Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Toktar, Gulmira" wg kryterium: Autor


Wyświetlanie 1-1 z 1
Tytuł:
Increase in the Free Finely-Dispersed Gold Recovery in the Flotation Cycle
Autorzy:
Toktar, Gulmira
Bakrayeva, Akbota
Abdyldayev, Nurgali
Banks, Graig E.
Kubaizhanov, Alibek
Powiązania:
https://bibliotekanauki.pl/articles/2202319.pdf
Data publikacji:
2023
Wydawca:
Polskie Towarzystwo Inżynierii Ekologicznej
Tematy:
hydrometallurgy
ore
recovery
free finely dispersed gold
flotation
sulfidiser
pulp dispersion
Opis:
This article presents the results of a comparative study for the increase in the free finely dispersed gold recovery from the gold-bearing ore produced in a deposit in Kazakhstan. The following minerals were identified in the sample under X-ray phase analysis: chalcopyrite and pyrite, as well as in a finely disseminated state in silicate minerals. Gold in the ore is present mainly (40.09%) in the free form under the results of phase analysis. Flotation tests of ore beneficiation were performed in FML-1 and FML-3 flotation machines with chamber volumes of 1.0 and 3.0 liters. A flotation combined concentrate with a gold content of 15.3 g/t was obtained (concentrate yield 9.45%), with gold recovery into concentrate 82.79% in the optimal mode: the grind of 90% in the class -0.071 mm; consumption of reagents: C7 foaming agent – 30 and 60 g/t, sodium butyl xanthate – 60 and 120 g/t; the time of the main flotation – 10 minutes, the control flotation – 7 minutes, at pH = 9. Flotation tailings contained 0.33 g/t of gold. The recovery showed a fairly high 84.42% (yield of the total concentrate 20.93%) with the gold content of 7.1 g/t with the use of a sulfidizing agent (Na2S) and additional dispersion of the pulp at pH = 9.0. A gold-bearing concentrate was obtained containing 4.0 g/t Au at a fineness of -0.05 mm and 6.8 g/t Au at a fineness of +0.05 mm. The beneficiation of the pulp with a fineness of +0.05 mm gave the recovery into the final concentrate equal to 89.94%.
Źródło:
Journal of Ecological Engineering; 2023, 24, 1; 115--119
2299-8993
Pojawia się w:
Journal of Ecological Engineering
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-1 z 1

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies