Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Al/Al" wg kryterium: Temat


Tytuł:
Effect of Titanium and Boron on the Stability of Grain Refinement of Al-Cu Alloy
Autorzy:
Górny, M.
Sikora, G.
Kawalec, M.
Powiązania:
https://bibliotekanauki.pl/articles/381182.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
quality management
Al-Cu alloy
fading effect
primary grains of α(Al)
zarządzanie jakością
metalografia
stop Al-Cu
zanik
ziarna pierwotne
Opis:
The present research was conducted on thin-walled castings with 5 mm wall thicknesses. This study addresses the effect of the influence of different master alloys, namely: (1) Al-5%Ti-1%B, (2) Al-5%Ti and (3) Al-3%B, respectively on the structure and the degree of undercooling (ΔTα = Tα-Tmin, where Tα - the equilibrium solidification temperature, Tmin - the minimum temperature at the beginning of α(Al) solidification) of an Al-Cu alloy. The process of fading has been investigated at different times spent on the refinement treatment ie. from 3, 20, 45 and 90 minutes respectively, from the dissolution of master alloys. A thermal analysis was performed (using a type-S thermocouple) to determine cooling curves. The degree of undercooling and recalescence were determined from cooling and solidification curves, whereas macrostructure characteristics were conducted based on a metallographic examination. The fading effect of the refinement of the primary structure is accompanied by a significant change in the number (dimension) of primary grains, which is strongly correlated to solidification parameters, determined by thermal analysis. In addition to that, the analysis of grain refinement stability has been shown with relation to different grain refinements and initial titanium concentration in Al-Cu base alloy. Finally, it has been shown that the refinement process of the primary structure is unstable and requires strict metallurgical control.
Źródło:
Archives of Foundry Engineering; 2016, 16, 3; 35-38
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Combustion Engine Cylinder Liners Made of Al-Si Alloys
Autorzy:
Orłowicz, A. W.
Tupaj, M.
Mróz, M.
Trytek, A.
Powiązania:
https://bibliotekanauki.pl/articles/382953.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
combustion engine
cylinder liner
Al-Si alloy
silnik spalinowy
tuleja cylindrowa
stop Al-Si
Opis:
The paper deals with problems related to application of aluminum-silicon alloys for combustion engine cylinder liners.
Źródło:
Archives of Foundry Engineering; 2015, 15, 2; 71-74
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Improvement of Al-Si Alloy Fatigue Strength by Means of Refining and Modification
Autorzy:
Tupaj, M.
Orłowicz, A. W.
Trytek, A.
Mróz, M.
Powiązania:
https://bibliotekanauki.pl/articles/379844.pdf
Data publikacji:
2019
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Al-Si alloy
fatigue limit
refining
modification
stop Al-Si
granica zmęczenia
rafinacja
modyfikacja
Opis:
The paper presents results of a study concerning an AlSi7Mg alloy and the effect of subjecting the liquid metal to four different processes: conventional refining with hexachloroethane; the same refining followed by modification with titanium, boron, and sodium; refining by purging with argon carried out in parallel with modification with titanium and boron salts and strontium; and parallel refining with argon and modification with titanium, boron, and sodium salts. The effect of these four processes on compactness of the material, parameters of microstructure, and fatigue strength of AlSi7Mg alloy after heat treatment. It has been found that the highest compactness (the lowest porosity ratio value) and the most favorable values of the examined parameters of microstructure were demonstrated by the alloy obtained with the use of the process including parallel purging with argon and modification with salts of titanium, boron, and sodium. It has been found that in the fatigue cracking process observed in all the four variants of the liquid metal treatment, the crucial role in initiation of fatigue cracks was played by porosity. Application of the process consisting in refining by purging with argon parallel to modification with Ti, B, and Na salts allowed to refine the microstructure and reduce significantly porosity of the alloy extending thus the time of initiation and propagation of fatigue cracks. The ultimate effect consisted in a distinct increase of the fatigue limit value.
Źródło:
Archives of Foundry Engineering; 2019, 4; 61-66
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Structure and mechanical properties of Al-Li alloys as cast
Autorzy:
Augustyn-Pieniążek, J.
Adrian, H.
Rzadkosz, S.
Choroszyński, M.
Powiązania:
https://bibliotekanauki.pl/articles/383253.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Al-Li alloy
aerospace industry
precipitation hardening
stop Al-Li
przemysł lotniczy
utwardzanie wydzieleniowe
Opis:
The high mechanical properties of the Al-Li-X alloys contribute to their increasingly broad application in aeronautics, as an alternative for the aluminium alloys, which have been used so far. The aluminium-lithium alloys have a lower specific gravity, a higher nucleation and crack spread resistance, a higher Young’s module and they characterize in a high crack resistance at lower temperatures. The aim of the research planned in this work was to design an aluminium alloy with a content of lithium and other alloy elements. The research included the creation of a laboratorial melt, the microstructure analysis with the use of light microscopy, the application of X-ray methods to identify the phases existing in the alloy, and the microhardness test.
Źródło:
Archives of Foundry Engineering; 2013, 13, 2; 5-10
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Badania stopów Al-Zr odlewanych w sposób ciągły
Studies of Al-Zr Alloys Produced by Continuous Casting
Autorzy:
Knych, T.
Uliasz, P.
Piwowarska-Uliasz, M.
Powiązania:
https://bibliotekanauki.pl/articles/381180.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
stop Al-Zr
odporność cieplna
odlewanie ciągłe
Al-Zr alloy
thermal resistance
continuous casting
Opis:
Praca zawiera badania własności mechanicznych, elektrycznych oraz odporności cieplnej badanych materiałów. Zakres pracy obejmuje badania nad procesem ciągnienia wlewków na druty o średnicy 3,5 mm, uzyskanych ze stopów Al-Zr w zakresie zawartości cyrkonu od 0,05 do 0,32, które zostały wytworzone w warunkach przemysłowych w linii ciągłego odlewania i walcowania (COiW). W artykule przedstawiono technologiczne krzywe umocnienia poszczególnych materiałów oraz wyniki badań obejmujące charakteryzację wybranych własności stopów Al-Zr.
The work includes the study of mechanical, electrical properties and thermal resistance of the tested materials. The scope of work includes research on the process of wire bar on the wires with a diameter of 3.5 mm, obtained from Al-Zr alloys of zirconium content of 0.05 to 0.32, which have been produced in industrial conditions in the continuous casting and rolling (CCR). The paper presents the technological curve and the strengthening of individual materials research, including characterization of selected properties of Al-Zr alloys.
Źródło:
Archives of Foundry Engineering; 2013, 13, 3 spec.; 63-68
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Hypoeutectic Al-Si Alloy with Cr, V and Mo to Pressure Die Casting
Autorzy:
Szymczak, T.
Gumienny, G.
Stasiak, I.
Pacyniak, T.
Powiązania:
https://bibliotekanauki.pl/articles/382365.pdf
Data publikacji:
2017
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
krystalizacja
odlewanie ciśnieniowe
stopy wieloskładnikowe
stopy Al-Si
metoda DTA
crystallization
pressure die casting
multicomponent Al-Si alloys
alloys Al-Si
DTA method
Opis:
This paper presents the results of hypoeutectic 226 grade alloy as well as prepared on its basis Al-Si alloy containing Cr, V and Mo. The additives tested were added as AlCr15, AlV10 and AlMo8 master alloys. Alloys tested were poured into DTA sampler as well as using pressure die casting. An amount of Cr, V and Mo additives in alloy poured into DTA sampler comprised within the range approximately 0.05-0.35%. Alloys to pressure die casting contained 0.05-0.20% Cr, V and Mo. The crystallization process was examined using the derivative thermal analysis (DTA). The microstructure of castings made in the DTA sampler as well as castings made with use of pressure die casting were examined. The basic mechanical properties of castings made using pressure die casting were defined too. It has been shown in the DTA curves of Al-Si alloy containing approximately 0.30 and 0.35% Cr, Mo, and V there is an additional thermal effect probably caused by a peritectic crystallization of intermetallic phases containing the aforementioned additives. These phases have a morphology similar to the walled and a relatively large size. The analogous phases also occur in pressure die casting alloys containing 0.10% or more additions of Cr, V and Mo. The appearance of these phases in pressure die casting Al-Si alloys coincides with a decrease in the value of the tensile strength Rm and the elongation A. It has been shown die castings made of Al-Si alloys containing the aforementioned additives have a higher Rm and A than 226 alloy.
Źródło:
Archives of Foundry Engineering; 2017, 17, 1; 153-156
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
The Role of Microstructure on the Corrosion Behaviour of as cast AlCu4MgSi and MgAl2Si Alloys
Autorzy:
Lachowicz, M. M.
Jasionowski, R.
Powiązania:
https://bibliotekanauki.pl/articles/381379.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
metallography
corrosion resistance
aluminum alloy
magnesium alloy
Al-Cu-Mg-Si alloy
Mg-Al-Si alloy
metalografia
odporność korozyjna
stop aluminium
stop magnezu
stop Al-Cu-Mg-Si
stop Mg-Al-Si
Opis:
In this work, the effect of the microstructure on corrosion behavior of selected Mg- and Al-based as cast alloys, was evaluated. The electrochemical examinations were carried out, and then a morphology of corrosion products formed due to local polarization on materials surface, was analyzed. It was documented that the presence of Mg2Si phase plays an important role in the corrosion course of Mg-based alloy. A selective etching was observed in sites of Mg2Si precipitates having “Chinese script”- like morphology. Analogous situation was found for Al-based alloy, where the key role was played by cathodic θ-CuAl2 phase.
Źródło:
Archives of Foundry Engineering; 2018, 18, 2; 125-130
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Optimization of squeeze parameters and modification of AlSi7Mg alloy
Autorzy:
Zyska, A.
Konopka, Z.
Łągiewka, M.
Nadolski, M.
Powiązania:
https://bibliotekanauki.pl/articles/381007.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
mechanical properties
Al alloy
squeeze casting technology
modification
właściwości mechaniczne
stop Al
technologia prasowania
modyfikacja
Opis:
The paper present the examination results concerning mechanical properties of castings made of AlSi7MG alloy in correlation both with the most significant squeeze casting parameters and with the modification treatment. Experiments were planned and held according to the 23 factorial design. The regression equations describing the influence of the squeeze pressure, the mould temperature, and the quantity of strontium modifier on the strength and elongation of the examined alloy were obtained. It was found that the main factor controlling the strength increase is the squeeze pressure, while the plasticity (A5) of the alloy is affected most advantageously by modification. The application of modification treatment in squeeze casting technology enables for production of the slab-type castings made of AlSi7Mg alloy exhibiting strength at the level of 230 MPa and elongation exceeding 14%.
Źródło:
Archives of Foundry Engineering; 2013, 13, 2; 113-116
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Mg-Al-RE Magnesium Alloys for High-Pressure Die-Casting
Autorzy:
Braszczyńska-Malik, K.
Powiązania:
https://bibliotekanauki.pl/articles/383025.pdf
Data publikacji:
2014
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
magnesium alloys Mg-Al-RE
high-pressure die casting
stopy magnezu Mg-Al-RE
odlewanie wysokociśnieniowe
Opis:
Experimental Mg-Al-RE type magnesium alloys for high-pressure die-casting are presented. Alloys based on the commercial AM50 magnesium alloy with 1, 3 and 5 mass % of rare earth elements were fabricated in a foundry and cast in cold chamber die-casting machines. The obtained experimental casts have good quality surfaces and microstructure consisting of an α(Mg)-phase, Al11RE3, Al10RE2Mn7 intermetallic compound and small amount of α+γ eutectic and Al2RE phases.
Źródło:
Archives of Foundry Engineering; 2014, 14, 2; 49-52
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of Cooling Rate on Intergranular Corrosion in Al-Si7-Mg Alloy
Autorzy:
Bernat, L.
Powiązania:
https://bibliotekanauki.pl/articles/381720.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Al-Si-Mg alloy
intergranular corrosion
cooling rate
stop Al-Si-Mg
korozja międzykrystaliczna
szybkość chłodzenia
Opis:
The use of aluminium cast alloys in automotive industry results from a tendency to considerably lower vehicle mass. Subject to working conditions, silumin casts may show occurrence of intergranular corrosion that reduces mechanical properties of the parts produced. The paper presents the influence of cooling rate – R of a plate cast of aluminium alloy EN AC-AlSi7Mg0,3 on the depth of appearance of intergranular corrosion. Samples were exposed to corrosive medium by immersion for 2,5; 12; 24 and 48 hours in an aqueous solution of NaCl+HCl+H2O. The study demonstrated that cooling rate – R and subsurface porosity significantly influence on distribution and depth of intergranular corrosion in casts of subeutectic silumin.
Źródło:
Archives of Foundry Engineering; 2015, 15, 3 spec.; 107-111
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Plasma Coatings on Aluminium-Silicon Alloy Surfaces
Autorzy:
Długosz, P.
Garbacz-Klempka, A.
Piwońska, J.
Darłak, P.
Młynarczyk, M.
Powiązania:
https://bibliotekanauki.pl/articles/2079836.pdf
Data publikacji:
2021
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
plasma coating
Al-Si alloy
plasma oxidation
anodizing
powłoki plazmowe
stop Al-Si
utlenianie plazmowe
anodowanie
Opis:
Plasma oxidation, similarly to anodic oxidation (anodizing), are classified as electrochemical surface treatment of metals such as Al, Mg, Ti and their alloys. This type of treatment is used to make surface of castings, plastically processed products, shaped with incremental methods to suitable for certain requirements. The most important role of the micro plasma coating is to protect the metal surface against corrosion. It is well known that coating of aluminium alloys containing silicon using anodic oxidation causes significant difficulties. They are linked to the eutectic nature of this alloy and result in a lack of coverage in silicon-related areas. The coating structure in these areas is discontinuous. In order to eliminate this phenomenon, it is required to apply oxidation coatings using the PEO (Plasma Electrolytic Oxidation) method. It allows a consistent, crystalline coating to be formed. This study presents the mechanical properties of the coatings applied to Al-Si alloy using the PEO method. As part of the testing, the coating thickness, microhardness and scratch resistance were determined. On the basis of the results obtained, it was concluded that the thickness of the coatings complies with the requirements of conventional anodizing. Additionally, microhardness values exceeded the results obtained with standard methods.
Źródło:
Archives of Foundry Engineering; 2021, 21, 3; 96-101
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Influence of annealing time and temperature on the Fe3Al intermetallic alloys microstructure modification
Autorzy:
Garbala, K.
Patejuk, A.
Powiązania:
https://bibliotekanauki.pl/articles/380040.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
intermetallic alloy
Fe3Al phase
microstructure modification
stop międzymetaliczny
faza Fe3Al
modyfikacja mikrostruktury
Opis:
There is an industry interesting in intermetallic alloys in recent years. There are widely possibilities to adopt this kind of materials for structural units. More expensive materials can be replaced by them. A property which limits their wider application is the low plasticity at environment and elevated temperatures. In paper the results of the thermal microstructure modification are shown. To this end, the influence of annealing time and temperature on the intermetallic phase Fe3Al grain size was investigated. The impact of these factors on micro-hardness was examined as well. It was found that these operations cause the grain size reduction and the micro-hardness decrease.
Źródło:
Archives of Foundry Engineering; 2011, 11, 2 spec.; 39-42
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Fluidity Characteristics of A201 and A206 Al-Cu Alloy
Autorzy:
Yildirim, K.
Helvaci, M.
Gürsoy, Ö.
Erzi, E.
Kahruman, C.
Dispinar, D.
Powiązania:
https://bibliotekanauki.pl/articles/380959.pdf
Data publikacji:
2018
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
Al-Cu alloy
casting
fluidity of alloy
mould coating
stop Al-Cu
odlew
lejność stopu
forma odlewnicza
Opis:
Al-4.5Cu alloys are widely used in aerospace industries due to their low weight and high mechanical properties. This group of aluminium alloys is known as 2xx series and exhibits the highest mechanical properties however this alloy is known to suffer from feedability and high tendency for hot tearing. Al-Si alloys (3xx) have improved fluidity and better feedability particularly by several modifications such as Ti, B or Sr. Eutectic temperature is decreased and mechanical properties can be enhanced. Yet, the strength values of this alloy group cannot reach the values of 2xx series. Therefore, in this study, the effect of Ag addition on the fluidity of Al-4.5Cu alloy has been investigated. Standard size spiral mould was used. The casting temperature was selected to be 770oC. Five castings were made and Weibull statistical approach was used to evaluate the results. In addition, coating of the die with BN was also investigated. It was found that Ag addition and BN coating of the die revealed the most reproducible, reliable and high fluidity values.
Źródło:
Archives of Foundry Engineering; 2018, 18, 1; 135-138
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Fatigue Resistance of A390.0 Alloy Modified with Phosphorus
Autorzy:
Wieszała, R.
Piątkowski, J.
Powiązania:
https://bibliotekanauki.pl/articles/381178.pdf
Data publikacji:
2015
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
fatigue wear
unilateral pulsating vibration
hypereutectic Al-Si alloy
zużycie zmęczeniowe
drganie pulsacyjne
stop nadeutektyczny Al-Si
Opis:
The paper presents fatigue tests (unilateral pulsating vibrations) for hypereutectic silumin AlSi17Cu5Mg aimed at simulation of deflection of the piston head in a combustion engine. The methodology of the tests and the way of marking the deflection of the tested material is described together with the detailed description of the test stand. The fatigue resistance ZG was identified in the tested material and a Wöhler diagram was prepared to show the areas of limited and unlimited fatigue resistance.
Źródło:
Archives of Foundry Engineering; 2015, 15, 3 spec.; 99-102
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Assessment of AlSi21CuNi alloy’s quality with use of ATND method
Autorzy:
Pezda, J.
Powiązania:
https://bibliotekanauki.pl/articles/380515.pdf
Data publikacji:
2013
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
hypereutectic Al-Si alloy
modification
ATND
mechanical properties
stop nadeutektyczny Al-Si
modyfikacja
metoda ATND
właściwości mechaniczne
Opis:
Majority of combustion engines is produced (poured) from Al-Si alloys with low thermal expansion coefficient, so called piston silumins. Hypereutectic alloys normally contain coarse, primary angular Si particles together with eutectic Si phase. The structure and mechanical properties of these alloys are highly dependent upon cooling rate, composition, modification and heat-treatment operations. In the paper one depicts use of the ATND method (thermal-voltage-derivative analysis) and regression analysis to assessment of quality of the AlSi21CuNi alloy modified with Cu-P on stage of its preparation, in aspect of obtained mechanical properties (R0,02, Rm, A5, HB). Obtained dependencies enable prediction of mechanical properties of the investigated alloy in laboratory conditions, using values of characteristic points from curves of the ATND method.
Źródło:
Archives of Foundry Engineering; 2013, 13, 4; 87-92
1897-3310
2299-2944
Pojawia się w:
Archives of Foundry Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł

Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies