Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Furan" wg kryterium: Temat


Tytuł:
Identification and Quantification of Gases Releasing from Furan no Bake Binder
Autorzy:
Acharya, S. G.
Vadher, J. A.
Kanjariya, P. V.
Powiązania:
https://bibliotekanauki.pl/articles/379863.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
furan
GC-MS
FTIR
binder
pyrolysis
furan no bake
spoiwo
piroliza
Opis:
Sand samples with furan binder were prepared using Sand, Furfuryl Alcohol and Toluene Sulfonic Acid with ratio 100:0.85:0.30. To identify and quantify gases releasing from furan binder various studies like FTIR, TGA and GC-MS were carried out. After analyzing our materials using above mentioned characterizations the chemical formula of the Resin and Binder and amount of gases releasing from composition were confirmed. After studying various reports on pyrolysis process of furan binder calculation of the % of various gases emitting during pyrolysis process of furan was carried out. Sample of gas collected from mold was analyzed using GC-MS. Based on GC-MS measurement various gases emitting from furan sand mold were identified and their amount were calculate and compared with the international standers of permissible gas emission limits in a foundry. The purpose of this paper is to assist foundries in pollution prevention by devising clean technologies which maintain or improve the quality of ambient surrounding. This paper aimed at minimization of pollution of air by using various techniques.
Źródło:
Archives of Foundry Engineering; 2016, 16, 3; 5-10
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Wpływ dodatku regeneratu na właściwości mas z żywicą furanową stosowanych na formy do odlewów ze staliwa manganowego
Influence of the reclaim on the properties of moulding sands with furfuryl resin applied for moulds for manganese steel castings
Autorzy:
Holtzer, M.
Bobrowski, A.
Drożyński, D.
Isendorf, B.
Mazur, M.
Powiązania:
https://bibliotekanauki.pl/articles/381676.pdf
Data publikacji:
2012
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
staliwo manganowe
masa furanowa
regeneracja mechaniczna
spoiwo furanowe
manganese cast steel
furan moulding sand
mechanical reclamation
furan binder
Opis:
W artykule omówiono wpływ dodatku regeneratu uzyskiwanego w procesie regeneracji mechanicznej do masy z żywicą furfurylową na osnowie piasku kwarcowego. Określono wpływ udziału regeneratu na takie parametry masy jak: wytrzymałość na rozciąganie, ścieralność, przepuszczalność i żywotność masy. Badania prowadzono przy udziale regeneratu w osnowie w ilości od 20 do 100%. Uzyskane wyniki wykazały, że optymalne właściwości, uzyskuje masa o składzie 60% regeneratu, 1 cz. mas. żywicy i 0,5 cz. mas. utwardzacza.
The influence of an addition of the reclaim, obtained in the mechanical reclamation process, to the moulding sand prepared on the basis of the high-silica sand with furfuryl resin, was discussed in the paper. The influence of the reclaim fraction on such moulding sand parameters as: tensile strength, wear resistance, permeability and bench life, was determined. Tests were performed at the reclaim fraction in the matrix being from 20 to 100%. The obtained results indicated that the optimal properties were exhibited by the moulding sand containing 60% of the reclaim, 40% new sand and 1 part by weigh of a resin and 0.5 part by weight of a hardener.
Źródło:
Archives of Foundry Engineering; 2012, 12, 1s; 57-62
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Role of Sand Grains in Sorption Processes by Surface Layers of Components of Sand Moulds
Autorzy:
Kaźnica, N.
Powiązania:
https://bibliotekanauki.pl/articles/383033.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
castings defects
moisture sorption
surface layer
furan moulding sands
sand grains
wady odlewnicze
wilgoć
warstwa powierzchniowa
masa formierska furanowa
furan
Opis:
The results of researches of sorption processes of surface layers of components of sand moulds covered by protective coatings are presented in the hereby paper. Investigations comprised various types of sand grains of moulding sands with furan resin: silica sand, reclaimed sand and calcined in temperature of 700 oC silica sand. Two kinds of alcoholic protective coatings were used – zirconium and zirconium – graphite. Tests were performed under condition of a constant temperature within the range 30 – 35oC and high relative air humidity 75 - 80%. To analyze the role of sand grains in sorption processes quantitavie moisture sorption with use of gravimetric method and ultrasonic method were used in measurements. The tendency to moisture sorption of surface layers of sand moulds according to the different kinds of sand grains was specified. The effectiveness of protective action of coatings from moisture sorption was analyzed as well. Knowledge of the role of sand grains from the viewpoint of capacity for moisture sorption is important due to the surface casting defects occurrence. In particular that are defects of a gaseous origin caused by too high moisture content of moulds, especially in surface layers.
Źródło:
Archives of Foundry Engineering; 2017, 17, 1; 87-92
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Synergy of practical knowledge of molding sands reclamation in heavy casting foundry of iron alloys
Autorzy:
Ignaszak, Z.
Prunier, J. B.
Powiązania:
https://bibliotekanauki.pl/articles/379704.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
furan molding sand
dry mechanical reclamation
iron alloy foundry
heavy casting
lifetime
furan sand
thermo mechanical database
masa formierska furanowa
sucha regeneracja mechaniczna
stop żelaza
odlew ciężki
trwałość
baza danych termomechaniczna
Opis:
The paper summarizes research realized by the author in laboratory and industrial conditions (foundries of cast steel and cast iron, castings up to 50 tons) on the effects of the chemically hardened molding sands regeneration using hard/soft rubbing in the dry reclamation. A reference was simultaneously made to advisability of application of the thermal regeneration in conditions, where chromite amount in the circulating (reclaimed) molding sand goes as high as above ten percent. An advisability of connecting standard and specialized methods of examination of the reclaimed sands and molding sands made using it was pointed out. A way of application of studies with the Hot Distortion Plus® method modified by the author for validation of modeling of the thermo-dynamic phenomena in the mold was shown.
Źródło:
Archives of Foundry Engineering; 2013, 13, 3; 30-36
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Effective Laboratory Method of Chromite Content Estimation in Reclaimed Sands
Autorzy:
Ignaszak, Z.
Prunier, J. B.
Powiązania:
https://bibliotekanauki.pl/articles/380085.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
chromite sand
magnetic recuperation
neodymium magnets
furan sand dry
reclamation
ferrous alloys
heavy castings
Opis:
The paper presents an original method of measuring the actual chromite content in the circulating moulding sand of foundry. This type of material is applied for production of moulds. This is the case of foundry which most frequently perform heavy casting in which for the construction of chemical hardening mould is used, both the quartz sand and chromite sand. After the dry reclamation of used moulding sand, both types of sands are mixed in various ratios resulting that in reclaimed sand silos, the layers of varying content of chromite in mixture are observed. For chromite recuperation from the circulating moulding sand there are applied the appropriate installations equipped with separate elements generating locally strong magnetic field. The knowledge of the current ratio of chromite and quartz sand allows to optimize the settings of installation and control of the separation efficiency. The arduous and time-consuming method of determining the content of chromite using bromoform liquid requires operational powers and precautions during using this toxic liquid. It was developed and tested the new, uncomplicated gravimetric laboratory method using powerful permanent magnets (neodymium). The method is used in the production conditions of casting for current inspection of chromite quantity in used sand in reclamation plant.
Źródło:
Archives of Foundry Engineering; 2016, 16, 3; 162-166
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Regeneracja zużytej masy z żywicą furfurylową na stanowisku laboratoryjnym
Reclamation of Used Furan Sand at Laboratory Stand
Autorzy:
Skrzyński, M.
Dańko, R.
Czapla, P.
Powiązania:
https://bibliotekanauki.pl/articles/380120.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
masy formierskie
żywica furfurylowa
regeneracja
regeneracja mechaniczna
molding sand
furan resin
regeneration
mechanical regeneration
Opis:
W publikacji przedstawiono wyniki badań regeneracji zużytej masy formierskiej z żywicą furfurylową, które zostały przeprowadzone na stanowisku doświadczalnym regeneratora wirnikowego RD-6. W badaniach określano wpływ sposobu prowadzenia procesu odzysku oraz zastosowanej metody odpylania regeneratu (odpylanie końcowe, odpylanie okresowe, odpylanie ciągłe) na jakość odzyskanego regeneratu. Jakość regeneratu określana była poprzez analizę straty prażenia, ilości pyłów powstających w procesie regeneracji oraz na podstawie określenia własności wytrzymałościowych masy formierskiej z regeneratem.
The paper presents the results of the regeneration of spent molding sand with furan resin, which were carried out at the experimental station rotary regenerator RD-6. In studies, the effects of the method of the reclamation process and the extraction of the dust (final dusting, periodic dusting, dusting continuous) on the quality of the recovered regenerate is determined. The quality of the reclaim was determined by analyzing the loss on ignition, the amount of dust generated in the process of regeneration, the sieve analysis and on the basis of determining the mechanical properties of the molding sands prepared with recovered material.
Źródło:
Archives of Foundry Engineering; 2014, 14, 4 spec.; 111-114
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Comparison of Molding Sand Technology Between Alphaset (APNB) and Furan (FNB)
Autorzy:
Ghosh, Dipak K.
Powiązania:
https://bibliotekanauki.pl/articles/381891.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Alphaset
Furan
foundries
molding sand
heat strength
residual strength
gases
environment
odlewanie
piasek formierski
wytrzymałość cieplna
Opis:
The paper focuses on investigation of properties of two most widely used self-set sand binder systems APNB and FNB across the Globe, for making molds and cores in foundries to produce castings of different sizes involving wide range of metals and alloys, ferrous and nonferrous. This includes study of compression strength values of samples made out of molding sand at different binder addition level using new, mechanically reclaimed (MR) and thermally reclaimed (TR) sand. Strength values studied include dry strength (at room temperature) at specified intervals simulating different stages of mold handling, namely stripping and pre heating, followed by degraded strength after application of thinner based zircon wash by brush, subsequent lighting of, then checking strength both in warm (degraded strength) & cold (recovered strength) conditions. Throughout the cycle of mold movement from stripping to knock out, strength requirements can be divided into two broad classifications, one from stripping to closing (dry strength) and another from pouring to knock out (hot & retained strength). Although the process for checking of dry strength are well documented, no method using simple equipments for checking hot & retained strength are documented in literature. Attempts have been made in this paper to use some simple methods to standardize process for checking high strength properties using ordinary laboratory equipments. Temperature of 450°C has been chosen by trial & error method to study high temperature properties to get consistent & amplified values. Volume of gases generated for both binders in laboratory at 850°C have also been measured. Nature of gases including harmful BTEX and PAH generated on pyrolysis of FNB and APNB bonded sands are already documented in a publication [1]. This exercise has once again been repeated in same laboratory, AGH University, Poland with latest binder formulations in use in two foundries in India.
Źródło:
Archives of Foundry Engineering; 2019, 4; 11-20
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Development of method for identification of compounds emitted during thermal degradation of binders used in foundry
Autorzy:
Kubecki, M.
Holtzer, M.
Grabowska, B.
Bobrowski, A.
Powiązania:
https://bibliotekanauki.pl/articles/382510.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
foundry binder
furan resin
gas chromatography
mass spectrometry
spoiwo odlewnicze
żywica furanowa
chromatografia gazowa
spektrometria masy
Opis:
The aim of the research was to develop a method for identification of compounds emitted during thermal degradation of binders used in foundry. Research were performed with the use of Certified Reference Materials mixtures of semi-volatiles compounds with furfuryl alcohol and aldehyde. Furfuryl-urea resin samples were also used. Station for thermal degradation of materials used in foundry was designed and made. Thermal degradation process conditions and gas chromatograph coupled with high resolution mass spectrometry operating conditions were established. Organic compounds emitted during degradation were identified. The paper briefly represents the range of study and the results obtained for furfuryl-urea resin thermal degradation. Significant information about volatile and semi-volatile organic compounds emitted in different temperatures is also discussed.
Źródło:
Archives of Foundry Engineering; 2011, 11, 3 spec.; 125-130
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Evaluation of Critical Parameters for Sand Inclusion Defect in FNB Casting
Autorzy:
Acharya, S. G.
Vadher, J. A.
Kothari, K. D.
Powiązania:
https://bibliotekanauki.pl/articles/381036.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
casting
evaluation of parameters
furan
grain fineness number
loss of ignition
pH
odlewnictwo
ocena parametrów
ziarno
Opis:
Casting covers major area of production all over the world. Resin bonded casting is widely used in today’s manufacturing industries. Furan No bake casting is most widely accepted in Indian foundries due to its excellent surface finish and dimensional stability. It is a self-setting binder and it has a lower work and strip times. Though the casting process is also known as process of uncertainty, in the present study, an attempt has been made to investigate the effect of Grain Fineness Number, Loss of Ignition, Potential of Hydrogen, % of Resin with respect to sand, Sand Temperature and Compressive strength of the mould on Sand Inclusion defect – one of the most dominating defect in the Krislur Castomech Pvt. Ltd. Industry situated at Bhavnagar, Gujarat, India. The experiments were conducted based on response surface methodology (RSM) and sequential approach using face centered central composite design. The results show that quadratic model with removal of some insignificant term is comparatively best fits for Sand Inclusion Defect.
Źródło:
Archives of Foundry Engineering; 2017, 17, 1; 5-12
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Identyfikacja związków termicznego rozkładu żywicy furanowej z zastosowaniem chromatografii gazowej w połączeniu ze spektrometrią masową (GC/MS)
Identification of Compounds from Thermal Decomposition of Furan Resin by Gas Chromatography Coupled with Mass Spectrometry (GC/MS)
Autorzy:
Żymankowska-Kumon, S.
Powiązania:
https://bibliotekanauki.pl/articles/379893.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
ochrona środowiska
żywica furanowa
chromatografia gazowa
spektrometria masowa
piroliza
environment protection
furan resin
gas chromatography
mass spectrometry
pyrolisis
Opis:
W celu wykonywania form i rdzeni dla odlewów ciężkich i lekkich stosowane są głównie żywice syntetyczne. Proces wiązania sypkiej masy samoutwardzalnej (SMS) z żywicą furfurylową (furanową) jest najczęściej stosowanym sposobem produkowania różnorodnych form i rdzeni dla praktycznie wszystkich stopów odlewniczych. Wszystkie nowoczesne żywice furanowe pozwalają na używanie dużej ilości regeneratu (praktycznie do 100%). Jako utwardzacze stosuje się kwasy organiczne i mieszaniny kwasów organicznych i nieorganicznych. Celem przeprowadzonych badań była identyfikacja związków pochodzących z rozkładu termicznego popularnej żywicy furanowej stosowanej w wielu krajowych odlewniach. Dodatkowo badaniom poddano katalizator, służący do utwardzenia żywicy. Do analizy zastosowano metodę chromatografii gazowej w połączeniu ze spektrometrią masową (GC/MS). Rozkład badanych próbek przeprowadzono w pirolizerze, w temperaturze 1300 °C, podłączonym do układu pomiarowego. Uzyskane wyniki pozwoliły na ocenę szkodliwości danej żywicy w stosunku do środowiska i otoczenia.
Synthetic resins are mainly used to produce moulds and cores for heavy and individual castings. These resins are recommended for the production of steel castings and are used in foundries. All modern furan resins allow the use of large quantities of reclaim (virtually 100%). As hardeners are used organic acids and mixtures of organic and inorganic acids. The aim of the study was to identify compounds from thermal decomposition of popular furan resin used in many foundries. In addition, the tests was a catalyst (hardener) used to cure the resin. Substances were identified by gas chromatography coupled with mass spectrometry (GC/MS) method, in the examined samples. The resin and hardener subjected to the high temperature (1300°C) in the pyrolyser. The results allowed the evaluation of harmfulness of resin with respect to the environment.
Źródło:
Archives of Foundry Engineering; 2015, 15, 4 spec.; 167-170
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of the Hardener on the Emission of Harmful Substances from Moulding Sands with Furan Resin in the Pyrolysis Process
Autorzy:
Holtzer, M.
Kmita, A.
Żymankowska-Kumon, S.
Bobrowski, A.
Dańko, R.
Powiązania:
https://bibliotekanauki.pl/articles/380824.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
furan resin
mould sand
emission of gases
pyrolisis
BTEX
PAH
żywica furanowa
masa formierska
emisja gazów
piroliza
Opis:
The furan resin offers advantages such as high intensity, low viscosity, good humidity resistance and is suitable for cast different casting alloys: steel, cast iron and non-ferrous metal casting. For hardening furan resins are used different hardeners (acid catalysts). The acid catalysts have significant effects on the properties of the cured binder (e,g. binding strength and thermal stability) [1 - 3]. Investigations of the gases emission in the test foundry plant were performed according to the original method developed in the Faculty of Foundry Engineering, AGH UST. The analysis is carried out by the gas chromatography method with the application of the flame-ionising detector (FID) (TRACE GC Ultra THERMO SCIENTIFIC).
Źródło:
Archives of Foundry Engineering; 2016, 16, 1; 107-111
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Evaluate Sulphur Diffusion at Mould-Metal Interface in No- Bake Mould System
Autorzy:
Sheladiya, M. V.
Acharya, S. G.
Mehta, K.
Acharya, G. D.
Powiązania:
https://bibliotekanauki.pl/articles/381595.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
foundry industries
no-bake technology
mould-metal interface
furan resin
sulphur diffusion
przemysł odlewniczy
technologia bez pieca
żywica furanowa
dyfuzja
Opis:
Casting process takes a major percentage of manufacturing products into consideration. No-bake casting is swiftly developing technology for foundry industries. In the no-bake family, furan no-bake casting process employs resins and acid catalyst to form a furan binder system. However, this process configures castings with augmented strength and quality surface finish. Compressive strength, transverse strength and tensile strength of moulds are also high in this furan binder system. Hence this method is apt for producing accurately dimensioned castings. Our well thought-out deliberations in the subsequent write up entail the numerous effects of variation of resin and acid catalyst on the surface defect i.e. sulfur diffusion on the surface of FNB casting. Furan resin; used in the production of casting is furfuryl alcohol and acid catalyst is sulphonic acid. Sulfur diffusion is tested by Energy-dispersive X-ray spectroscopy (EDX) analysis and also by the spectrometer with jet stream technology. This paper also comprises economic advantages of optimizing resin because furan resin is expensive and catalyst with reduction of sulfur diffusion defect as it saves machining, labor cost, and energy.
Źródło:
Archives of Foundry Engineering; 2019, 1; 63-70
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Structural Changes in the Furan Resins by UV Radiation and Atmospheric Air
Autorzy:
Bobrowski, A.
Powiązania:
https://bibliotekanauki.pl/articles/381893.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
furan resins
furfuryl alcohol
structural changes
spectroscopy FTIR
spectrum FTIR
żywice furanowe
alkohol furfurylowy
zmiany strukturalne
spektroskopia FTIR
widma FTIR
Opis:
In this paper, the results of research of structural changes that occur during in furan resins with different content of furfuryl alcohol by UV radiation and atmospheric air are presented. The research was carried out by transmission method (KBr pellets), using FTIR spectrometer Excalibur 3000 for the three samples of furan resins with different content of furfuryl alcohol. As a result of UV radiation and oxidizing atmosphere only the sample of the resin Kaltharz 8616 remained liquid. Two others (Kaltharz U 404 and Kaltharz 8117) were cured after 1
Źródło:
Archives of Foundry Engineering; 2015, 15, 1 spec.; 5-8
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Thermal Utilization of the Post Reclamation Dust from Molding Sand with Furan Resin in Test Unit
Autorzy:
Holtzer, M.
Dańko, R.
Dańko, J.
Powiązania:
https://bibliotekanauki.pl/articles/382999.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
thermal utilization
post reclamation dust
furan resin
environmental protection
foundry engineering
utylizacja termiczna
pył poregeneracyjny
żywica furanowa
ochrona środowiska
Opis:
Mechanical reclamation process of spent moulding sands generate large amounts dusts containing mainly rubbed spent binding agents and quartz dust. The amounts of post-reclamation dusts, depending of the reclamation system efficiency and reclaim dedusting system, can reach 5-10% in relation to the total reclaimed moulding sand. This dust due to the high content of the organic substances is a threat to the environment and therefore requires the storage on landfills specially adapted for this type of waste. On the other hand, the presence of organic substances causes that these dusts have relatively high energy values that could be used. However, at present there is no coherent, environmentally friendly concept for the management of this type of dust. The paper presents the results of tests of thermal utilization the dusts (as a source of energy) were carried out at AGH University of Science and Technology. Thermal utilization of dusts was carried out in the co-burning with carbon carriers process or in individual burning (Patent PL 227878 B1 and patent application PL - 411 902).
Źródło:
Archives of Foundry Engineering; 2018, 18, 4; 15-18
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Influence of Selected Water and Alcohol Based Coatings on Bending Strength of Foundry Moulds and Cores Manufactured in Furan Technology
Autorzy:
Romelczyk, R.
Przyszlak, N.
Siodmok, B.
Dorula, J.
Studnicki, A.
Powiązania:
https://bibliotekanauki.pl/articles/382706.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
water based coating
alcohol based coating
bending strength
moulding sand
furan resin
powłoka wodna
wytrzymałość na zginanie
masa formierska
żywica furanowa
Opis:
The subject of this paper was to compare the influence of selected coatings on bending strength of moulds and cores manufactured in a furan technology. In a range of study, there were used three kinds of coatings - water based coating and two kind of alcohol based coating manufactured by FOSECO. Coating were applicated by brush, overpouring/flow and spraying. For each application method, there were realized different kind of drying- at ambient temperature, in a furnace and by burning. Physicochemical properties of coatings were such selected to accommodate them to the application method and type of coating. Based on the conducted studies it was observed that for water based coating application method doesn’t have an important influence on bending strength and it is necessary to optimize the time and temperature of drying to achieve better results of bending strength. For alcohol based coatings, drying by burning causes significant deterioration of bending strength of the mould and core and drying process at ambient allows to obtain high bending strength of mould/cores in regard to time of drying.
Źródło:
Archives of Foundry Engineering; 2018, 18, 2; 169-172
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies