The electrical conductivity σ (T) and thermoelectric power S(T) measurements of Sr₂InV₃O₁₁ showed the insulating state and the change of sign of thermopower from p to n at $T_{n-p}$=400 K. The I-V characteristics provided the evidence of symmetrical and non-linear behaviour typical of strong emission of charge carriers induced by temperature and voltage. Relative dielectric permittivity $ε_{r}$ as well as loss tangent (tan δ) strongly depend both on the temperature in the range of 295-400 K and the frequency in the range of 5×10² to 1×10⁶ Hz, showing the broad maximum at 320 K. These effects are considered as a relaxation process like in the Maxwell-Wagner or Jonscher model as well as the conduction of electric current, as determined by the Joule-Lenz law.
Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies
Informacja
SZANOWNI CZYTELNICY!
UPRZEJMIE INFORMUJEMY, ŻE BIBLIOTEKA FUNKCJONUJE W NASTĘPUJĄCYCH GODZINACH:
Wypożyczalnia i Czytelnia Główna: poniedziałek – piątek od 9.00 do 19.00