Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę ""Spawanie laserowe"" wg kryterium: Wszystkie pola


Wyświetlanie 1-1 z 1
Tytuł:
Assessment of gold with titanium alloy weldability in conditions of a dental technique laboratory
Autorzy:
Jania, G.
Żmudzki, J.
Topolska, S.
Powiązania:
https://bibliotekanauki.pl/articles/24200598.pdf
Data publikacji:
2022
Wydawca:
Stowarzyszenie Komputerowej Nauki o Materiałach i Inżynierii Powierzchni w Gliwicach
Tematy:
titanium alloy
gold
laser welding
prosthetic
implant denture
microstructure
stop tytanu
złoto
spawanie laserowe
protetyka
proteza implantu
mikrostruktura
Opis:
Purpose: In dental practice, there is necessary to weld gold with titanium under the conditions of a dental technique laboratory, which is difficult. The aim was to assess the weldability of pure gold with the titanium alloy Ti6Al4V using a prosthetic laser welding machine. Design/methodology/approach: Gold wire in a diameter of 0.4 mm made with the use of a jewellery drawbar (GOLDPORT, Szczecin, Poland) was welded to a titanium alloy Ti6Al4V substrate of dental implant abutment screw (MegaGen). Dental laser welding parameters (Bego Laser Star T plus) were 230 V; 6.5 ms; 2.5 Hz; laser spot 0.3 mm, and argon blow. Samples were included in resin, ground (500-4000 SiC), polished (Al2O3 suspension) and etched (Kroll solution) per 20 s before observation under a light microscope. Findings: There were well-welded and poorly joined zones. The discontinuities and voids there were not visible or sparse next to the initial weld point. Dendritic structure at well-welded remelting zones and two-phase microstructure of titanium and Ti3Au phase were found. The heat-affected zone was about of 20 microns. Research limitations/implications: Light microscopy was used, and precise phase identification required further investigations. Weld strength assessment requires further micro-hardness and load-bearing ability tests. Weldability concerns the model system with pure gold. Practical implications: In the case of elements with dimensions below 0.4 mm, the use of a laser with a smaller spot should be considered for better control of the remelting zone and mechanical positioning of the elements in order to stabilize and avoid discontinuities and voids. Originality/value: Prosthetic laser welding with a laser spot about of 0.3 mm allows to obtain well-welded parts of 0.3 mm in diameter under stable stitching conditions and higher than 0.4 mm in dimensions.
Źródło:
Archives of Materials Science and Engineering; 2022, 118, 1; 36--41
1897-2764
Pojawia się w:
Archives of Materials Science and Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies