Results of the investigation of thermal degradation of polyolefins in the laboratory-scale set-up reactors are presented in the paper. Melting and cracking processes were carried out in two different types of reactors at the temperature of 390-420[degrees]C. This article presents the results obtained for conversion of polyolefin waste in a reactor with a stirrer. Next, they were compared with the results obtained for the process carried out in a reactor with a molten metal bed, which was described in a previous publication. For both processes, the final product consisted of a gaseous (2-16 % mass) and a liquid (84-98 % mass) part. No solid product was produced. The light, "gasoline" fraction of the liquid hydrocarbons mixture (C4-C10) made up over 50% of the liquid product. The overall (vapor) product may be used for electricity generation and the liquid product for fuel production.
Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies
Informacja
SZANOWNI CZYTELNICY!
UPRZEJMIE INFORMUJEMY, ŻE BIBLIOTEKA FUNKCJONUJE W NASTĘPUJĄCYCH GODZINACH:
Wypożyczalnia i Czytelnia Główna: poniedziałek – piątek od 9.00 do 19.00