Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Du, Y." wg kryterium: Autor


Wyświetlanie 1-3 z 3
Tytuł:
Effect of minor Cu addition on the precipitation sequence of an as-cast Al-Mg-Si 6005 alloy
Wpływ niewielkiej zawartości miedzi na sekwencje wydzieleń w odlewanych stopach Al-Mg-Si 6005
Autorzy:
Li, K.
Song, M.
Du, Y.
Fang, X.
Powiązania:
https://bibliotekanauki.pl/articles/355082.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stopy aluminium
dyfrakcja rentgenowska
transmisyjna mikroskopia elektronowa
badania twardości
aluminum alloys
precipitation
ageing
phase transformation
Opis:
The whole precipitation sequences of two as-cast Al-Mg-Si 6005 alloys (containing no Cu or 0.1 wt.% Cu) at 150 degree Celsjus were investigated using X-ray diffraction, transmission electron microscopy and hardness examinations. The precipitation sequence of the Cu-free alloy can be expressed as: super-saturated solid solution (SSSS) → spherical G.P. zones → pre - β'' → β'' → U2 +Si + β x → Si + β β xwhile that of the Cu-containing alloy can be expressed as: SSSS → spherical G.P. zones + platelet-like G.P. zones → pre - β → β'' → Q' + β + Si → Q + β + Si. A new type of βprecipitate, namely β x here, has been discovered in the Cu-free alloy. The addition of minor Cu is found to accelerate the microstructural evolution by inducing the formation of a new type of platelet-like G.P. zone along {111} Al planes, and improve the hardening response at the over-aged stage by forming Q' and Q precipitates.
Kompletna sekwencja wydzieleń dwóch odlanych stopów Al-Mg-Si 6005 (zawierąjacych 0 i 0.1%.wag Cu), w temperaturze 150 stopni Celsjusza, została zbadana przy użyciu dyfrakcji rentgenowskiej, transmisyjnej mikroskopii elektronowej i badań twardości. Sekwencja wydzieleń w stopie nie zawierającym Cu może być przedstawiona następująco: przesycony roztwór stały → sferyczne strefy Guiniera-Prestona → pre - β'' → β'' → U2 +Si + β x → Si + β β x natomiast dla stopu zawierającego Cu następująco: przesycony roztwór stały → sferyczne i płytkowe strefy Guiniera-Prestona → pre - β → β'' → Q' + β + Si → Q + β + Si. Nowy rodzaj wydzieleń β, tj. β x , został odkryty w stopie niezawierajacym Cu. Stwierdzono, że dodatek niewielkiej ilości Cu przyspiesza zmiany mikrostruktury poprzez indukowanie tworzenia nowego typu płytkowych stref Guiniera-Prestona wzdłuż płaszczyzny {111}Al. i poprawia utwardzenie poprzez tworzenie wydzieleń Q' i Q.
Źródło:
Archives of Metallurgy and Materials; 2012, 57, 2; 458-466
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Y Addition Effects on Hot Deformation Behavior of Cu-Zr Alloys with High Zr Content
Autorzy:
Tian, K.
Tian, B.
Volinsky, A. A.
Zhang, Y.
Liu, Y.
Du, Y.
Powiązania:
https://bibliotekanauki.pl/articles/350979.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Cu-1%Zr alloy
high Zr content
yttrium
hot deformation activation energy
dynamic recrystallization
Opis:
Isothermal hot compression experiments were carried out using the Gleeble-1500D thermal mechanical simulator. The flow stress of the Cu-1%Zr and Cu-1%Zr-0.15%Y alloys was studied at hot deformation temperature of 550°C, 650°C, 750°C, 850°C, 900°C and the strain rate of 0.001 s-1, 0.01 s-1, 0.1 s-1, 1 s-1, 10 s-1. Hot deformation activation energy and constitutive equations for two kinds of alloys with and without yttrium addition were obtained by correlating the flow stress, strain rate and deformation temperature. The reasons for the change of hot deformation activation energy of the two alloys were analyzed. Dynamic recrystallization microstructure evolution for the two kinds of alloys during hot compression deformation was analyzed by optical and transmission electron microscopy. Cu-1%Zr and Cu-1%Zr-0.15%Y alloys exhibit similar behavior of hot compression deformation. Typical dynamic recovery occurs during the 550-750°C deformation temperature, while dynamic recrystallization (DRX) occurs during the 850-900°C deformation temperature. High Zr content and the addition of Y significantly improved Cu-1%Zr alloy hot deformation activation energy. Compared with hot deformation activation energy of pure copper, hot deformation activation energy of the Cu-1%Zr and Cu-1%Zr-0.15%Y alloys is increased by 54% and 81%, respectively. Compared with hot deformation activation energy of the Cu-1%Zr alloy, it increased by 18% with the addition of Y. The addition of yttrium refines grain, advances the dynamic recrystallization critical strain point and improves dynamic recrystallization.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 2; 875-882
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
A Visual Detection Method of Longitudinal Crack Based on Computer Image Processing During Slab Continuous Casting
Autorzy:
Liu, Y.
Wang, X.
Sun, Y.
Du, F.
Gao, Y.
Wang, F.
Wang, J.
Powiązania:
https://bibliotekanauki.pl/articles/351636.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
longitudinal crack
visual detection
image processing
continuous casting
Opis:
Based on the mould temperature measured by thermocouples during slab continuous casting, a difference of temperature thermograph is developed to detect slab cracks. In order to detect abnormal temperature region caused by longitudinal crack, the suspicious regions are extracted and divided by virtue of computer image processing algorithms, such as threshold segmentation, connected region judgement and boundary tracing. The abnormal regions are then determined and labeled with the eight connected component labeling algorithm. The boundary of abnormal region is also extracted to depict characteristics of longitudinal crack. Based on above researches, longitudinal crack with abnormal temperature region can be detected and is different from other abnormalities. Four samples of temperature drop are picked up to compare with longitudinal crack on the abnormal region formation, length, width, shape, et al. The results show that the abnormal region caused by longitudinal crack has a linear and vertical shape. The height of abnormal region is more than the width obviously. The ratio of height to width is usually larger than that of other temperature drop regions. This method provides a visual and easy way to detect longitudinal crack and other abnormities. Meanwhile it has a positive meaning to the intelligent and visual mould monitoring system of continuous casting.
Źródło:
Archives of Metallurgy and Materials; 2018, 63, 2; 673-680
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-3 z 3

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies