Niskotarciowe powłoki na bazie MoS2 z podwarstwami chromu na odlewniczych stopach aluminium Production of low friction MoS2 (Ti,W) coatings with Cr interlayer deposited on silumin
I have attempted to meet request on lightweight functional materials with low friction coefficient and high wear resistance reported by various areas of industry. For this purpose I attempted to combine good tribological properties of MoS2 (Ti,W) coatings base and modified and refined silumin. In addition, under MoS2 (Ti,W) coating the Cr interlayer was deposited having the task to increase the adhesion of the coating to the substrate. In such a composite tribological tests were the major studies. Additionally, for the characterization of deposited coatings the following studies were conducted: qualitative analysis of the phase composition of X-ray diffraction (XRD), linear analysis of the distribution of selected elements (EDS), nano-hardness and Young modulus were measured.
Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies
Informacja
SZANOWNI CZYTELNICY!
UPRZEJMIE INFORMUJEMY, ŻE BIBLIOTEKA FUNKCJONUJE W NASTĘPUJĄCYCH GODZINACH:
Wypożyczalnia i Czytelnia Główna: poniedziałek – piątek od 9.00 do 19.00