Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "TI" wg kryterium: Temat


Wyświetlanie 1-9 z 9
Tytuł:
Research on the Characterization of Ti Inclusions and Their Precipitation Behavior in Tire Cord Steel
Autorzy:
Lei, Jialiu
Zhao, Dongnan
Fu, Yongjun
Xu, Xianfeng
Powiązania:
https://bibliotekanauki.pl/articles/383339.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
precipitation behavior
Ti inclusions
concentration product
tire cord steel
characterization
linka stalowa
wtrącenia Ti
odpady
Opis:
In the present investigation, the morphology of Ti inclusions in high strength tire cord steel was investigated and their precipitation behavior was discussed using a precipitation and growth model. The results show that Ti inclusions mainly exist in the form of TiN. The two-dimensional characterization of Ti inclusions is square-like with sharp edges and corners, while its three-dimensional shape exhibits a cubic or rectangular-prism morphology. The Ti inclusions do not precipitate when the solid fraction of tire cord during solidification is less than 0.987, and their final radius is closely related to the cooling rate and initial concentration product. The higher the cooling speed, the smaller the final radius, when the cooling speed is constant, the final radius of Ti inclusions is mainly determined by the initial concentration product, w[N]0×w[Ti]0. In order to retard the precipitation and growth of Ti inclusions in tire cord steel, the cooling rate and initial concentration product can be taken into consideration.
Źródło:
Archives of Foundry Engineering; 2019, 3; 33-37
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Structural stability of the high-aluminium zinc alloys modified with Ti addition
Autorzy:
Krajewski, W. K.
Zak, P. L.
Orava, J.
Greer, A. L.
Krajewski, P. K.
Powiązania:
https://bibliotekanauki.pl/articles/382429.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
wysokoaluminiowy stop cynku
dodatek Ti
stabilność strukturalna
high-aluminium zinc alloys
Ti addition
structural stability
XRD examinations
Opis:
The subject of the paper is structural stability of the Zn-26 wt.% Al binary alloys doped with 2.2 wt.% Cu or 1.6 wt.% Ti addition. The structural stability of Zn-Al alloys with increased Al content is connected with stability of solid solution of zinc in aluminium [...] , which is the main component of these alloys microstructure. Such a solution undergoes phase transformations which are accompanied, among others, by changes in dimensions and strength properties. The structural stability of the ZnAL26Cu2.2 and ZnAl26Ti1.6 alloys was investigated using XRD examinations during long term natural ageing after casting, as well as during long term natural ageing after super-saturation and quenching. On the basis of the performed examinations it was stated that small Ti addition to the binary ZnAl25 alloy, apart from structure refinement, accelerates decomposition of the primary [...] phase giving stable structure in a shorter period of time in comparison with the alloy without Ti addition. Addition of Ti in amount of 1.6 wt.%, totally replacing Cu, allows obtaining stable structure and dimensions and allows avoiding structural instability caused by the metastable [...] CuZn4 phase present in the ZnAl26Cu2.2 alloy.
Źródło:
Archives of Foundry Engineering; 2012, 12, 1; 61-66
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Aluminium loss during Ti-Al-X alloy smelting using the VIM Technology
Autorzy:
Smalcerz, Albert
Blacha, L.
Łabaj, J.
Powiązania:
https://bibliotekanauki.pl/articles/1837812.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
melting of Ti-Al alloys
induction vacuum furnace
evaporation of metals
stopy Ti-Al
indukcyjny piec próżniowy
odparowanie
Opis:
Titanium alloys belonging to the group of modern metallic materials used in many industries, including the aerospace industries. Induction crucible vacuum furnaces and induction furnaces with cold crucible are most commonly used for their smelting. When operating these devices, one can deal with an adverse phenomenon of decrease in the content of alloy elements that are characterized by higher equilibrium vapour pressure than the matrix metal or titanium, in the metal bath. In the paper, results of the study on aluminium evaporation from the Ti-Al-Nb, Ti-Al-V and Ti-Al alloys (max 6.2 % wt.) during smelting in a vacuum induction melting (VIM) furnace are presented. The experiments were performed at 10 to 1000 Pa for 1973 K and 2023 K. A significant degree of aluminium loss has been demonstrated during the analysed process. The values of relative aluminium loss for all the alloys ranged from 4 % to 25 %. Lowering the pressure in the melting system from 1000 Pa to 10 Pa resulted in increased values of aluminium evaporation flux from 4.82⋅10-5 to 0.000327 g⋅cm-2⋅s-1 for 1973 K and from 9.28⋅10-5 to 0.000344 g⋅cm-2⋅s-1 for 2023 K. The analysis of the results obtained took into account the value of the actual surface of the liquid metal. In the case of melting metals in an induction furnace, this surface depends on the value of power emitted in the charge. At greater power, we observe a significant increase in the bath surface due to the formation of a meniscus.
Źródło:
Archives of Foundry Engineering; 2021, 21, 1; 11-17
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Analysis of Ti6Al4V P/M Properties Under Thermomechanical Compression Tests
Autorzy:
Sleboda, T.
Fourie, J.
Powiązania:
https://bibliotekanauki.pl/articles/379823.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Ti6Al4V alloy
thermomechanical condition
compression test
stop Ti6Al4V
warunki termomechaniczne
próba ściskania
Opis:
Since titanium powder metallurgy poses opportunities for the manufacture of a range of components, there now exists the need to establish its performance characteristics under industrial conditions that these components need to operate under. In line with this, there is a need to analysing amongst others the mechanical properties of Ti6Al4V P/M [1, 5] under various thermomechanical conditions and compression tests. The main objective of the research is to study and compare the properties after forging of high quality Ti6Al4V powder metallurgy alloy with that of titanium ingot. Both samples has been manufactured under the same thermo mechanical conditions. P/M alloy will be prepared from the mixture of elemental powders, and will have the chemical composition of that of ingot Ti6Al4V alloy as per ASTM 1580-1 standard. Powder mixtures will be fully densified by hot compaction under precisely controlled conditions using the Thermal Technology Inc. press at AGH University of Science and Technology in Poland. Various physical tests will be conducted including mechanical property tests and microstructural analysis. Additionally simulations will be performed using simulation software, GForm ™ , using parameters used on actual forgings. Results will be compared to physical tests performed earlier.
Źródło:
Archives of Foundry Engineering; 2013, 13, 3 spec.; 149-152
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Metal-metal Cast Composites
Autorzy:
Braszczyńska-Malik, K. N.
Przełożyńska, E.
Powiązania:
https://bibliotekanauki.pl/articles/382051.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
composite
AZ91
magnesium alloys
Ti6Al4V particles
microstructure
kompozyt
stop magnezu
cząstki Ti6Al4V
mikrostruktura
Opis:
Microstructure of experimental AZ91 magnesium matrix composite with Ti6Al4V particles is presented. Composite were fabricated by casting method. The obtained experimental composite exhibited uniform distribution of Ti6Al4V particles within the matrix alloy. Neither clusters of particles nor any new phases creating during component reactions are observed.
Źródło:
Archives of Foundry Engineering; 2014, 14, 3 spec.; 110-113
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Aluminium loss during Ti-Al-X alloy smelting using the VIM Technology
Autorzy:
Smalcerz, A.
Blacha, L.
Łabaj, J.
Powiązania:
https://bibliotekanauki.pl/articles/1837853.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
melting of Ti-Al alloys
induction vacuum furnace
evaporation of metals
Opis:
Titanium alloys belonging to the group of modern metallic materials used in many industries, including the aerospace industries. Induction crucible vacuum furnaces and induction furnaces with cold crucible are most commonly used for their smelting. When operating these devices, one can deal with an adverse phenomenon of decrease in the content of alloy elements that are characterized by higher equilibrium vapour pressure than the matrix metal or titanium, in the metal bath. In the paper, results of the study on aluminium evaporation from the Ti-Al-Nb, Ti-Al-V and Ti-Al alloys (max 6.2 % wt.) during smelting in a vacuum induction melting (VIM) furnace are presented. The experiments were performed at 10 to 1000 Pa for 1973 K and 2023 K. A significant degree of aluminium loss has been demonstrated during the analysed process. The values of relative aluminium loss for all the alloys ranged from 4 % to 25 %. Lowering the pressure in the melting system from 1000 Pa to 10 Pa resulted in increased values of aluminium evaporation flux from 4.82⋅10-5 to 0.000327 g⋅cm-2⋅s-1 for 1973 K and from 9.28⋅10-5 to 0.000344 g⋅cm-2⋅s-1 for 2023 K. The analysis of the results obtained took into account the value of the actual surface of the liquid metal. In the case of melting metals in an induction furnace, this surface depends on the value of power emitted in the charge. At greater power, we observe a significant increase in the bath surface due to the formation of a meniscus.
Źródło:
Archives of Foundry Engineering; 2021, 21, 1; 11-17
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Possibilities of Fabricating Mg-Al-RE Cast Magnesium Matrix Composites Reinforced with Ti Particles
Autorzy:
Przełożyńska, E.
Braszczyńska-Malik, K. N.
Powiązania:
https://bibliotekanauki.pl/articles/379632.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
magnesium matrix composite
Mg-Al-Mn alloy
rare earth elements (REE)
Ti particle
microstructure investigations
kompozyt magnezowy
stop Mg-Al-Mn
pierwiastki ziem rzadkich
cząstka Ti
badania mikrostruktury
Opis:
The results of microstructure investigations of an experimental magnesium matrix composite reinforced with Ti particles are presented. The experimental Mg-5Al-5RE magnesium alloy was used as the matrix alloy. The examined composite was reinforced with 30 wt% titanium spherical particles. The investigated material was obtained by the stir-casting method. The microstructure of the fabricated composite was characterized by a uniform arrangement of the Ti particles within the magnesium matrix. No new phases (created due to reaction between the matrix and Ti particles) were revealed by XRD techniques.
Źródło:
Archives of Foundry Engineering; 2015, 15, 3 spec.; 73-76
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The quality of welded connections elements from the steel 30HGS and titanium alloy Ti6Al4V
Autorzy:
Łapiński, Z.
Dziedzic, A.
Bochnowski, W.
Adamiak, S.
Sandomierski, S.
Powiązania:
https://bibliotekanauki.pl/articles/382853.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
obróbka cieplna
metalografia
mikrotwardość
spawanie
stop tytanu Ti-6Al-4V
stal 30HGS
heat treatment
metallography
factography
microhardness
welding
head weld
titanium alloy Ti-6Al-4V
steel 30HGS
Opis:
The aim of that work was the evaluation of the quality of welded connections elements (welds) from the 30HGS steel and titanium alloy Ti6Al4V. The metallographic, factographic tests were used, and measurements of microhardness with the Vickers method. In the head weld of the 30HGS steel there were non-metallic partial division and bubbles observed. The average microhardness in the head connection was 320 HV0.1. There was no significant increase/decrease observed of microhardness in the head influence zone of the weld. There was a good condition of head connections observed, in accordance with the standard EN12517 and EN25817. In the head weld of Ti6Al4V titanium alloy there were single, occasional non-metallic interjections and bubbles observed. There were no cracks both on the weld, and on the border of the heat influence zone. The value of microhardness in head connection was in the range 300-445 HV0.1. Reveal a very good condition of the head connections in accordance with the standard EN12517 and EN25817. The factographic tests prove the correctness of welded connections done and then heat treatment in case of steel and titanium alloy.
Źródło:
Archives of Foundry Engineering; 2012, 12, 2; 159-166
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermal Analysis of the ZnAl10 Alloy Modified by Ti Additions in AlTi5C0.15 and ZnTi3.2 Inoculants
Autorzy:
Piwowarski, G.
Buraś, J.
Krajewski, W. K.
Krajewski, P. K.
Powiązania:
https://bibliotekanauki.pl/articles/383098.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
alloy ZnAl
grain refinement
thermal analysis
inoculants
modified by Ti
stop ZnAl
ziarna
analiza termiczna
modyfikatory
Opis:
Cast alloys on the Zn matrix and of an increased Al content are characterised by good technological and mechanical properties, due to which they should meet special, more demanding requirements. However, the basic problem in these alloys technology, apart from a high tendency for gases pick-up and oxidation of liquid metals, is a tendency to form coarse-grained dendritic structures in castings solidifying in sand moulds, what - in turn - unfavourably influences their plastic properties [1, 2, 7, 11]. Therefore several treatments aimed at obtaining fine-grained structure and improving plastic properties are applied in these alloys technology. The presented study concerns the modification process of binary, middle-aluminium Zn alloys performed by additions of inoculants containing titanium and investigations of these modifications influence on the structure refinement degree. The Zn-10wt% Al (ZnAl10) alloy modified, before pouring into a sand mould, either by addition of the traditional inoculant i.e. Al-3wt% Ti-0.15wt% C (AlTi3C0.15 – TiCAl) or the new inoculant Zn-3.2wt% Ti (ZnTi3.2) was tested. Within investigations the thermal analysis was performed, especially cooling curves and their first derivatives, and also measurements by means of the differential scanning calorimetry (DSC), with a purpose of determining the modification influence on undercooling degree changes. Microstructures of the tested alloy were observed by the light microscopy (LM). The applied modification of middle-aluminium zinc alloys by AlTi3C0.15 and ZnTi3.2 inoculants causes a significant refinement of the alloy structure. Inoculants applied in investigations have a strong nucleating activity, which is confirmed by decreasing of undercooling and the temperature recalescence in cooling curves, which occurs simultaneously with grain refinements.
Źródło:
Archives of Foundry Engineering; 2014, 14, 4 spec.; 101-106
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-9 z 9

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies