Powiązania:
https://bibliotekanauki.pl/articles/351316.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
microstructure
SDAS
IN713C
superalloy
Opis:
The primary objective was to test a usefulness of the specific fixed-effect model for the analysis of quantitative relationships gathered from the image analysis of the material microstructures. The dataset was obtained from the investigation of turbine blades made from superalloy IN713C. The analysis based on the general linear model resulted in informative plots revealing mutual relationships between secondary dendrite arm spacing and the mean plane section area of carbides in the material. Directions for further research also were obtained.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 1; 235-239
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Metallographic Study and Repeatability Analysis of γ Phase Precipitates in Cored, Thin-Walled Castings Made from IN713C Superallo
Autorzy:
Szczotok, A.
Pietraszek, J.
Radek, N.
Powiązania:
https://bibliotekanauki.pl/articles/354156.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
IN713C
superalloy
γ' phase
metallography
statistical analysis
Opis:
The study describes the influence of a surface modification in cored, thin-walled castings of blades from IN-713C nickel superalloy on γ' phase precipitates. The blades were produced by using the investment casting process in the laboratory conditions as parts for a low-pressure turbine rotor. The microstructural observations of the γ' phase precipitates on the cross sections of the blades were performed. The observations were followed by quantitative metallography evaluation, and finally, a comparison of the precipitates between one blade with the conventionally applied ceramic core and one with the core covered layer contained a surface modifier (5% of CoAl2O4) was made.
Źródło:
Archives of Metallurgy and Materials; 2017, 62, 2A; 595-601
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-4 z 4

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies