A conventional powder metallurgy method (PM) was used to produce Al-SiC and Al4Cu alloy matrix composites with 2.5,
5, 7.5 and 10 wt% of SiC particles. Two different sizes of the reinforcing phase particles were applied to determine their effect on
composite microstructure. The sintering process was carried out at 600°C under nitrogen atmosphere, and its consequence was the
appearance of aluminium nitrides in composite microstructure acting as an additional strengthening phase. The composites were
next re-pressed and re-sintered (2p2s) under the same conditions. The main aim of this article was to examine the microstructure
of the SiC reinforced Al and Al4Cu alloy matrix composites. To achieve this goal and characterize the sintered materials, scanning
electron microscopy (SEM), transmission electron microscopy (TEM) and X-ray diffraction (XRD) techniques were used.
Ta witryna wykorzystuje pliki cookies do przechowywania informacji na Twoim komputerze. Pliki cookies stosujemy w celu świadczenia usług na najwyższym poziomie, w tym w sposób dostosowany do indywidualnych potrzeb. Korzystanie z witryny bez zmiany ustawień dotyczących cookies oznacza, że będą one zamieszczane w Twoim komputerze. W każdym momencie możesz dokonać zmiany ustawień dotyczących cookies
Informacja
SZANOWNI CZYTELNICY!
UPRZEJMIE INFORMUJEMY, ŻE BIBLIOTEKA FUNKCJONUJE W NASTĘPUJĄCYCH GODZINACH:
Wypożyczalnia i Czytelnia Główna: poniedziałek – piątek od 9.00 do 19.00