Tytuł:
Combined Effect of CrB2 Micropowder and VN Nanopowder on the Strength and Wear Re-sistance of Fe‒Cu–Ni–Sn Matrix Diamond Composites
Autorzy:
Ratov, Boranbay
Mechnik, Volodymyr
Rucki, Miroslaw
Gevorkyan, Edwin
Kilikevicius, Arturas
Kolodnitskyi, Vasyl
Siemiatkowski, Zbigniew
Umirova, Gulzada
Chałko, Leszek
Józwik, Jerzy
Zhanggirkhanova, Arailym
Chishkala, Vladimir
Korostyshevskyi, Dmytro
Powiązania:
https://bibliotekanauki.pl/articles/2201897.pdf
Data publikacji:
2023
Wydawca:
Stowarzyszenie Inżynierów i Techników Mechaników Polskich
Tematy:
diamond composite
electroconsolidation
composite microstructure
adhesion
CrB2
VN nanopowder
micropowder
VN
wear resistance
cutting tools
mining tools
Opis:
The paper presents research results on the enhancement of diamond composites designed for tools application for mining industry, hard rocks cutting, able to withstand harsh conditions under heavy dynamical loads. In the present study, both CrB2 micropowder and VN nanopowder additives were used in proportions up to 5 wt.% and 6 wt.%, respectively, together with the basic matrix composition of 51 wt.% Fe, 32 wt.% Cu, 9 wt.% Ni, and 8 wt.% Sn. Addition of both components, CrB2 and VN, appeared to be ad-vantageous in proportion of 2 wt.% and 4 wt.%, respectively. This composition exhibited the highest relative density of 0.9968, better than that without additives. Similarly, the highest values of compressive strength Rcm and flexural strength Rbm were reached for the composite with the same percentage of CrB2 and VN. Compared to the composite with no addition of CrB2 and VN, Rcm improved by almost 70%, while Rbm by 81%. Additionally, the abovementioned additives enhanced the ability of the matrix to prevent the diamond reinforcement from being torn out of the composite, which is very important under harsh working conditions of the cutting tools. The presence of CrB2 micropowder and VN nanopowder promoted densification of the matrix and adhesion between the diamond grits and the Fe‒Cu–Ni–Sn matrix.
Źródło:
Advances in Science and Technology. Research Journal; 2023, 17, 1; 23--34
2299-8624
Pojawia się w:
Advances in Science and Technology. Research Journal
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies