To improve mechanical properties and increasing useful life of metal pieces, different methods of welding are used for repairing surface crack of metal pieces. In this research, performance of flame welding method by spraying pure iron powder evaluated for repairing surface grooves of structural steel. First, four specimens including one control specimen and other three specimens grooved specimens in depth of 1mm and in length of 12.5mm and groove width in the sizes of 0.5, 0.75 and 1mm.were prepared then, powder melted using oxyacetylene reducing flame and spraying iron powder in the flame path and attached to the inner surface of the groove and finally, the specimen repaired. Results showed that after repairing surface groove, tensile strength of the repaired specimens were reached to the tensile strength of control specimen with the margin of 2.5%.
Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies
Informacja
SZANOWNI CZYTELNICY!
UPRZEJMIE INFORMUJEMY, ŻE BIBLIOTEKA FUNKCJONUJE W NASTĘPUJĄCYCH GODZINACH:
Wypożyczalnia i Czytelnia Główna: poniedziałek – piątek od 9.00 do 19.00