The material selected for this investigation was low alloy weld metal deposit after TIG welding with various amount of oxygen
in weld metal deposit (WMD). After TIG process it is difficult to get proper amount of oxygen in WMD on the level much lower
than 350 ppm. The highest impact toughness of low alloy WMD corresponds with the amount of oxygen in WMD above 350 ppm.
In the paper focuses on low alloy steel after innovate welding method with micro-jet cooling that could be treated as a chance on
rising amount of oxygen in weld. Weld metal deposit (WMD) was carried out for TIG welding with micro-jet cooling with various
amount of oxygen in WMD. In that paper various gas mixtures (gas mixtures Ar-O2 and Ar-CO2) were tested for micro-jet cooling
after TIG welding. An important role in the interpretation of the results can give methods of artificial intelligence.
Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies
Informacja
SZANOWNI CZYTELNICY!
UPRZEJMIE INFORMUJEMY, ŻE BIBLIOTEKA FUNKCJONUJE W NASTĘPUJĄCYCH GODZINACH:
Wypożyczalnia i Czytelnia Główna: poniedziałek – piątek od 9.00 do 19.00