Informacja

Drogi użytkowniku, aplikacja do prawidłowego działania wymaga obsługi JavaScript. Proszę włącz obsługę JavaScript w Twojej przeglądarce.

Wyszukujesz frazę "Mosialek, A." wg kryterium: Autor


Wyświetlanie 1-5 z 5
Tytuł:
The first record and occurrence of the ornate cow tick Dermacentor reticulatus (Fabricius, 1794) in south-western Poland
Autorzy:
Cuber, P.
Solarz, K.
Mosialek, A.
Jakubiec-Spanier, M.
Spanier, A.
Powiązania:
https://bibliotekanauki.pl/articles/6404.pdf
Data publikacji:
2013
Wydawca:
Polskie Towarzystwo Parazytologiczne
Tematy:
first record
occurrence
ornate cow tick
Dermacentor reticulatus
tick
dog
animal infestation
new location
South-Western Poland
Źródło:
Annals of Parasitology; 2013, 59, 1
0043-5163
Pojawia się w:
Annals of Parasitology
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Ba0.5Sr0.5Co0.8Fe0.2O3-σ and La0.6Sr0.4Co0.8Fe0.2O3-σ composite cathode for solid oxide fuel cell
Autorzy:
Mosiałek, M.
Kędra, A.
Krzan, M.
Bielańska, E.
Tatko, M.
Powiązania:
https://bibliotekanauki.pl/articles/355878.pdf
Data publikacji:
2016
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
barium strontium cobalt ferrite
lanthanum strontium cobalt ferrite
solid oxide fuel cell
oxygen reduction reaction
electrochemical impedance spectroscopy
Opis:
Composite cathodes contain Ba0.5Sr0.5Co0.8Fe0.2O3-σ and La0.6Sr0.4Co0.8Fe0.2O3-σ were tested in different configuration for achieving cathode of area specific resistance lower than Ba0.5Sr0.5Co0.8Fe0.2O3-σ and La0.6Sr0.4Co0.8Fe0.2O3-σ cathodes. Electrodes were screen printed on samaria-doped ceria electrolyte half-discs and tested in the three electrode setup by the electrochemical impedance spectroscopy. Microstructure was observed by scanning electron microscopy. The lowest area specific resistance 0.46 and 2.77 Ω cm-2 at 700 °C and 600 °C respectively revealed composite cathode contain Ba0.5Sr0.5Co0.8Fe0.2O3-σ and La0.6Sr0.4Co0.8Fe0.2O3-σ in 1:1 weight ratio. The area specific resistance of this cathode is characterized by the lowest activation energy among tested cathodes.
Źródło:
Archives of Metallurgy and Materials; 2016, 61, 3; 1483-1488
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Ionic conductivity of the CeO2-Gd2O3-SrO system
Przewodnictwo jonowe w układzie CeO2-Gd2O3-SrO
Autorzy:
Dudek, M.
Mosiałek, M.
Mordarski, G.
Socha, R.
Rapacz-Kmita, A.
Powiązania:
https://bibliotekanauki.pl/articles/352955.pdf
Data publikacji:
2011
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
elektrolity stałe tlenku ceru
roztwór stały
stałotlenkowe ogniwo paliwowe
solid oxide electrolytes
ceria-based solid solutions
co-doping
solid oxide fuel cell
Opis:
The Pechini method was used to synthesize nanopowders of CeO2-based solid solutions with the formula Ce0.8-xGd0.2SrxO2- for 0
Jednofazowe proszki roztworów stałych Ce0:8-xGd0:2SrxO2- dla 0
Źródło:
Archives of Metallurgy and Materials; 2011, 56, 4; 1249-1255
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Dual Pore Cathode Materials for Solid Oxide Fuel Cells
Autorzy:
Mosiałek, M.
Zimowska, M.
Kharitonov, D.
Górski, M.
Krzan, M.
Komenda, A.
Powiązania:
https://bibliotekanauki.pl/articles/354965.pdf
Data publikacji:
2020
Wydawca:
Polska Akademia Nauk. Czytelnia Czasopism PAN
Tematy:
solid oxide fuel cell
yttrium iron cobaltite
lanthanum strontium cobalt ferrite
composite cathode
electrochemical impedance spectroscopy
Opis:
In this work, we developed the lanthanum strontium cobalt ferrite and it’s composite with yttrium iron cobaltite (mass ratio of 1:1) cathodes as a thin layer on Ce0.8Sm0.2O1.9 electrolyte. Two kinds of electrode pastes were prepared, with and without 6 mm polystyrene beads as an additional pore former. The performance of cathode materials was investigated by electrochemical impedance spectroscopy as a function of electrode morphology, oxygen partial pressure, potential, and temperature. The polarization resistance of the more porous electrodes was lower than those electrodes prepared without additional pore former in the whole potential range at 800°C, slightly lower at 700°C and 600°C. The addition of yttrium iron cobaltite decreased the performance of both types of cathodes. The lower polarization resistance of porous cathodes is due to the facilitated gas diffusion through their structure.
Źródło:
Archives of Metallurgy and Materials; 2020, 65, 3; 1217-1221
1733-3490
Pojawia się w:
Archives of Metallurgy and Materials
Dostawca treści:
Biblioteka Nauki
Artykuł
Tytuł:
Degradation of nanoclay-filled polylactide composites
Autorzy:
Rapacz-Kmita, A.
Stodolak-Zych, E.
Dudek, M.
Szaraniec, B.
Rozycka, A.
Mosialek, M.
Mandecka-Kamien, L.
Powiązania:
https://bibliotekanauki.pl/articles/110832.pdf
Data publikacji:
2013
Wydawca:
Politechnika Wrocławska. Oficyna Wydawnicza Politechniki Wrocławskiej
Tematy:
nanocomposite materials
food packaging
polymer
smectite clay
Opis:
Nanoclay-filled polylactide (PLA 3051D) composite materials were tested in this study and their capacity for degradation was investigated. Activated and lyophilized smectite clay was used. The filler, its morphology, and grain size distribution were characterized by the use of transmission electron microscopy, scanning electron microscopy, and the dynamic light scattering technique. Samples of pure polylactide and polylactide filled with 3% wt., 5% wt., and 10% wt. of nanoclay in subsequent series were obtained by injection molding. The optimum amount of the filler in the nanocomposites was evalu-ated based on an assessment of mechanical properties as well as capacity to degrade. The 3% wt. mass fraction of nanofiller in the polylactide matrix was found to be the most effective in enhancement of both tensile strength (RM) and Young’s Modulus (E). It was also reported that polylactide nanocomposites filled with 3% wt. of smectite clay were characterized by the highest decrease in molecular mass of the matrix polymer after degradation tests (6 weeks incubation in water at 80°C). The observed decrease in degradation time and the overall changes distinguished in the nanocomposite structure suggest the poten-tial for application of the material in the packaging industry.
Źródło:
Physicochemical Problems of Mineral Processing; 2013, 49, 1; 91-99
1643-1049
2084-4735
Pojawia się w:
Physicochemical Problems of Mineral Processing
Dostawca treści:
Biblioteka Nauki
Artykuł
    Wyświetlanie 1-5 z 5

    Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies