In this study, lateritic nickel ore from Manisa-Çaldağ, Turkey was subjected to sulfation roasting. Experimental parameters were as follows, acid concentration (10-90 wt.%), roasting temperature (200-900°C) and time (15-90 min). Effect of sodium sulfate addition (1-9 wt.%) on dissolutions of nickel and cobalt was also investigated. It was concluded that iron dissolution has increased with increased acid concentration. Dissolutions of nickel and cobalt increased with increasing roasting temperature and time below the decomposition temperature of related metal sulfates. It was concluded that addition of sodium sulfate in roasting stage has no significant effect on dissolutions of related metals.
Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies
Informacja
SZANOWNI CZYTELNICY!
UPRZEJMIE INFORMUJEMY, ŻE BIBLIOTEKA FUNKCJONUJE W NASTĘPUJĄCYCH GODZINACH:
Wypożyczalnia i Czytelnia Główna: poniedziałek – piątek od 9.00 do 19.00